Polymer Property : Zone 4 = 518 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Zone 4 270 °C
518 °F
Die
Premix Thermoplastics PRE-ELEC® PA 1412 Conductive Thermoplastic Compound
PRE-ELEC® PA 1412 is a conductive thermoplastic compound based on polyamide 6. Conductivity is achieved by using conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PA 1..
Zone 4 270 °C
518 °F
Cylinder
Premix Thermoplastics PRE-ELEC® PP 1396 Conductive Thermoplastic Compound
PRE-ELEC® PP 1396 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Zone 4 270 - 280 °C
518 - 536 °F
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer
Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr..
Zone 4 270 - 320 °C
518 - 608 °F
Topas Advanced Polymers TOPAS® 6017S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6017S-04 is an injection molding grade with a high heat distortion temperature (170°C) and exceptional dimensional stability. It is a glass-clear amorphous polymer with outstanding moisture..
Zone 4 270 °C
518 °F
Extrusion Coating
DuPont™ Appeel® 20D875 Ethylene Acrylate
Appeel® 20D875 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad tempe..
Zone 4 270 °C
518 °F
Nozzle
BASF Ultradur® S 4090 GX 14% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stab..
Zone 4 270 °C
518 °F
Nozzle
BASF Ultradur® S 4090 G2 10% Glass Filled PBT
Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers..
Zone 4 270 - 295 °C
518 - 563 °F
Nozzle
BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Conditioned)
Description Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, impact modified PA6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughnes..
Zone 4 270 °C
518 °F
Nozzle
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Conditioned)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Zone 4 270 - 295 °C
518 - 563 °F
Nozzle
BASF Ultramid® TG3S 15% Glass Filled PA6 (Dry)
Description: Ultramid TG3S is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a ba..
Zone 4 270 - 295 °C
518 - 563 °F
Nozzle
BASF Ultramid® TG3S BK 5966 15% Glass Filled PA6 (Dry)
Description: Ultramid TG7S Bk-102 is a 34% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the..
Zone 4 270 - 295 °C
518 - 563 °F
Nozzle
BASF Ultramid® TG3S 15% Glass Filled PA6 (Conditioned)
Description: Ultramid TG3S is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a ba..
Zone 4 270 - 295 °C
518 - 563 °F
Nozzle
BASF Ultramid® TG3S BK 5966 15% Glass Filled PA6 (Conditioned)
Description: Ultramid TG7S Bk-102 is a 34% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the..
Zone 4 270 °C
518 °F
Nozzle
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET
Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl..
Zone 4 270 °C
518 °F
Nozzle
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 30% of glass fibers for industrial parts with high dimensional stab..
Zone 4 270 - 295 °C
518 - 563 °F
Nozzle
BASF Ultramid® 8333G HI HS BK 106 33% Glass Filled PA6 (Dry)
Description Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, impact modified PA6 injection molding compound pigmented black developed for applications requiring improved dry as molded toughnes..
Zone 4 270 °C
518 °F
Nozzle
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Dry)
Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire..
Zone 4 270 °C
518 °F
Nozzle
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET
PBT + PET, injection-molding grade containing 20% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin..
Zone 4 270 °C
518 °F
Nozzle
BASF Ultradur® B 4040 G6 30% Glass Filled PBT + PET
PBT + PET, injection-molding grade containing 30% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin..
Zone 4 270 °C
518 °F
Nozzle
BASF Ultradur® B 4300 G10 50% Glass Filled PBT
Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou..