| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 3 | 285 - 300 °C | 545 - 572 °F | |
|
Nilit Nilamid A3 H G10 50% Glass Reinforced PA66
Description: Nilamid A3 H G10 (50% Glass Reinforced) is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance,..
|
|||
| Zone 3 | 220 - 300 °C | 428 - 572 °F | |
|
Akro-Plastic Akromid® S3 GF 30 4 (3552) PA 6.10 Dry, 30% Glass Filled
(discontinued **)
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
|
|||
| Zone 3 | 280 - 300 °C | 536 - 572 °F | |
|
Lehmann & Voss LUVOCOM® 3/CF/10/BK Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
|
|||
| Zone 3 | 280 - 300 °C | 536 - 572 °F | |
|
Lehmann & Voss LUVOCOM® 3/CF/12/EG Polyamide 6, with carbon fiber, high viscosity
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable..
|
|||
| Zone 3 | 280 - 300 °C | 536 - 572 °F | |
|
Lehmann & Voss LUVOCOM® 3-7088/GY7012 Polyamide 6, with carbon fiber and glass fiber, low-warpage
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall..
|
|||
| Zone 3 | 280 - 300 °C | 536 - 572 °F | |
|
Lehmann & Voss LUVOCOM® 3-8266/BL Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Zone 3 | 280 - 300 °C | 536 - 572 °F | |
|
Lehmann & Voss LUVOCOM® 3-8269 Polyamide 6, with basalt fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.dynamic stressReduced moment of inertia compared with metal parts.Be..
|
|||
| Zone 3 | 280 - 300 °C | 536 - 572 °F | |
|
Lehmann & Voss LUVOCOM® 3-8351 Polyamide 6, with carbon fiber
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated el..
|
|||
| Zone 3 | 280 - 300 °C | 536 - 572 °F | |
|
Lehmann & Voss LUVOCOM® 3-8363 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Zone 3 | 280 - 300 °C | 536 - 572 °F | |
|
Eurostar Starflam RF023P PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam RF0023P is a Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Reinforced Polyamide 66/6 Injection Molding (also known as Starflam PA66C U2 Z23)Information provided by Eurostar.
|
|||
| Zone 3 | 260 - 300 °C | 500 - 572 °F | |
|
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Zone 3 | 260 - 300 °C | 500 - 572 °F | |
|
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Zone 3 | 260 - 300 °C | 500 - 572 °F | |
|
Akro-Plastic Akromid® A3 GF 10 (2852) PA 6.6 Dry, 10% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Zone 3 | 260 - 300 °C | 500 - 572 °F | |
|
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Zone 3 | 260 - 300 °C | 500 - 572 °F | |
|
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Zone 3 | 260 - 300 °C | 500 - 572 °F | |
|
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
|
|||
| Zone 3 | 225 - 300 °C | 437 - 572 °F | |
|
Akro-Plastic Akromid® B3 (2500) PA 6 Dry
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Zone 3 | 225 - 300 °C | 437 - 572 °F | |
|
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Zone 3 | 225 - 300 °C | 437 - 572 °F | |
|
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Dry, 25% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| Zone 3 | 225 - 300 °C | 437 - 572 °F | |
|
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled
In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele..
|
|||
| Zone 3 | 220 - 300 °C | 428 - 572 °F | |
|
Akro-Plastic Akromid® S3 GF 23 1 (2917) PA 6.10 Dry, 23% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
|
|||
| Zone 3 | 220 - 300 °C | 428 - 572 °F | |
|
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
|
|||