| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time |
10.0
min @Temperature 121 °C |
0.167
hour @Temperature 250 °F |
Let sit for 24 hours to develop a final cure |
|
Lord Adhesives HPC-5B Hydrogenated Nitrile Butadiene Rubber Coating
LORD HPC-5B and HPC-5C are one-part, room temperature curing HNBR coatings which feature robust adhesion and exceptional mechanical properties. These coatings greatly enhance fluid and ozone resista..
|
|||
| Cure Time |
10.0
min @Temperature 121 °C |
0.167
hour @Temperature 250 °F |
Let sit for 24 hours to develop a final cure |
|
Lord Adhesives HPC-6B Ethylene Acrylic Elastomer Coating
LORD HPC-6B and HPC-6C are one-part, room temperature curing ethylene acrylic elastomer (AEM) coatings which feature robust adhesion and exceptional mechanical properties. These coatings enhance ozo..
|
|||
| Cure Time |
10.0
min @Temperature 125 °C |
0.167
hour @Temperature 257 °F |
|
|
Gwent Electronic Materials C2000904P3 Platinum Ink
It can be used on partially stabilized zirconia and tape cast Materials. The Platinum powder contained within this paste has low shrinkage and high adhesion to ceramic substrates. Screen Printing E..
|
|||
| Cure Time |
10.0
min @Temperature 130 °C |
0.167
hour @Temperature 266 °F |
box oven |
|
Gwent Electronic Materials C2070126P5 High Brightness Phosphor Ink (White)
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
|
|||
| Cure Time |
10.0
min @Temperature 130 °C |
0.167
hour @Temperature 266 °F |
belt dryer |
|
Gwent Electronic Materials C2081126P2 Conductive Silver Polymer Paste
This product is a thermoplastic screen printing ink, developed for use in membrane touch switch applications as well as counter electrode in electrochemical sensors and conductive tracks. It may be ..
|
|||
| Cure Time |
10.0
min @Temperature 130 °C |
0.167
hour @Temperature 266 °F |
box oven |
|
Gwent Electronic Materials C2101125P4 High Brightness Phosphor Ink
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
|
|||
| Cure Time |
10.0
min @Temperature 125 °C |
0.167
hour @Temperature 257 °F |
|
|
Tra-Con Tra-Bond 77-2LTC Low Temperature Cure SMD Adhesive
TRA-BOND 77-2LTC one component, solvent-free, insulative epoxy adhesive is designed to cure at temperatures as low as 80°C. This adhesive is specifically designed for attaching surface mounted devi..
|
|||
| Cure Time |
10.0
min @Temperature 150 °C |
0.167
hour @Temperature 302 °F |
|
|
Tra-Con Tra-Duct 2979 Microelectronic Conductive Epoxy Adhesive
TRA-DUCT 2979 is a fast curing one-part epoxy adhesive with superior electrical conductivity and bonding capability. It has been shown to retain these properties through hundreds of hours of rapid t..
|
|||
| Cure Time |
10.0
min @Temperature 150 °C |
0.167
hour @Temperature 302 °F |
|
|
Tra-Con Tra-Duct 2979LV Microelectronic Conductive Epoxy Adhesive
TRA-DUCT 2979LV is a fast curing one-part epoxy adhesive with superior electrical conductivity and bonding capability. It has been shown to retain these properties through hundreds of hours of rapid..
|
|||
| Cure Time |
10.0
min @Temperature 120 °C |
0.167
hour @Temperature 248 °F |
|
|
Trelleborg Emerson & Cuming Eccobond® 927-10 E Needle Bonding Epoxy Adhesive
Emerson & Cuming 927-10 E Eccobond® Needle Bonding Epoxy AdhesiveOne component, fast curing, epoxy adhesive for needle bonding with polypropylene hubs. Also recommended for bonding sealing or insul..
|
|||
| Cure Time |
10.0
min @Temperature 160 °C |
0.167
hour @Temperature 320 °F |
|
|
Trelleborg Emerson & Cuming Eccobond® D 778 One-Component Fast Cure Epoxy Adhesive
Emerson & Cuming D 778 Eccobond® One-Component Fast Cure Epoxy AdhesiveHigh strength, semi-flexible, thixotropic, fast heat curing, epoxy structural adhesive. Good peel strength (20 pli). Recommend..
|
|||
| Cure Time |
10.0
min @Temperature 140 °C |
0.167
hour @Temperature 284 °F |
|
|
Tra-Con Tra-Bond 526M05 Rapid Low Temperature Cure Adhesive
TRA-BOND 526M05 is a low viscosity, fast cure at low temperature, long pot-life adhesive. Information provided by Tra-Con Inc.
|
|||
| Cure Time |
10.0
min @Temperature 155 °C |
0.167
hour @Temperature 311 °F |
TC90 |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
|
|||
| Cure Time |
10.0
min @Temperature 25.0 °C |
0.167
hour @Temperature 77.0 °F |
Tack Free |
|
Chesterton ARC 5 Paste grade Rapid Cure Abrasion Control
Description: ARC 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patc..
|
|||
| Cure Time |
10.0
min @Temperature 100 °C |
0.167
hour @Temperature 212 °F |
Minimum Bond Line |
|
Epoxy Technology EPO-TEK® 330 Low Viscosity, Optical Epoxy
Product Description: EPO-TEK® 330 is a two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications.Advan..
|
|||
| Cure Time |
10.0
min @Temperature 150 °C |
0.167
hour @Temperature 302 °F |
Minimum Bond Line |
|
Epoxy Technology EPO-TEK® H20F Electrically Conductive, Flexible Epoxy
Product Description: EPO-TEK® H20F is a two component, flexible silver epoxy. It was designed for flexible type circuitry, such as switching circuits in a flexible panel system, as well as large di..
|
|||
| Cure Time |
10.0
min @Temperature 100 °C |
0.167
hour @Temperature 212 °F |
minimum |
|
Epoxy Technology EPO-TEK® H54 High Temperature Epoxy
Product Description: EPO-TEK® H54 is a two component, high Tg, electrically and thermally insulating epoxy adhesive for general bonding and high temperature packaging in medical, hybrid, and optica..
|
|||
| Cure Time |
10.0
min @Temperature 43.0 °C |
0.167
hour @Temperature 109 °F |
Light Load |
|
Chesterton ARC MX5 Rapid Curing Fine Particle Wear Compound
Description: An advanced ceramic reinforced composite for the emergency repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a th..
|
|||
| Cure Time |
10.0
min @Temperature 204 °C |
0.167
hour @Temperature 399 °F |
|
|
3M Scotchkote™ 206N Fusion Bonded Epoxy Coating (Fluid Bed Grade)
3M Scotchkote Fusion-Bonded Epoxy Coating 206N (Fluid Bed Grade) is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of metal. The epoxy is applied to preheate..
|
|||
| Cure Time |
10.0
min @Temperature 93.3 °C |
0.167
hour @Temperature 200 °F |
Step 1, preceeded by >10 min. air set |
|
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, Jet Black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, s..
|
|||
| Cure Time |
10.0
min @Temperature 93.3 °C |
0.167
hour @Temperature 200 °F |
Step 1, preceeded by >10 min. air set |
|
Aremco Ceramacoat™ 845-BLU High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, blue coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu..
|
|||
| Cure Time |
10.0
min @Temperature 130 °C |
0.167
hour @Temperature 266 °F |
box oven |
|
Gwent Electronic Materials D2090130P5 Pink Dielectric Ink
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
|
|||