Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 4 = 500 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Zone 4 260 °C
500 °F
Barrel Temp of Main Extruder
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin
SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processa..
Zone 4 260 - 290 °C
500 - 554 °F
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC)
TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che..
Zone 4 260 - 290 °C
500 - 554 °F
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high ..
Zone 4 260 °C
500 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 21E830 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Zone 4 260 °C
500 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 41E710 Anhydride Modified LLDPE
BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi..
Zone 4 260 °C
500 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 41E762 Anhydride Modified LLDPE
BYNEL® 41E762 is an anhydride-modified, linear low-density polyethylene (LLDPE) resin. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextru..
Zone 4 260 °C
500 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 41E850 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Zone 4 260 °C
500 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 41E871 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Zone 4 260 °C
500 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 50E662 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Zone 4 260 °C
500 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 50E725 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Zone 4 260 °C
500 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 50E739 Anhydride Modified Polypropylene
BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen..
Zone 4 260 °C
500 °F
Extrusion Coating
DuPont™ Appeel® 20D784 Ethylene Acrylate
Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature ..
Zone 4 260 °C
500 °F
CoExtrusion with Nylon Processing
DuPont™ Bynel® 41E766 Anhydride Modified LLDPE
BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext..
Zone 4 260 - 300 °C
500 - 572 °F
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Zone 4 260 - 300 °C
500 - 572 °F
Akro-Plastic Akromid® A3 GF 10 (2852) PA 6.6 Dry, 10% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Zone 4 260 - 300 °C
500 - 572 °F
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Zone 4 260 - 300 °C
500 - 572 °F
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Zone 4 260 - 300 °C
500 - 572 °F
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Zone 4 260 - 300 °C
500 - 572 °F
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Zone 4 260 - 300 °C
500 - 572 °F
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Zone 4 260 °C
500 °F
Nozzle
BASF Ultradur® B 4330 G6 HR 30% Glass Filled PBT
Description: Is a PBT-I, injection-molding grade with 30% glass fibers, for rigid, tough and dimensionally stable technical parts with increased requirements on hydrolysis resistance and toughness, ..
Zone 4 260 °C
500 °F
Nozzle
BASF Ultradur® B 4300 G6 HR 30% Glass Filled BK 15116 PBT
Description: injection-molding grade with 30% glass-fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance. For example automotive connectors..