| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time |
360
-
480
min <br>@Temperature 25.0 °C
|
6.00
-
8.00
hour <br>@Temperature 77.0 °F
|
De-mold Time |
|
Northstar Polymers MPP-A47A Liquid Castable Polyurethane
MPP-A47A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott..
|
|||
| Cure Time |
360
min <br>@Temperature 23.0 °C
|
6.00
hour <br>@Temperature 73.4 °F
|
Stainless steel, handling strength |
|
Permabond F202 Anaerobic Retainer
The unique 'toughening' process incorporated into Permabond® F202 gives this anaerobic adhesive excellent resistance to peel and impact forces. Primarily designed for use on metal surfaces, it is a..
|
|||
| Cure Time |
360
min <br>@Temperature 23.0 °C
|
6.00
hour <br>@Temperature 73.4 °F
|
Stainless steel, handling strength |
|
Permabond HH120 Anaerobic Threadlocker
Permabond® HH120 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Its high viscosity allows for ..
|
|||
| Cure Time |
360
min <br>@Temperature 23.0 °C
|
6.00
hour <br>@Temperature 73.4 °F
|
Stainless steel, handling strength |
|
Permabond HL126 Anaerobic Threadlocker
PERMABOND® HL126 Threadlocker is a water thin product for locking pre-assembled parts through wicking action. PERMABOND® HL126 Threadlocker prevents vibration loosening. Because of the low viscosi..
|
|||
| Cure Time |
360
min <br>@Temperature 23.0 °C
|
6.00
hour <br>@Temperature 73.4 °F
|
Stainless steel, handling strength |
|
Permabond HM160 Anaerobic Retaining Compound
Permabond® HM160 is a medium viscosity liquid adhesive that cures when confined between metal parts to form a tough, hard plastic. In the uncured, liquid state, the adhesive wets the metal surfaces..
|
|||
| Cure Time |
360
min <br>@Temperature 23.0 °C
|
6.00
hour <br>@Temperature 73.4 °F
|
Stainless steel, handling strength |
|
Permabond HM165 Anaerobic Retainer
Permabond® HM165 is a high viscosity anaerobic retaining compound that cures when confined between metal parts to form a tough bond. It is best suited for cylindrical parts and where high temperatu..
|
|||
| Cure Time |
360
min <br>@Temperature 23.0 °C
|
6.00
hour <br>@Temperature 73.4 °F
|
Zinc, working strength |
|
Permabond LH150 Anaerobic Threadsealant
Permabond® LH150 Pipe Sealant with PTFE is designed for sealing and locking tapered metal pipe threads and fittings. It is ideal for stainless steel and other passive metals. Instant sealing of up ..
|
|||
| Cure Time |
360
min <br>@Temperature 23.0 °C
|
6.00
hour <br>@Temperature 73.4 °F
|
M10 steel, working strength |
|
Permabond LM113 Anaerobic Threadlocker
Permabond® LM113 Threadlocker is a medium viscosity product for locking small threaded fasteners, such as screws and bolts or hydraulic fittings that might require disassembly. Due to its thixotrop..
|
|||
| Cure Time |
360
min <br>@Temperature 23.0 °C
|
6.00
hour <br>@Temperature 73.4 °F
|
Stainless steel, handling strength |
|
Permabond F201 Anaerobic Retainer
Permabond® F201 is an anaerobic adhesive which has been developed to give excellent resistance to peel and impact forces. This toughening, combined with good adhesion to aluminum and copper alloys,..
|
|||
| Cure Time |
360
min <br>@Temperature 23.0 °C
|
6.00
hour <br>@Temperature 73.4 °F
|
Stainless steel, handling strength |
|
Permabond HH040 Anaerobic Retainer
Permabond® HH040 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure unitiz..
|
|||
| Cure Time |
360
min <br>@Temperature 23.0 °C
|
6.00
hour <br>@Temperature 73.4 °F
|
M10 steel, full strength |
|
Permabond MM115 Anaerobic Threadlocker
Permabond® MM115 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and maintenance...
|
|||
| Cure Time |
360
min <br>@Temperature 23.0 °C
|
6.00
hour <br>@Temperature 73.4 °F
|
Zinc, full strength |
|
Permabond MM115P Pure Anaerobic Threadlocker
Permabond® MM115 PURE Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and mainten..
|
|||
| Cure Time |
360
min <br>@Thickness 2.00 mm
|
6.00
hour <br>@Thickness 0.0787 in
|
room temp |
|
Loctite® 5920™ RTV Silicone Sealant
LOCTITE® 5920™ is a moisture-curing, non-corrosive silicone. The thixotropic nature of LOCTITE® 5920™ reduces the migration of liquid product after application to the substrate. It has been desi..
|
|||
| Cure Time |
360
min <br>@Temperature 32.0 °C
|
6.00
hour <br>@Temperature 89.6 °F
|
Light Load |
|
Chesterton ARC 855 Abrasion Control Liquid
Description: An advanced ceramic composite formulated to protect equipment from aggressive chemical attack, corrosion, and erosion. The product is a low viscosity composite that is easily applied by..
|
|||
| Cure Time |
360
min <br>@Temperature 32.0 °C
|
6.00
hour <br>@Temperature 89.6 °F
|
Light Load |
|
Chesterton ARC 890 Course Grade Sliding Wear Compound
An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at the thickness of 6 mm (1/4”)..
|
|||
| Cure Time |
360
min <br>@Temperature 32.0 °C
|
6.00
hour <br>@Temperature 89.6 °F
|
Light Load |
|
Chesterton ARC 897 Fine Grade Sliding Wear Compound
Description: ARC 897 is an advanced ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a t..
|
|||
| Cure Time |
360
min <br>@Temperature 16.0 °C
|
6.00
hour <br>@Temperature 60.8 °F
|
Overcoat Begin |
|
Chesterton ARC S7 High Temperature & Chemical Resistant Novolac Vinyl Ester Coating
Description: ARC S7 is a low VOC, epoxy novolac vinyl ester based coating intended for high temperature exposures in chemically aggressive applications where the risk for thermal cycling may be pres..
|
|||
| Cure Time |
360
min <br>@Temperature 10.0 °C
|
6.00
hour <br>@Temperature 50.0 °F
|
Tack Free |
|
Chesterton ARC SD4i High temperature ceramic reinforced erosion resistant coating
Description: An advanced ceramic composite for resurfacing and protection of metal surfaces in immersion service. It is normally applied in a thickness range of 250-370 microns (10-15 mils) per coat..
|
|||
| Cure Time |
360
min <br>@Temperature 60.0 °C
|
6.00
hour <br>@Temperature 140 °F
|
|
|
Cytec EN-2523 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
|
|||
| Cure Time |
360
min <br>@Temperature 60.0 °C
|
6.00
hour <br>@Temperature 140 °F
|
|
|
Cytec EN-2527 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
|
|||
| Cure Time |
360
min <br>@Temperature 60.0 °C
|
6.00
hour <br>@Temperature 140 °F
|
|
|
Cytec EN-2541 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
|
|||
| Cure Time |
360
min <br>@Temperature 25.0 °C
|
6.00
hour <br>@Temperature 77.0 °F
|
Tack Free |
|
Chesterton ARC HT-S High Temperature Corrosion Resistant Coating
Description: ARC HT-S is a high temperature corrosion resistant coating for continuous operating conditions at elevated temperatures. It is easily applied by brush or roller and can be sprayed with ..
|
|||
| Cure Time |
360
min <br>@Temperature 32.0 °C
|
6.00
hour <br>@Temperature 89.6 °F
|
Light Load |
|
Chesterton ARC MX2 High Wear Fine Particle Wear Compound
Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion and chemical attack. It is applied at a thickness of 3 mm (1/8”..
|
|||
| Cure Time |
360
min <br>@Temperature 107 °C
|
6.00
hour <br>@Temperature 225 °F
|
|
|
Aremco Pyro-Putty™ 950 High Temperature Ceramic-Metallic Putty, Ceramic Fiber Filled
Ceramic Fiber-Filled, Organic Caulk.For Sealing High Temperature Joints to 950°F.Cures Into a Tough, Pliable, Inert Material.
|
|||
| Cure Time |
360
min <br>@Temperature 25.0 °C
|
6.00
hour <br>@Temperature 77.0 °F
|
|
|
Tra-Con Tra-Bond 224-8 Room Temperature Cure Epoxy Adhesive
TRA-BOND 224-8 room temperature cure epoxy adhesive is a thermally conductive version of 224-1. This adhesive develops structural strength rapidly. When cured at room temperature, this adhesive prov..
|
|||
| Cure Time |
360
min <br>@Temperature 23.0 °C
|
6.00
hour <br>@Temperature 73.4 °F
|
Stainless steel, handling strength |
|
Permabond A011 Anaerobic Threadlocker
Permabond® A011 is an anaerobic adhesive designed for locking and sealing threaded or coaxially fitting metal parts where subsequent dismantling is required. Its controlled strength ensures fatigue..
|
|||
| Cure Time |
360
min <br>@Temperature 32.0 °C
|
6.00
hour <br>@Temperature 89.6 °F
|
Foot Traffic |
|
Chesterton ARC CS2 Low-viscosity, Composite concrete primer sealer
Description: An advanced composite formulated to protect concrete surfaces from mild chemical attack. It is normally applied at a thickness of 250-375 microns (10-15 mils) per coat. Non-shrinking. 1..
|
|||
| Cure Time |
360
min <br>@Temperature 23.0 °C
|
6.00
hour <br>@Temperature 73.4 °F
|
Stainless steel, handling strength |
|
Permabond A126 Anaerobic Retainer
Permabond® A126 is a high-strength anaerobic adhesive for permanent assembly of coaxial assemblies or threaded metal components. The exceptionally low viscosity of this product makes it ideal for u..
|
|||
| Cure Time |
360
min <br>@Temperature 23.0 °C
|
6.00
hour <br>@Temperature 73.4 °F
|
Stainless steel, handling strength |
|
Permabond A131 Anaerobic Threadsealant
Permabond® A131 is an anaerobic adhesive designed to seal threaded metal pipe connections carrying a wide variety of gases and liquids, including potable water. Suitable for use on both parallel an..
|
|||