Polymer Property : Cure Time = 4320 min Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Cure Time 4320 min
<br>@Temperature 25.0 °C
72.0 hour
<br>@Temperature 77.0 °F
50%; Recommended for 1/8&quot; dia bead
Parker Chomerics Tecknit® 72-00151 Silver-Filled Flexible Resin Caulking System
Description: TECKNIT standard electrically conductive caulks consist of four one-component resin systems filled with silver plated glass or copper particles. These systems are formulated to provide ..
Cure Time 4320 min
<br>@Temperature 23.0 °C
72.0 hour
<br>@Temperature 73.4 °F
Parker Chomerics THERM-A-FORM T644 Cure-in-Place Potting and Underfill Material
Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co..
Cure Time 4320 min
<br>@Temperature 25.0 °C
72.0 hour
<br>@Temperature 77.0 °F
50%; Full Cure
Parker Chomerics Tecknit CON/RTV-I One Part: Silver-Filled Silicone RTV
Description: TECKNIT CON/RTV-I system is a pure silver loaded, one component RTV silicone adhesive sealant. It is ready to use without mixing and cures quickly at room temperature on exposure to moi..
Cure Time 4320 - 7200 min
<br>@Temperature 25.0 °C
72.0 - 120 hour
<br>@Temperature 77.0 °F
Complete Cure Cycle
Northstar Polymers MPC-W44A Polyurethane Gel
MPC-W44A is a polyurethane gel formulation specifically designed for padding and cushioning application that requires Shore Durometer OOO scale hardness. Produces good rebound characteristics and g..
Cure Time 4320 min
<br>@Temperature 23.0 °C
72.0 hour
<br>@Temperature 73.4 °F
Aluminum, working strength
Permabond HH131 High Temperature Threadlocker
Permabond® HH131 is a very high temperature resistant, high strength anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. It is used for ..
Cure Time 4320 min
<br>@Temperature 23.0 °C
72.0 hour
<br>@Temperature 73.4 °F
M10 steel, full strength
Permabond LM113 Anaerobic Threadlocker
Permabond® LM113 Threadlocker is a medium viscosity product for locking small threaded fasteners, such as screws and bolts or hydraulic fittings that might require disassembly. Due to its thixotrop..
Cure Time 4320 min
<br>@Temperature 23.0 °C
72.0 hour
<br>@Temperature 73.4 °F
Zinc, working strength
Permabond LM113 Anaerobic Threadlocker
Permabond® LM113 Threadlocker is a medium viscosity product for locking small threaded fasteners, such as screws and bolts or hydraulic fittings that might require disassembly. Due to its thixotrop..
Cure Time 4320 - 5760 min
<br>@Temperature 25.0 °C
72.0 - 96.0 hour
<br>@Temperature 77.0 °F
Complete Cure Cycle
Northstar Polymers SAI-1 Low Viscosity Variable Ratio Polyurethane Gel
SAI-1 is custom formulated polyurethane gel material to yield very soft elastomer gel material from low viscosity components at room temperature. This material is variable mixing ratio so that the ..
Cure Time >= 4320 min
<br>@Temperature 25.0 °C
>= 72.0 hour
<br>@Temperature 77.0 °F
Lord Adhesives HPC-3B Fluoroelastomer Coating
LORD HPC-3B and HPC-3C are two-part, room temperature curing fluoroelastomer coatings which feature robust adhesion and exceptional mechanical properties. These coatings greatly enhance fuel and flu..
Cure Time 4320 min
<br>@Temperature 25.0 °C
72.0 hour
<br>@Temperature 77.0 °F
Tra-Con Tra-Bond 716C01 Medium Viscosity Epoxy Adhesive
TRA-BOND 716C01 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications. This two-part amber adhesive is easily mixed, used and cured at room temperature..
Cure Time 4320 min
<br>@Temperature 25.0 °C
72.0 hour
<br>@Temperature 77.0 °F
Tra-Con Tra-Bond 724-14C Polyurethane Adhesive
TRA-BOND 724-14C premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong, resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, mylar..
Cure Time 4320 min
<br>@Temperature 25.0 °C
72.0 hour
<br>@Temperature 77.0 °F
Tra-Con Tra-Bond 724-20 Polyurethane Adhesive
TRA-BOND 724-20 polyurethane adhesive is designed for good adhesion, providing strong, resilient bonds to a wide variety of substrates including aluminum, solder, nylon, mylar and steel. TRA-BOND 72..
Cure Time 4320 min
<br>@Temperature 25.0 °C
72.0 hour
<br>@Temperature 77.0 °F
Tra-Con Tra-Bond FDA12 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA12 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admin..
Cure Time 4320 min
<br>@Temperature 25.0 °C
72.0 hour
<br>@Temperature 77.0 °F
Tra-Con Tra-Duct 916H02 Room Temperature Cure, Conductive Silver Epoxy Adhesive
TRA-DUCT 916H02 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical pr..
Cure Time 4320 min
<br>@Temperature 23.0 °C
72.0 hour
<br>@Temperature 73.4 °F
Master Bond EP21TDC-2 Highly Flexible Cryogenic Epoxy Compound
Master Bond Polymer System EP21TDC-2 is a two component highly flexible epoxy resin compound for high performance bonding, sealing, coating and encapsulation. It is formulated to cure fully at ambie..
Cure Time 4320 min
<br>@Temperature 25.0 °C
72.0 hour
<br>@Temperature 77.0 °F
Tra-Con Tra-Bond Ablebond 862-2 Room Temperature Cure Epoxy Adhesive
Ablebond 862-2 room temperature curing epoxy adhesive is designed for solder pad encapsulation or sealing the head/disk area in floppy disc assemblies. This resilient compound is suitable for bondin..
Cure Time 4320 min
<br>@Temperature 25.0 °C
72.0 hour
<br>@Temperature 77.0 °F
Tra-Con Tra-Bond FDA12WH01 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA12 WH01 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug ..
Cure Time 4320 min
<br>@Temperature 16.0 °C
72.0 hour
<br>@Temperature 60.8 °F
Full Chemical
Chesterton ARC 858 Abrasion resistant rebuilding and faring composite
An advanced ceramic composite for the repair and protection of all metal surfaces subjected to erosion, corrosion and chemical attack. It is normally applied at a thickness of 0.15 mm (60 mils) or m..
Cure Time 4320 min
<br>@Temperature 10.0 °C
72.0 hour
<br>@Temperature 50.0 °F
Full Load
Chesterton ARC 897 Fine Grade Sliding Wear Compound
Description: ARC 897 is an advanced ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a t..
Cure Time 4320 min
<br>@Temperature 16.0 °C
72.0 hour
<br>@Temperature 60.8 °F
Full Chemical
Chesterton ARC 897 Fine Grade Sliding Wear Compound
Description: ARC 897 is an advanced ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a t..
Cure Time 4320 min
<br>@Temperature 10.0 °C
72.0 hour
<br>@Temperature 50.0 °F
Full Load
Chesterton ARC BX2 Contractor Grade Fine Sliding Wear Compound
Description: ARC BX2 is an advanced contractor grade ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It ..
Cure Time 4320 min
<br>@Temperature 10.0 °C
72.0 hour
<br>@Temperature 50.0 °F
Full Load
Chesterton ARC PW Potable Water Coating
Description: ARC PW is a 100% solids lining certified for NSF/ANSI 61 potable water, cold water service. It is recommended to be applied by brush, roll or spray at 500-750 microns (20-30 mils) total..
Cure Time 4320 - 7200 min
<br>@Temperature 24.0 °C
72.0 - 120 hour
<br>@Temperature 75.2 °F
full cure
BCC Products BC 8990 Polyurethane Elastomer
BC8990 is a two-component urethane elastomer compound specifically designed for general purpose molding and casting of various shapes. This product is a safe, easy-to-handle, room temperature mixing..
Cure Time 4320 min
<br>@Temperature 25.0 °C
72.0 hour
<br>@Temperature 77.0 °F
Atom Adhesives AA-BOND FDA16 Epoxy Adhesive
AA-BOND FDA16 is a medium viscosity epoxy resin system specifically developed for medical device applications. AA-BOND FDA16 has been tested in accordance with USP biological reactivity tests, in vi..
Cure Time 4320 - 7200 min
<br>@Temperature 24.0 °C
72.0 - 120 hour
<br>@Temperature 75.2 °F
full cure
BCC Products BC 8675E Polyurethane Elastomer
BC 8675E is a multi-purpose elastomer that can perform many functions. Typical product features are: easy to use, cures at room temperature, resists moisture absorption, excellent in use for molds f..