| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time |
480
min @Temperature 82.2 °C |
8.00
hour @Temperature 180 °F |
Complete Cure Cycle |
|
Northstar Polymers MSB-D60A High Performance Polyurethane Cast Elastomer System
This is an Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires some lord bearing, high tensile strength, cut/tear res..
|
|||
| Cure Time |
480
-
960
min @Temperature 71.1 - 82.2 °C |
8.00
-
16.0
hour @Temperature 160 - 180 °F |
Complete Cure Cycle |
|
Northstar Polymers MSN-V40A Polyester Base Low-Rebound Impact/Vibration Dampening Gel
This polyurethane casting material is developed for applications that require Shore OO 40 range casting material with vibration dampening property and higher strength than standard polyurethane gel ..
|
|||
| Cure Time |
480
min @Temperature 25.0 °C |
8.00
hour @Temperature 77.0 °F |
De-mold Time |
|
Northstar Polymers GK-7 Low Viscosity Polyurethane Gel Cast
This material is formulated for production of thin polyurethane gel film or parts. The low viscosity property of the mixed component enables the user to cast this into a thin layer without entrappi..
|
|||
| Cure Time |
480
min @Temperature 93.3 °C |
8.00
hour @Temperature 200 °F |
|
|
Lord Adhesives Thermosetâ„¢ LS 213-9 Unfilled Epoxy Encapsulant
Lord LS 213-9 is a one component epoxy coating and impregnating compound featuring low viscosity, good moisture resistance and excellent dielectric properties. Typical applications include transform..
|
|||
| Cure Time |
480
min @Temperature 60.0 °C |
8.00
hour @Temperature 140 °F |
|
|
Tra-Con Tra-Bond 724-17GR Polyurethane Adhesive
TRA-BOND 724-17GR premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, mylar..
|
|||
| Cure Time |
480
min @Temperature 75.0 °C |
8.00
hour @Temperature 167 °F |
|
|
Tra-Con Tra-Bond 832-5 Flexible Epoxy
TRA-BOND 832-5 is a flexible two component epoxy which is intended for bonding materials with mis-matched coefficients of expansion. It exhibits flexibility associated with polyurethanes but does no..
|
|||
| Cure Time |
480
min @Temperature 75.0 °C |
8.00
hour @Temperature 167 °F |
|
|
Tra-Con Tra-Bond 872-7TN1 Flexible Thixotropic Epoxy Adhesive
TRA-BOND 872-7TN1 is a flexible thixotropic epoxy. The high viscosity and long worklife make this material easy to handle. Also, the high thermal conductivity makes this product ideal for electronic..
|
|||
| Cure Time |
480
-
960
min @Temperature 25.0 °C |
8.00
-
16.0
hour @Temperature 77.0 °F |
|
|
Trelleborg Emerson & Cuming Eccobond® 1309 General Purpose Catalyst
Emerson & Cuming 1309 Eccobond® General Purpose CatalystFaster curing version of 9. Very fast room temperature curing, low viscosity, general purpose. Short working life. Imparts excellent chemical..
|
|||
| Cure Time |
480
-
960
min @Temperature 25.0 °C |
8.00
-
16.0
hour @Temperature 77.0 °F |
|
|
Trelleborg Emerson & Cuming Eccobond® 24 LV General Purpose Catalyst
Emerson & Cuming 24 LV Eccobond® General Purpose CatalystFaster curing, shorter working life version of 23 LV. Recommended for small mass castings due to higher exotherm. Cure Type: Room Temp or He..
|
|||
| Cure Time |
480
min @Temperature 25.0 °C |
8.00
hour @Temperature 77.0 °F |
|
|
Tra-Con Tra-Bond 868-3N1 Room Temperature Cure Adhesive
TRA-BOND 868-3N1 room temperature cure adhesive provides strong bonds to difficult-to-bond metals, such as gold, silver, copper, brass, and solder.Information provided by Tra-Con Inc.
|
|||
| Cure Time |
480
min @Temperature 4.00 °C |
8.00
hour @Temperature 39.2 °F |
Full Chemical |
|
Chesterton ARC 5 Paste grade Rapid Cure Abrasion Control
Description: ARC 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patc..
|
|||
| Cure Time |
480
min @Temperature 25.0 °C |
8.00
hour @Temperature 77.0 °F |
Light Load |
|
Chesterton ARC 890 Course Grade Sliding Wear Compound
An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at the thickness of 6 mm (1/4”)..
|
|||
| Cure Time |
480
min @Temperature 25.0 °C |
8.00
hour @Temperature 77.0 °F |
Light Load |
|
Chesterton ARC 897 Fine Grade Sliding Wear Compound
Description: ARC 897 is an advanced ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a t..
|
|||
| Cure Time |
480
min @Temperature 25.0 °C |
8.00
hour @Temperature 77.0 °F |
Tack Free |
|
Chesterton ARC 982 100% Novolac acid resistant coating
Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. A low viscosity composite that is applied by brush, squeegee, or a plural compo..
|
|||
| Cure Time |
480
min @Temperature 16.0 °C |
8.00
hour @Temperature 60.8 °F |
Light Load |
|
Chesterton ARC 988 Composite
Description: A high performance, quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by severe chemical and physi..
|
|||
| Cure Time |
480
min @Temperature 25.0 °C |
8.00
hour @Temperature 77.0 °F |
Light Load |
|
Chesterton ARC BX2 Contractor Grade Fine Sliding Wear Compound
Description: ARC BX2 is an advanced contractor grade ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It ..
|
|||
| Cure Time |
480
min @Temperature 10.0 °C |
8.00
hour @Temperature 50.0 °F |
Full Load |
|
Chesterton ARC NVE SYSTEM Vinyl Ester Lining
Description: ARC NVE is a high performance, quartz reinforced, three-component, modified novolac vinyl ester lining capable of being applied to horizontal and vertical surfaces. The NVE system kit i..
|
|||
| Cure Time |
480
min @Temperature 10.0 °C |
8.00
hour @Temperature 50.0 °F |
Tack Free |
|
Chesterton ARC S1 General purpose coating
Description: An advanced polymer composite formulated to protect metal surfaces from corrosion and chmical attack. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrink..
|
|||
| Cure Time |
480
min @Temperature 25.0 °C |
8.00
hour @Temperature 77.0 °F |
Light Load |
|
Chesterton ARC MX2 High Wear Fine Particle Wear Compound
Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion and chemical attack. It is applied at a thickness of 3 mm (1/8”..
|
|||
| Cure Time |
480
-
660
min @Temperature 22.0 °C |
8.00
-
11.0
hour @Temperature 71.6 °F |
|
|
Dow Corning 3-4241 DIELECTRIC TOUGH GEL KIT
Two-part, translucent green, RT or heat cure, UV indicator, long working time, tough primerless chemical adhesion, UL 94 V-1 flammability classification.Information provided by Dow Corning
|
|||
| Cure Time |
480
min @Temperature 5.00 °C |
8.00
hour @Temperature 41.0 °F |
Dry to Handle Time; ASTM D1640 clause 7.7.1 |
|
3M Scotchkote™ 323 Purple Patch Compound
3M Scotchkote 323 Purple Patch Compound is an ambient temperature cure, two-part system designed to protect metal, concrete and other surfaces from corrosion and deterioration. Scotchkote 323 Purple..
|
|||
| Cure Time |
480
-
720
min @Temperature 24.0 °C |
8.00
-
12.0
hour @Temperature 75.2 °F |
demold time |
|
BCC Products BC 8880 Polyurethane Elastomer Surface Coat
BC8880 is a two-part urethane gel coat which exhibits excellent handling characteristics and very low moisture sensitivity. Its characteristics include a high modulus and a high hardness. It is a br..
|
|||
| Cure Time |
480
min @Temperature 24.0 °C |
8.00
hour @Temperature 75.2 °F |
handling time |
|
BCC Products BC 9020 Silicone RTV Rubber
BC 9020 is a violet colored, two-component, flowable compound that regardless of thickness or confinement, cures at room temperature. The cured rubber is high strength and high tear with good elonga..
|
|||
| Cure Time |
480
min @Temperature 149 °C |
8.00
hour @Temperature 300 °F |
Alternate |
|
Aremco Aremco-Bond™ 2335 Ultra High Temperature Epoxy
Ceramic-Filled, Low Expansion, High Lap-Shear Strength & Chemical Resistance, Low Outgassing.
|
|||
| Cure Time |
480
min @Temperature 60.0 °C |
8.00
hour @Temperature 140 °F |
|
|
Tra-Con Tra-Bond 724-17GR1B3 Polyurethane Adhesive
TRA-BOND 724-17GR1B3 premixed and frozen polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, myl..
|
|||
| Cure Time |
480
-
840
min @Temperature 24.0 °C |
8.00
-
14.0
hour @Temperature 75.2 °F |
demold time |
|
BCC Products BC 8675E Polyurethane Elastomer
BC 8675E is a multi-purpose elastomer that can perform many functions. Typical product features are: easy to use, cures at room temperature, resists moisture absorption, excellent in use for molds f..
|
|||
| Cure Time |
480
min @Temperature 10.0 °C |
8.00
hour @Temperature 50.0 °F |
Full Load |
|
Chesterton ARC NVE VC Vinyl Ester Sealer
Description: ARC NVE VC (Veil Coat) is a two-component, modified epoxy novolac vinyl ester sealer coat formulated for application by brush, roller or spray at 0.15-0.25 mm (0.07-0.010”) wet film th..
|
|||
| Cure Time |
480
min @Temperature 43.0 °C |
8.00
hour @Temperature 109 °F |
Light Load |
|
Chesterton ARC S1HB Sprayable high-viscosity, 100% solids, advanced coating
An advanced composite formulated to protect concrete and metal surfaces from corrosion and chemical attack. It is normally applied at a thickness of 1-2 mm (40-80 mils) per coat. However, greater si..
|
|||