Polymer Property : Cure Time = 0.250 hour Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 95.0 °C
0.250 hour

@Temperature 203 °F
NextGen Adhesives P907-04 Fiber Optic Adhesive
Description: NGAC P907-04 is a low viscosity and room temperature curing adhesive specifically formulated for fiber optic terminations.Advantages and Applications: Uses include the termination of si..
Cure Time 15.0 min

@Temperature 115 °C
0.250 hour

@Temperature 239 °F
Parker Chomerics CHO-BOND 360-208 Conductive Epoxy
Low cost, electrically conductive epoxy adhesive that combines the good adhesive characteristics as epoxy, and the superior electrical conductivity of silver. It is recommended as a thermo-setting E..
Cure Time 15.0 min

@Temperature 23.0 °C
0.250 hour

@Temperature 73.4 °F
Zinc, handling strength
Permabond HM118 Anaerobic Threadlocker
Permabond® HM118 Threadlocker is an excellent general-purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Cure is fast and reliable on s..
Cure Time 15.0 min

@Temperature 23.0 °C
0.250 hour

@Temperature 73.4 °F
M10 steel, handling strength
Permabond HM160 Anaerobic Retaining Compound
Permabond® HM160 is a medium viscosity liquid adhesive that cures when confined between metal parts to form a tough, hard plastic. In the uncured, liquid state, the adhesive wets the metal surfaces..
Cure Time 15.0 min

@Temperature 120 °C
0.250 hour

@Temperature 248 °F
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating
Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the..
Cure Time 15.0 min

@Temperature 120 °C
0.250 hour

@Temperature 248 °F
Resinlab® EP1325 Thixotropic, Heat Curing Epoxy Adhesive
Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where ..
Cure Time 15.0 min

@Temperature 23.0 °C
0.250 hour

@Temperature 73.4 °F
Zinc, handling strength
Permabond MM115P Pure Anaerobic Threadlocker
Permabond® MM115 PURE Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and mainten..
Cure Time 15.0 min

@Temperature 130 °C
0.250 hour

@Temperature 266 °F
Gwent Electronic Materials D2081009D6 Polymer Dielectric
Transparent green colored screen printable polymer dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode. The ..
Cure Time 15.0 min

@Temperature 150 °C
0.250 hour

@Temperature 302 °F
Momentive Performance Materials LVG342 Low Volatile Silicone Adhesive, Mixed, White
LVG342 low volatile silicone adhesive is a two component, thixotropic silicone adhesive that cures very quickly at elevated temperatures to a durable elastomer. LV342 was specifically developed for..
Cure Time 15.0 min

@Temperature 125 °C
0.250 hour

@Temperature 257 °F
Henkel Frekote 44-NC Mold Release Agent
A non-CFC release agent designed to provide multiple releases with no contaminating transfer. Can be used for the release of thermoplastics, thermosetting resins, boron, aramid, graphite / carbon fi..
Cure Time 15.0 min

@Temperature 90.0 °C
0.250 hour

@Temperature 194 °F
Tra-Con Tra-Bond 526H02
Information provided by Tra-Con Inc.
Cure Time 15.0 min

@Temperature >=105 °C
0.250 hour

@Temperature >=221 °F
Trelleborg Emerson & Cuming Eccobond® 45 Two-Component General Purpose Epoxy Adhesive
Emerson & Cuming 45 Eccobond® Two-Component General Purpose Epoxy AdhesiveFilled, general purpose, room temperature curing, epoxy adhesive and sealant. Flexibility can be adjusted by the amount of ..
Cure Time 15.0 min

@Temperature 90.0 °C
0.250 hour

@Temperature 194 °F
1 drop applications
Tra-Con Tra-Bond F109CLR Fiber Optic Epoxy Adhesive
TRA-BOND F109CLR is a clear, low viscosity epoxy specially designed for terminating plastic fibers. This blush free epoxy is an excellent choice for high humidity environments where absolute clarity..
Cure Time 15.0 min

@Temperature 90.0 °C
0.250 hour

@Temperature 194 °F
1 drop applications
Tra-Con Tra-Bond F131 High Tg Room Temperature Cure Fiber Optic Adhesive
TRA-BOND F131 is a fiber-optic adhesive used for terminating ALL types of fiber-optic connectors as well as LED displays, lenses and other optical components. It produces a typical Tg of 95°C thus ..
Cure Time 15.0 min

@Temperature 32.0 °C
0.250 hour

@Temperature 89.6 °F
Light Load
Chesterton ARC 5 Paste grade Rapid Cure Abrasion Control
Description: ARC 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patc..
Cure Time 15.0 min

@Temperature 25.0 °C
0.250 hour

@Temperature 77.0 °F
Tack Free
Chesterton ARC MX5 Rapid Curing Fine Particle Wear Compound
Description: An advanced ceramic reinforced composite for the emergency repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a th..
Cure Time 15.0 min

@Temperature 177 °C
0.250 hour

@Temperature 350 °F
Recommended Cure Cycle
Arlon 55978X030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Cured/Uncured Layers Appearance: Gray silicone gum on glass fiber fabricThis data Represents typical values for the production material..
Cure Time 15.0 min

@Temperature 177 °C
0.250 hour

@Temperature 350 °F
Recommended Cure Cycle
Arlon 56606R026M 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release li..
Cure Time 15.0 - 30.0 min

@Temperature 150 °C
0.250 - 0.500 hour

@Temperature 302 °F
ACC QGel 315 QSI Quantum Silicones General Purpose Silicone Gel
QGel 315 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid..
Cure Time 15.0 min

@Temperature 200 °C
0.250 hour

@Temperature 392 °F
ACC QLE 1050 QSI Quantum Silicones 30 Durometer Clear, Addition Cure, 1-part Elastomer for Coating
QLE 1050 is a 100% silicone solids elastomer designed for use as a conformal coating, but can also be used for cloth coating applications. Key Features: 100% solids Transparent, ideal for pigmentat..
Cure Time 15.0 min

@Temperature 177 °C
0.250 hour

@Temperature 350 °F
Recommended Cure Cycle
Arlon 51426R020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the pr..
Cure Time 15.0 min

@Temperature 177 °C
0.250 hour

@Temperature 350 °F
Recommended Cure Cycle
Arlon 56224R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info..
Cure Time 15.0 min

@Temperature 65.0 °C
0.250 hour

@Temperature 149 °F
Tra-Con Tra-Bond 224-8 Room Temperature Cure Epoxy Adhesive
TRA-BOND 224-8 room temperature cure epoxy adhesive is a thermally conductive version of 224-1. This adhesive develops structural strength rapidly. When cured at room temperature, this adhesive prov..
Cure Time 15.0 min

@Temperature 23.0 °C
0.250 hour

@Temperature 73.4 °F
Brass, working strength
Permabond HM135 Anaerobic Retainer
Permabond® HM135 is a fast curing, medium viscosity anaerobic adhesive for locking and sealing threads and retaining cylindrical components. It gives maximum torque strength on brass or plated bras..
Cure Time 15.0 min

@Temperature 23.0 °C
0.250 hour

@Temperature 73.4 °F
M10 steel, handling strength
Permabond MH052 Anaerobic Threadsealant
Permabond® MH052 is ideal for the sealing of threaded joints. It is approved for use with natural gas and LPG for working pressure up to 20 bar (290 psi) and also for gaseous oxygen up to 10 bar (1..
Cure Time 15.0 min

@Temperature 23.0 °C
0.250 hour

@Temperature 73.4 °F
M10 steel, handling strength
Permabond A126 Anaerobic Retainer
Permabond® A126 is a high-strength anaerobic adhesive for permanent assembly of coaxial assemblies or threaded metal components. The exceptionally low viscosity of this product makes it ideal for u..
Cure Time 15.0 min

@Temperature 23.0 °C
0.250 hour

@Temperature 73.4 °F
M10 steel, handling strength
Permabond A134 Anaerobic Retainer
Permabond® A134 is a high-strength anaerobic product designed for the permanent locking and sealing of metal parts. Its 'non-drip' formulation makes it suitable for use on larger fittings, coarse t..