| Hold Pressure |
80.0
-
100
MPa
|
11600
-
14500
psi
|
|
Eurotec® Tecoform® PO20 GR10 NL HS POM, 10% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
| Hold Pressure |
80.0
-
100
MPa
|
11600
-
14500
psi
|
|
Eurotec® Tecoform® PO20 NL IL POM, impact modified, natural
Information provided by Eurotec®
|
| Hold Pressure |
80.0
-
100
MPa
|
11600
-
14500
psi
|
|
Eurotec® Tecoform® PO20 NL RT POM, PTFE modified, natural
Information provided by Eurotec®
|
| Hold Pressure |
80.0
-
100
MPa
|
11600
-
14500
psi
|
|
Eurotec® Tecoform® PO30 GB30 NL HS POM, 30% glass bead reinforced, heat stabilized, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NA30 NL RM PA6.6, MoS2 modified, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NA40 GR15 NL HS PA6.6, 15% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NA40 GR25 NL XA60 PA6.6, 25% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NA40 GR40 NL RM PA6.6, 40% glass fiber reinforced, MoS2 modified, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NA40 GR50 NL RM PA6.6, 50% glass fiber reinforced, MoS2 modified, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NA40 KG30 NL 0B PA6.6, 30% glass fiber/glass bead reinforced, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NB30 BK EF PA6, unfilled, black, suitable for electrostatic powder coating
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NB40 GR20 NL XA60 PA6, 20% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NB40 NL IX PA6, impact modified, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NBX0 HF75 NL PA6, 75% heavy reinforced, improved flexibility, natural
Information provided by Eurotec®
|
| Hold Pressure |
60.0
-
100
MPa
|
8700
-
14500
psi
|
|
Eurotec® Tecopet® PT70 GR15 NL100 PR PET, 15% glass fiber reinforced, heat stabilized, natural, fast crystallization grade
Information provided by Eurotec®
|
| Hold Pressure |
80.0
-
100
MPa
|
11600
-
14500
psi
|
|
Eurotec® Tecoform® PO20 NL RW POM, surface modified, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NA40 CR20 BK111 PA6.6, 20% carbon fiber reinforced, black
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NA40 GR35 NL HS PA6.6, 35% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NA40 NL E PA6.6, unfilled, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NA40 NL IL PA6.6, impact modified, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NB30 MF30 BK001 HS PA6, 30% mineral reinforced, heat stabilized, black
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NB40 GR30 NL AX70 PA6, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
|
| Hold Pressure |
60.0
-
100
MPa
|
8700
-
14500
psi
|
|
Eurotec® Tecopet® PT70 GR15 NL100 MB PET, 15% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecotek® PC30 NL VB03 PC, unfilled, UV stabilized, high impact, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® Nb40 GR30 NL PA6, 30% glass fiber reinforced, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NB40 GR30 NL XA60 PA6, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NB40 GR50 NL PA6, 50% glass fiber reinforced, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NB40 NL E PA6, unfilled, natural
Information provided by Eurotec®
|
| Hold Pressure |
50.0
-
100
MPa
|
7250
-
14500
psi
|
|
Eurotec® Tecomid® NB40 NL IH PA6, impact modified, natural
Information provided by Eurotec®
|