Polymer Property : Hold Pressure = 150 MPa Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Hold Pressure 30.0 - 150 MPa
4350 - 21800 psi
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Hold Pressure 30.0 - 150 MPa
4350 - 21800 psi
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM  (discontinued **)&lt
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Hold Pressure 30.0 - 150 MPa
4350 - 21800 psi
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)  
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Hold Pressure 30.0 - 150 MPa
4350 - 21800 psi
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM  (discontinued **)&l
Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu..