| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 4 | 230 - 250 °C | 446 - 482 °F | Extrusion Molding |
|
LG Chemical KEYFLEX BT 2140D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Low ModulusApplication: Films & SheetsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Zone 4 | 230 - 250 °C | 446 - 482 °F | Extrusion Molding |
|
LG Chemical KEYFLEX BT HB9242D Ester Type TPE
Description: TPC-ET, Blow Moldable, Low Modulus, Black ColorApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical
|
|||
| Zone 4 | 230 - 250 °C | 446 - 482 °F | Extrusion Molding |
|
LG Chemical KEYFLEX BT HB9255D Ester Type TPE
Description: TPC-ET, Blow Moldable, Medium Modulus, Black ColorApplication: Air duct, Hose & TubingCAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provided by LG Chemical
|
|||
| Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
|
LG Chemical LG713 ABS, Low Gloss
Feature: Extrusion Molding, Low Gloss, ExtrusionApplication: Automotive Interior Housing (Cover Etc)CAS No. 25120-20-1, 9003-56-9 and 31621-07-5Information provided by LG Chemical
|
|||
| Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
|
LG Chemical LI931 Extrusion ASA
Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical
|
|||
| Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
|
LG Chemical MU620 ABS, Low Deformation
Feature: Extrusion Molding, Low DeformationApplication: Mock-UpCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
|
LG Chemical PI641 ABS, High Impact
Feature: Extrusion Molding, General Purpose, High ImpactApplication: Pipe FittingCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
|
LG Chemical PI642G ABS, General Purpose, High Modulus
Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
|
LG Chemical RS650 ABS
Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
|
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane
Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
|
LG Chemical RS657 ABS, Chemical Resistance to Cyclopentane
Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
|
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity
Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
|
LG Chemical RS800D ABS, High Impact, Chemical Resistance to HCFC
Feature: Extrusion Molding, High Impact, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
|
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC
Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
|
LG Chemical SH610A ABS, High Impact
Feature: Extrusion Molding, General Purpose, High ImpactApplication: Bag, Automobile InteriorCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
|
LG Chemical SH610S ABS, Excellent Surface, High Impact
Feature: Extrusion Molding, Excellent Surface, High ImpactApplication: Bag, miscellaneousCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Zone 4 | 200 - 250 °C | 392 - 482 °F | Extrusion Molding |
|
LG Chemical SH625 ABS, High Impact, High Flow
Feature: Extrusion Molding, High Impact, High FlowApplication: Ski Flat, MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Zone 4 | 220 - 250 °C | 428 - 482 °F | |
|
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma..
|
|||
| Zone 4 | 220 - 250 °C | 428 - 482 °F | |
|
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC)
TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist..
|
|||