Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 3 = 554 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Zone 3 275 - 290 °C
527 - 554 °F
Nilit Nilamid A3 H ZB High Impact PA66
Description: Nilamid A3 H ZB is high impact NYLON 66. The product maintains excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas ..
Zone 3 270 - 290 °C
518 - 554 °F
Eurostar Star X 1615 33V S4 PA66, Glass Fiber Reinforced, UV stabilized, Injection Molding
Star X 1615 33V S4 is an Impact Modified, Glass Fiber Reinforced, UV stabilized Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 3 270 - 290 °C
518 - 554 °F
Eurostar Staramide A24G6K PA66, 30% Glass Fiber Reinforced, Heat stabilized, Injection Molding
Staramide A24G6K is an Easy Flow, Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Zone 3 270 - 290 °C
518 - 554 °F
Eurostar Staramide A40 PA66, Extrusion
Staramide A40 is Unreinforced, High Viscosity Polyamide 66, Extrusion ResinInformation provided by Eurostar.
Zone 3 270 - 290 °C
518 - 554 °F
Eurostar Staramide ACF2 PA66, 10% Carbon Fiber Reinforced, Heat stabilized, Injection Molding
Staramide ACF2 is a 10% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Zone 3 270 - 290 °C
518 - 554 °F
Eurostar Staramide ACF3 PA66, 15% Carbon Fiber Reinforced, Heat stabilized, Injection Molding
Staramide ACF3 is a 15% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Zone 3 270 - 290 °C
518 - 554 °F
Eurostar Staramide ACF4 PA66, 20% Carbon Fiber Reinforced, Heat stabilized, Injection Molding
Staramide ACF3 is a 20% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Zone 3 270 - 290 °C
518 - 554 °F
Eurostar Staramide AG3X3 PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding
Staramide AG3X3 is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Zone 3 270 - 290 °C
518 - 554 °F
Eurostar Staramide AK6 PA66, 30% Mineral Reinforced, Injection Molding
Staramide AK6 is a 30% Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Zone 3 275 - 290 °C
527 - 554 °F
Eurostar Staramide PB00A PA6, 50% Glass Bead Filled, Injection Molded
Staramide PB00A is a 50% Glass Bead Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Zone 3 270 - 290 °C
518 - 554 °F
Eurostar Staramide R1000 PA66, Injection Molded
Staramide R1000 is an Unreinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 3 270 - 290 °C
518 - 554 °F
Eurostar Staramide RB004 PA66, 20% Glass Bead Filled, Injection Molded
Staramide RB004 is a 20% Glass Bead Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 3 270 - 290 °C
518 - 554 °F
Eurostar Staramide RF004XXC PA6, 20% Glass Fiber Filled, Injection Molded
Staramide RF004XXC is a 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 3 270 - 290 °C
518 - 554 °F
Eurostar Staramide RF007S PA66, 35% Glass Fiber Filled, Injection Molded
Staramide RF007S is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Zone 3 270 - 290 °C
518 - 554 °F
Eurostar Staramide RF008U PA66/6, 40% Glass Filled, Injection Molded
Staramide RF008U is a 40% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 40V S4)Information provided by Eurostar.
Zone 3 270 - 290 °C
518 - 554 °F
Eurostar Staramide RF006XXP PA66, 30% Glass Fiber Filled, Injection Molded
Staramide RF006XXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006)Information provided by Eurostar.