Polymer Property : Zone 4 = 265 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Zone 4 265 - 295 °C
509 - 563 °F
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66
Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a..
Zone 4 265 °C
509 °F
Honeywell Aegis™ HFX High Barrier Nylon  (discontinued **)
Description: Aegis® HFX is an oxygen scavenging polyamide composition formulated specifically for use in high performance packaging applications where high gas barrier is required. This product is ..