Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Cure Time = 10.0 min Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Cure Time 10.0 - 30.0 min

@Temperature 93.0 - 121 °C
0.167 - 0.500 hour

@Temperature 199 - 250 °F
Lord Adhesives Chemglaze® V004 Polyurethane Coating
Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m..
Cure Time 10.0 min

@Temperature 93.0 °C
0.167 hour

@Temperature 199 °F
off-line cycle
Lord Adhesives Flocklok® 7000/7204 Flock Adhesive
LORD Flocklok® 7000/7204 adhesive is a two-part, single-coat adhesive used for adhering polyester or nylon flock fibers to a variety of thermoplastics, including PVC, Alcryn®, Sunprene®, ny..
Cure Time 10.0 min

@Temperature 80.0 °C
0.167 hour

@Temperature 176 °F
Gwent Electronic Materials C2040308D2 Silver/Silver Chloride Paste
Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 40/60. The paste is in a ready to use form at a viscosity suitable for automatic or semi-automatic screen printing. The paste..
Cure Time 10.0 min

@Temperature 130 °C
0.167 hour

@Temperature 266 °F
box oven
Gwent Electronic Materials C2080211P2 High Brightness Phosphor Ink (Blue/Green & Blue)
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
Cure Time 10.0 min

@Temperature 125 °C
0.167 hour

@Temperature 257 °F
Gwent Electronic Materials C2090428D4 Gold Ink
Gold Ink is a fritted system that has been designed as a screen printing ink for uses on Alumina. It is also suitable for firing onto other high temperature substrates. This product should be used ..
Cure Time 10.0 min

@Temperature 130 °C
0.167 hour

@Temperature 266 °F
belt dryer
Gwent Electronic Materials C2110817D5 Conductive Silver Polymer Paste
This product is a thermoplastic screen printing ink, developed for use in membrane touch switch applications as well as counter electrode in electro-chemical sensors and conductive tracks. It may b..
Cure Time 10.0 min

@Temperature 80.0 °C
0.167 hour

@Temperature 176 °F
Gwent Electronic Materials C60531D1 Silver / Silver Chloride Paste
C60531D1 has a ratio of Silver to Silver Chloride of 90/10. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a fa..
Cure Time 10.0 min

@Temperature 80.0 °C
0.167 hour

@Temperature 176 °F
Gwent Electronic Materials C61003P7 Silver / Silver Chloride Paste
C61003P7 has a ratio of Silver to Silver Chloride of 60/40. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a fa..
Cure Time 10.0 - 30.0 min

@Temperature 93.0 - 121 °C
0.167 - 0.500 hour

@Temperature 199 - 250 °F
Lord Adhesives Chemglaze® V209 Polyurethane Coating
Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m..
Cure Time 10.0 min

@Temperature 130 °C
0.167 hour

@Temperature 266 °F
box oven
Gwent Electronic Materials D2070209P6 White Dielectric Paste
This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera..
Cure Time 10.0 min

@Temperature 120 °C
0.167 hour

@Temperature 248 °F
Press Cure
Shin-Etsu Silicones LIMSâ„¢ KE2004-20A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
Cure Time 10.0 min

@Temperature 150 °C
0.167 hour

@Temperature 302 °F
Tra-Con Tra-Bond 526M01 Rigid Thixotropic Adhesive
TRA-BOND 526M01 is two-component, rigid, thixotropic material developed specifically for fiber optic applications. The material is a cream color when mixed and changes to a red amber color when full..
Cure Time 10.0 min

@Temperature 100 °C
0.167 hour

@Temperature 212 °F
Minimum Bond Line
Epoxy Technology EPO-TEK® 353ND High Temperature Epoxy
Product Description: EPO-TEK® 353ND is a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applications. It is one of the most popular EPO-TEK® bra..
Cure Time 10.0 min

@Temperature 150 °C
0.167 hour

@Temperature 302 °F
Minimum Bond Line
Epoxy Technology EPO-TEK® H20F Electrically Conductive, Flexible Epoxy
Product Description: EPO-TEK® H20F is a two component, flexible silver epoxy. It was designed for flexible type circuitry, such as switching circuits in a flexible panel system, as well as large di..
Cure Time 10.0 min

@Temperature 150 °C
0.167 hour

@Temperature 302 °F
Atom Adhesives AA-DUCT 2979 Epoxy Adhesive
AA-DUCT 2979 is a fast curing one part epoxy adhesive with superior electrical conductivity and bonding capability. AA-DUCT 2979 has been shown to retain their properties through hundreds of hours o..
Cure Time 10.0 min

@Temperature 93.3 °C
0.167 hour

@Temperature 200 °F
Step 1, preceeded by >10 min. air set
Aremco Quartz-Coat™ 845 High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, brown-black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps..
Cure Time 10.0 min

@Temperature 75.0 °C
0.167 hour

@Temperature 167 °F
Recoat, at 50% humidity
Blue River Coatings High Performance Acrylic Sanding Sealer
BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC SANDING SEALER is a waterbased wood sealer to fill the grain. The product is designed to be a sandable self-sealing topcoat for wood. HIGH PERFORMANCE AC..
Cure Time 10.0 min

@Temperature 75.0 °C
0.167 hour

@Temperature 167 °F
Dust Free, at 50% humidity
Blue River Coatings Undercoat Primer
BLUE RIVER COATINGS UNDERCOAT PRIMER is a high quality, single component primer, not requiring any catalyzing agent. Performance obtained is equal or superior to that of two-component, catalyzed epo..
Cure Time 10.0 min

@Temperature 93.3 °C
0.167 hour

@Temperature 200 °F
Step 1, preceeded by >10 min. air set
Aremco Ceramacoat™ 845-BLU High Temperature Ceramic-Inorganic Coating
Single part, waterborne, silicon-filled, phosphate-bonded, blue coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu..
Cure Time 10.0 min

@Temperature 80.0 °C
0.167 hour

@Temperature 176 °F
Gwent Electronic Materials C2060602D1 Membrane Touch Switch Paste
The ink should be gently stirred before use avoiding introduction of air bubbles. It is a polymer based system for printing on polyester, PVC, etc.Can be used in membrane touch switch applicationsSc..
Copyright © lookpolymers.com All Rights Reserved