Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Cure Time = 20.0 hour Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Cure Time 1200 min
<br>@Temperature 25.0 °C
20.0 hour
<br>@Temperature 77.0 °F
Full Load
Chesterton ARC 10 Paste grade machinable composite
Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance and corrosion resistance. It is non-sag..
Cure Time 1200 min
<br>@Temperature 25.0 °C
20.0 hour
<br>@Temperature 77.0 °F
Overend Coat
Chesterton ARC 855 Abrasion Control Liquid
Description: An advanced ceramic composite formulated to protect equipment from aggressive chemical attack, corrosion, and erosion. The product is a low viscosity composite that is easily applied by..
Cure Time 1200 min
<br>@Temperature 25.0 °C
20.0 hour
<br>@Temperature 77.0 °F
Full Load
Chesterton ARC 858 Abrasion resistant rebuilding and faring composite
An advanced ceramic composite for the repair and protection of all metal surfaces subjected to erosion, corrosion and chemical attack. It is normally applied at a thickness of 0.15 mm (60 mils) or m..
Cure Time 1200 min
<br>@Temperature 32.0 °C
20.0 hour
<br>@Temperature 89.6 °F
Full Load
Chesterton ARC 890 Course Grade Sliding Wear Compound
An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at the thickness of 6 mm (1/4”)..
Cure Time 1200 min
<br>@Temperature 32.0 °C
20.0 hour
<br>@Temperature 89.6 °F
Full Load
Chesterton ARC 897 Fine Grade Sliding Wear Compound
Description: ARC 897 is an advanced ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a t..
Cure Time 1200 min
<br>@Temperature 32.0 °C
20.0 hour
<br>@Temperature 89.6 °F
Full Load
Chesterton ARC 982 100% Novolac acid resistant coating
Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. A low viscosity composite that is applied by brush, squeegee, or a plural compo..
Cure Time 1200 min
<br>@Temperature 16.0 °C
20.0 hour
<br>@Temperature 60.8 °F
Light Load/Overcoat End
Chesterton ARC 982 100% Novolac acid resistant coating
Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. A low viscosity composite that is applied by brush, squeegee, or a plural compo..
Cure Time 1200 min
<br>@Temperature 32.0 °C
20.0 hour
<br>@Temperature 89.6 °F
Full Load
Chesterton ARC BX1 Sliding Wear Compound
Description: An advanced contractor grade ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at..
Cure Time 1200 min
<br>@Temperature 32.0 °C
20.0 hour
<br>@Temperature 89.6 °F
Full Load
Chesterton ARC BX2 Contractor Grade Fine Sliding Wear Compound
Description: ARC BX2 is an advanced contractor grade ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It ..
Cure Time 1200 min
<br>@Temperature 32.0 °C
20.0 hour
<br>@Temperature 89.6 °F
Full Load
Chesterton ARC CS4 low-viscosity, 100% solids, barrier coating
Description: An advanced composite formulated to protect concrete surfaces from harsh chemical attack. It is normally applied at a thickness of 250-375 microns (10-15 mils) per coat in a 2 coat syst..
Cure Time 1200 min
<br>@Temperature 32.0 °C
20.0 hour
<br>@Temperature 89.6 °F
Full Load
Chesterton ARC I BX1 Impact & Wear Resistant Epoxy Composite
Description: An advanced grade epoxy and urethane composite for the repair and protection of all metal surfaces subjected to severe abrasion and impact. It is normally applied at a thickness of 6 mm..
Cure Time 1200 min
<br>@Temperature 25.0 °C
20.0 hour
<br>@Temperature 77.0 °F
Full Load
Chesterton ARC MX1 Vertical Build Extreme Wear Compound
Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It is applied at a thickness of 6 mm (1/4”)..
Cure Time 1200 min
<br>@Temperature 25.0 °C
20.0 hour
<br>@Temperature 77.0 °F
Overcoat End
Chesterton ARC S2 Ceramic reinforced erosion resistant coating
Description: An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% soli..
Cure Time 1200 min
<br>@Temperature 25.0 °C
20.0 hour
<br>@Temperature 77.0 °F
Overcoat End
Chesterton ARC SD4i High temperature ceramic reinforced erosion resistant coating
Description: An advanced ceramic composite for resurfacing and protection of metal surfaces in immersion service. It is normally applied in a thickness range of 250-370 microns (10-15 mils) per coat..
Cure Time 1200 min
<br>@Temperature 25.0 °C
20.0 hour
<br>@Temperature 77.0 °F
Overcoat End
Chesterton MRS S2 Metal Rebuilding System
An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% solids. MRS S2 is..
Cure Time 1200 min
<br>@Temperature 25.0 °C
20.0 hour
<br>@Temperature 77.0 °F
Overcoat End
Chesterton MRS SD4i Metal Rebuilding System
An advanced ceramic composite for resurfacing and protection of metal surfaces in immersion service. It is normally applied in a thickness range of 250-370 microns (10 – 15 mils) per coat. Non-shri..
Cure Time 1200 min
<br>@Temperature 32.0 °C
20.0 hour
<br>@Temperature 89.6 °F
Full Load
Chesterton ARC MX2 High Wear Fine Particle Wear Compound
Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion and chemical attack. It is applied at a thickness of 3 mm (1/8”..
Cure Time 1200 min
<br>@Temperature 25.0 °C
20.0 hour
<br>@Temperature 77.0 °F
Full Load
Chesterton ARC MXC Castable Extreme Wear Compound
Description: An advanced ceramic composite, with flowable viscosity, for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It can be hand tro..
Cure Time 1200 min
<br>@Temperature 25.0 °C
20.0 hour
<br>@Temperature 77.0 °F
ACC QGel 300 QSI Quantum Silicones High Strength Gel
QGel 300 is a clear, very soft, tough, moderately cross-linked, silicone polymer. Silicone gels are used to provide protection from vibration, thermal or mechanical shock. Silicone gels also provide..
Cure Time 1200 min
<br>@Temperature -4.00 °C
20.0 hour
<br>@Temperature 24.8 °F
3M Scotchcast™ 2104 Electrical Insulating Resin
Scotchcast 2104 Electrical Insulating Resin is a hard, two-part, polyurethane resin encapsulant designed especially for permanent splice protection. 2104 is formulated for virtually every electrical..
Cure Time 1200 min
<br>@Temperature 32.0 °C
20.0 hour
<br>@Temperature 89.6 °F
Full Load
Chesterton ARC CS2 Low-viscosity, Composite concrete primer sealer
Description: An advanced composite formulated to protect concrete surfaces from mild chemical attack. It is normally applied at a thickness of 250-375 microns (10-15 mils) per coat. Non-shrinking. 1..
Cure Time 1200 min
<br>@Temperature 25.0 °C
20.0 hour
<br>@Temperature 77.0 °F
Full Load
Chesterton MRS 10 Metal Rebuilding System
Description: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance It is non-sagging, non-shrinking and 10..
Cure Time 1200 min
<br>@Temperature 25.0 °C
20.0 hour
<br>@Temperature 77.0 °F
Full Load
Chesterton MRS 58 Metal Rebuilding System
An advanced ceramic composite for the repair and protection of all metal surfaces subjected to erosion, corrosion and chemical attack. It is normally applied at a thickness of 1.5 mm (60 mils) or mo..
Cure Time 1200 min
<br>@Temperature 32.0 °C
20.0 hour
<br>@Temperature 89.6 °F
Full Load
Chesterton MRS 58 Metal Rebuilding System
An advanced ceramic composite for the repair and protection of all metal surfaces subjected to erosion, corrosion and chemical attack. It is normally applied at a thickness of 1.5 mm (60 mils) or mo..
Copyright © lookpolymers.com All Rights Reserved