Processing Properties Metric English Comments
Cure Time 960 - 1440 min
<br>@Temperature 25.0 °C
16.0 - 24.0 hour
<br>@Temperature 77.0 °F
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
Cure Time 960 - 1440 min
<br>@Temperature 82.2 °C
16.0 - 24.0 hour
<br>@Temperature 180 °F
Complete Cure Cycle
Northstar Polymers MSS-A80AQ High Performance Polyurethane Cast Elastomer System 80A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
Cure Time 960 - 1440 min
<br>@Temperature 82.2 °C
16.0 - 24.0 hour
<br>@Temperature 180 °F
Complete Cure Cycle
Northstar Polymers MSS-A85BQ High Performance Polyurethane Cast Elastomer System 85A
This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio..
Cure Time 720 - 1440 min
<br>@Temperature 23.0 °C
12.0 - 24.0 hour
<br>@Temperature 73.4 °F
Resin Technology Group 120-EX Oxy-Bond™ Two-Component Epoxy Adhesive
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma..
Cure Time 360 - 1440 min
<br>@Temperature 23.0 °C
6.00 - 24.0 hour
<br>@Temperature 73.4 °F
Zinc, working strength
Permabond LH197 Anaerobic Gasketmaker
Permabond® LH197 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is highly flexible, making it ideal for dissimilar surfaces where differential th..
Cure Time 360 - 1440 min
<br>@Temperature 23.0 °C
6.00 - 24.0 hour
<br>@Temperature 73.4 °F
Zinc, working strength
Permabond LM012 Anaerobic Threadsealant
Permabond® LM012 is an unfilled, medium viscosity anaerobic adhesive. Its major benefit as related to other pipe sealants is that it is an unfilled resin that is compatible with hydraulic fluids. I..
Cure Time 360 - 1440 min
<br>@Temperature 23.0 °C
6.00 - 24.0 hour
<br>@Temperature 73.4 °F
Zinc, working strength
Permabond F201 Anaerobic Retainer
Permabond® F201 is an anaerobic adhesive which has been developed to give excellent resistance to peel and impact forces. This toughening, combined with good adhesion to aluminum and copper alloys,..
Cure Time 360 - 1440 min
<br>@Temperature 23.0 °C
6.00 - 24.0 hour
<br>@Temperature 73.4 °F
Zinc, working strength
Permabond HH040 Anaerobic Retainer
Permabond® HH040 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure unitiz..
Cure Time 360 - 1440 min
<br>@Temperature 23.0 °C
6.00 - 24.0 hour
<br>@Temperature 73.4 °F
Zinc, working strength
Permabond HH040 Pure NSF 61 Approved Anaerobic Retainer
Permabond® HH040 PURE is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure u..
Cure Time 360 - 1440 min
<br>@Temperature 23.0 °C
6.00 - 24.0 hour
<br>@Temperature 73.4 °F
Zinc, working strength
Permabond MH199 Anaerobic Gasketmaker
Permabond® MH199 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets, thereby offering po..
Cure Time 720 - 1440 min
<br>@Temperature 23.9 °C
12.0 - 24.0 hour
<br>@Temperature 75.0 °F
plus 2 hrs at 150-200°F
Master Bond EP21LV-LO Two Component, Lower Viscosity, Room Temperature Curing Epoxy System
Product Description: Master Bond EP21LV-LO is a two component, lower viscosity, room temperature curing epoxy system for high performance bonding, sealing, coating and encapsulation. This user frien..
Cure Time 720 - 1440 min
<br>@Temperature 23.9 °C
12.0 - 24.0 hour
<br>@Temperature 75.0 °F
plus 2 hrs at 150-200°F
Master Bond EP21NDFG Two component epoxy compound for high performance applications
Product Description: Master Bond EP21NDFG is a two component, room temperature curing epoxy adhesive featuring outstanding physical properties, easy processing and a non-drip, paste-like consistency..
Cure Time 720 - 1440 min
<br>@Temperature 23.9 °C
12.0 - 24.0 hour
<br>@Temperature 75.0 °F
plus 2 hrs at 150-200°F
Master Bond EP21NDLO Low Outgassing, Room Temperature Curing Two Component Epoxy
Master Bond EP21ND-LO is a two component, room temperature curing epoxy system for bonding, sealing and coating featuring outstanding physical properties. EP21ND-LO has a convenient one to one mix r..
Cure Time 1080 - 1440 min
<br>@Temperature 23.0 °C
18.0 - 24.0 hour
<br>@Temperature 73.4 °F
Master Bond EP30 Optically Clear, Low Viscosity Two Component Epoxy
Master Bond Polymer System EP30 is a low viscosity, two component epoxy system for high performance bonding, coating, sealing, potting and encapsulation. It readily cures at room temperature or more..
Cure Time 960 - 1440 min
<br>@Temperature 25.0 °C
16.0 - 24.0 hour
<br>@Temperature 77.0 °F
Trelleborg Emerson & Cuming Eccobond® 15 LV Clear Variable Hardness Low Viscosity Catalyst
Emerson & Cuming 15 LV Clear Eccobond® Variable Hardness Low Viscosity CatalystLow viscosity. Easy-to-use, simple mix ratios. Hardness of cured castings can be controlled by the amount of hardener ..
Cure Time 960 - 1440 min
<br>@Temperature 25.0 °C
16.0 - 24.0 hour
<br>@Temperature 77.0 °F
Trelleborg Emerson & Cuming Eccobond® 15 LV Variable Hardness Low Viscosity Catalyst
Emerson & Cuming 15 LV Eccobond® Variable Hardness Low Viscosity CatalystLow viscosity. Easy-to-use, simple mix ratios. Hardness of cured castings can be controlled by the amount of hardener used. ..
Cure Time 960 - 1440 min
<br>@Temperature 25.0 °C
16.0 - 24.0 hour
<br>@Temperature 77.0 °F
Trelleborg Emerson & Cuming Eccobond® 15 Variable Hardness Catalyst
Emerson & Cuming 15 Eccobond® Variable Hardness CatalystEasy-to-use, simple mix ratios. Hardness of cured castings can be controlled by the amount of hardener used. Long working life. Yields cured ..
Cure Time 960 - 1440 min
<br>@Temperature 25.0 °C
16.0 - 24.0 hour
<br>@Temperature 77.0 °F
Trelleborg Emerson & Cuming Eccobond® 23 LV General Purpose Catalyst
Emerson & Cuming 23 LV Eccobond® General Purpose CatalystExcellent low temperature performance properties, excellent thermal shock/cycle and impact resistance. Good hardener for cryogenic applicati..
Cure Time 960 - 1440 min
<br>@Temperature 25.0 °C
16.0 - 24.0 hour
<br>@Temperature 77.0 °F
Trelleborg Emerson & Cuming Eccobond® 43 Heat Cure Catalyst
Emerson & Cuming 43 Eccobond® Heat Cure CatalystRoom temperature gelling version of 28. Excellent for low stress potting and bonding. Will post cure in actual use. Combines the benefits of both 9 a..
Cure Time 1080 - 1440 min
<br>@Temperature 23.9 °C
18.0 - 24.0 hour
<br>@Temperature 75.0 °F
ambient temperatures
Master Bond EP40 High Shear and Peel Strength, Two Component, Flexible Epoxy
Master Bond Polymer System EP40 is newly developed two component highly flexible epoxy compound for high performance bonding, potting, encapsulation, and sealing with outstanding shear and peel stre..
Cure Time 1080 - 1440 min
<br>@Temperature 23.0 °C
18.0 - 24.0 hour
<br>@Temperature 73.4 °F
Master Bond Supreme 11HT High Temperature Resistant Two Component Epoxy System
Master Bond Polymer System Supreme 11HT is an easy to use two part epoxy adhesive/sealant combining both high shear and high peel strengths along with a relatively fast cure at room temperature. Sup..
Cure Time 960 - 1440 min
<br>@Temperature 25.0 °C
16.0 - 24.0 hour
<br>@Temperature 77.0 °F
Trelleborg Emerson & Cuming Eccobond® 15 Clear Variable Hardness Catalyst
Emerson & Cuming 15 Clear Eccobond® Variable Hardness CatalystEasy-to-use, simple mix ratios. Hardness of cured castings can be controlled by the amount of hardener used. Long working life. Yields ..
Cure Time 300 - 1440 min
<br>@Temperature 22.0 °C
5.00 - 24.0 hour
<br>@Temperature 71.6 °F
Dow Corning Q3-6575 DIELECTRIC GEL A/B KIT
Two-part, clear, RT or heat cure and low temperature (-80°C/-112°F)stability.Information provided by Dow Corning
Cure Time 960 - 1440 min
<br>@Temperature 21.0 °C
16.0 - 24.0 hour
<br>@Temperature 69.8 °F
De-Mold Time: 1.5-2 hrs
3M Scotchcast™ 2130 Flame-Retardant Compound
3M Scotchcast Flame-Retardant Compound 2130 is a two-part polyurethane resin designed to replace the cable jacket when splicing or repairing mine and portable cables. Its unique formulation makes it..
Cure Time 960 - 1440 min
<br>@Temperature 21.0 °C
16.0 - 24.0 hour
<br>@Temperature 69.8 °F
De-Mold Time: 1.5-2 hrs
3M Scotchcast™ 2131 Flame-Retardant Compound
3M Scotchcast Flame-Retardant Compound 2131 is a two-part polyurethane resin designed to replace the cable jacket when splicing or repairing mine and portable cables. It formulation makes it particu..
Cure Time 960 - 1440 min
<br>@Temperature 24.0 °C
16.0 - 24.0 hour
<br>@Temperature 75.2 °F
demold time
BCC Products BC 8990 Polyurethane Elastomer
BC8990 is a two-component urethane elastomer compound specifically designed for general purpose molding and casting of various shapes. This product is a safe, easy-to-handle, room temperature mixing..
Cure Time 360 - 1440 min
<br>@Temperature 23.0 °C
6.00 - 24.0 hour
<br>@Temperature 73.4 °F
Zinc, working strength
Permabond A011 Anaerobic Threadlocker
Permabond® A011 is an anaerobic adhesive designed for locking and sealing threaded or coaxially fitting metal parts where subsequent dismantling is required. Its controlled strength ensures fatigue..
Cure Time 360 - 1440 min
<br>@Temperature 23.0 °C
6.00 - 24.0 hour
<br>@Temperature 73.4 °F
Zinc, working strength
Permabond A113 Anaerobic Threadlocker
Designed for the locking and sealing of metal parts, Permabond® A113 is ideally suited for use on components that need to be dismantled for maintenance. Giving vibration resistance it can be used ..
Cure Time 360 - 1440 min
<br>@Temperature 23.0 °C
6.00 - 24.0 hour
<br>@Temperature 73.4 °F
Zinc, working strength
Permabond A130 Anaerobic Threadlocker
Designed for the locking and sealing of metal parts, Permabond® A130 is ideally suited for use on components that need to be dismantled for maintenance. Giving vibration resistance it can be used t..