| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7194/GY PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7238 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7506 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7776 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Emergency running pro..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7905 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7916 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7920/RD PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8000 PEEK, with carbon fiber, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8048 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8052/EM/BL PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8065 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8157 PEEK, with CNT
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8234 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynam..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8278/GY PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8354 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8476 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1502-7866/GN4 PPSU, unreinforced
Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105/BL8052 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105/GF/30/BK-1 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105/GF/30/NAT-2 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105/XCF/20 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-0831 PEEK, unreinforced, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-1330 PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7128 PEEK, with glass fiber, low-warpage
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Not flammable.High continuos use temperature.High..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7327 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7685 PEEK, unreinforced
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Super..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-7781 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105-8001 PEEK, with glass spheres
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105/TF/20/NAT PEEK, with PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio..
|
|||
| Zone 3 | 390 - 400 °C | 734 - 752 °F | |
|
Lehmann & Voss LUVOCOM® 1105/XCF/15-S PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||