Processing Properties Metric English Comments
Cure Time 240 - 360 min
<br>@Temperature 45.0 °C
4.00 - 6.00 hour
<br>@Temperature 113 °F
Resinlab® EP1285HD-9 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
Cure Time 180 - 360 min
<br>@Temperature 25.0 °C
3.00 - 6.00 hour
<br>@Temperature 77.0 °F
De-mold Time
Northstar Polymers MCP-V40A Polyurethane Gel
MCP-V40A is a polyurethane gel formulation specifically designed for padding and cushioning applications, where low rebound property of the material is critical. This viscoelastic polymer is a two..
Cure Time 180 - 360 min
<br>@Temperature 25.0 °C
3.00 - 6.00 hour
<br>@Temperature 77.0 °F
De-mold Time
Northstar Polymers MPC-W44A Polyurethane Gel
MPC-W44A is a polyurethane gel formulation specifically designed for padding and cushioning application that requires Shore Durometer OOO scale hardness. Produces good rebound characteristics and g..
Cure Time 240 - 360 min
<br>@Temperature 25.0 °C
4.00 - 6.00 hour
<br>@Temperature 77.0 °F
De-mold Time
Northstar Polymers MPP-A60A Liquid Castable Polyurethane
MPP-A60A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott..
Cure Time 180 - 360 min
<br>@Temperature 23.0 °C
3.00 - 6.00 hour
<br>@Temperature 73.4 °F
M10 steel, working strength
Permabond HH131 High Temperature Threadlocker
Permabond® HH131 is a very high temperature resistant, high strength anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. It is used for ..
Cure Time 180 - 360 min
<br>@Temperature 23.0 °C
3.00 - 6.00 hour
<br>@Temperature 73.4 °F
M10 steel, working strength
Permabond HH167 Anaerobic Retainer
Permabond® HH167 is a high viscosity gap filling silver paste, which can be used for repairing metal machinery parts. It is ideal for repairing worn shafts, broken threads, damaged keyways and spli..
Cure Time 180 - 360 min
<br>@Temperature 23.0 °C
3.00 - 6.00 hour
<br>@Temperature 73.4 °F
Zinc, working strength
Permabond HH190 Anaerobic Gasketmaker
Permabond® HH190 Gasketmaker is an anaerobic curing flange sealant that can replace, or be used as a dressing for, conventional pre-cut gaskets. Since HH190 is a flowable paste, it conforms to the ..
Cure Time 180 - 360 min
<br>@Temperature 23.0 °C
3.00 - 6.00 hour
<br>@Temperature 73.4 °F
Zinc, working strength
Permabond HM129 Anaerobic Threadlocker
Permabond® HM129 is a high strength medium viscosity anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. Cure is fast and reliable on st..
Cure Time 180 - 360 min
<br>@Temperature 23.0 °C
3.00 - 6.00 hour
<br>@Temperature 73.4 °F
Zinc, working strength
Permabond HM160 Anaerobic Retaining Compound
Permabond® HM160 is a medium viscosity liquid adhesive that cures when confined between metal parts to form a tough, hard plastic. In the uncured, liquid state, the adhesive wets the metal surfaces..
Cure Time 180 - 360 min
<br>@Temperature 23.0 °C
3.00 - 6.00 hour
<br>@Temperature 73.4 °F
M10 steel, working strength
Permabond HM165 Anaerobic Retainer
Permabond® HM165 is a high viscosity anaerobic retaining compound that cures when confined between metal parts to form a tough bond. It is best suited for cylindrical parts and where high temperatu..
Cure Time 180 - 360 min
<br>@Temperature 23.0 °C
3.00 - 6.00 hour
<br>@Temperature 73.4 °F
Brass, working strength
Permabond LH050 Anaerobic Threadsealant
Permabond® LH050 pipe sealant with PTFE is a general purpose pipe sealant that provides instant air pressure seal up to 1000 psi with limited hand tightening. After cure, the sealing capability is ..
Cure Time 180 - 360 min
<br>@Temperature 23.0 °C
3.00 - 6.00 hour
<br>@Temperature 73.4 °F
Brass, working strength
Permabond LH150 Anaerobic Threadsealant
Permabond® LH150 Pipe Sealant with PTFE is designed for sealing and locking tapered metal pipe threads and fittings. It is ideal for stainless steel and other passive metals. Instant sealing of up ..
Cure Time 180 - 360 min
<br>@Temperature 23.0 °C
3.00 - 6.00 hour
<br>@Temperature 73.4 °F
M10 steel, working strength
Permabond LH150 Anaerobic Threadsealant
Permabond® LH150 Pipe Sealant with PTFE is designed for sealing and locking tapered metal pipe threads and fittings. It is ideal for stainless steel and other passive metals. Instant sealing of up ..
Cure Time 180 - 360 min
<br>@Temperature 23.0 °C
3.00 - 6.00 hour
<br>@Temperature 73.4 °F
M10 steel, working strength
Permabond LH197 Anaerobic Gasketmaker
Permabond® LH197 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is highly flexible, making it ideal for dissimilar surfaces where differential th..
Cure Time 300 - 360 min
<br>@Temperature 25.0 °C
5.00 - 6.00 hour
<br>@Temperature 77.0 °F
De-mold Time
Northstar Polymers MPP-A80E High Performance Polyether
This high performance polyether system is one of a family of polymer systems developed by Northstar Polymers for specific demanding work environments. Urethane elastomers molded with this system ex..
Cure Time 180 - 360 min
<br>@Temperature 23.0 °C
3.00 - 6.00 hour
<br>@Temperature 73.4 °F
M10 steel, working strength
Permabond MH199 Anaerobic Gasketmaker
Permabond® MH199 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets, thereby offering po..
Cure Time 240 - 360 min
<br>@Temperature 149 - 160 °C
4.00 - 6.00 hour
<br>@Temperature 300 - 320 °F
second, Post cure for and additional 4-8 hours at 350-375°F
Master Bond EP112M Two Component, Medium Viscosity Heat Curing Cycloaliphatic Epoxy Resin
Product Description: Master Bond Polymer System EP112M is a solventless, medium viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor ..
Cure Time 240 - 360 min
<br>@Temperature 93.3 °C
4.00 - 6.00 hour
<br>@Temperature 200 °F
Master Bond EP29LP Low Exotherm, Low Viscosity Two Component Epoxy System
Master Bond Polymer System EP29LP is a two component high performance epoxy resin system featuring low viscosity, long pot life and low exotherm. As an adhesive this versatile material will form bon..
Cure Time 240 - 360 min
<br>@Temperature 93.3 °C
4.00 - 6.00 hour
<br>@Temperature 200 °F
Master Bond EP37-3 Optically Clear, Impact Resistant Two Component Epoxy
Master Bond Polymer System EP37-3 is a low viscosity, resilient, optically clear two component epoxy resin system designed for high performance bonding, coating and casting applications. As an adhes..
Cure Time 240 - 360 min
<br>@Temperature 65.6 °C
4.00 - 6.00 hour
<br>@Temperature 150 °F
At 150°F
Master Bond EP62-1 High Glass Transition Temperature Epoxy System
Master Bond EP62-1 is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. The cured epoxy resin ex..
Cure Time 240 - 360 min
<br>@Temperature 60.0 - 70.0 °C
4.00 - 6.00 hour
<br>@Temperature 140 - 158 °F
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System
Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi..
Cure Time 240 - 360 min
<br>@Temperature 25.0 °C
4.00 - 6.00 hour
<br>@Temperature 77.0 °F
Tra-Con Tra-Bond 2106 Fast Cure, Medium Viscosity Epoxy Adhesive
TRA-BOND 2106 is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This clear, two-part, medium viscosity syste..
Cure Time 240 - 360 min
<br>@Temperature 25.0 °C
4.00 - 6.00 hour
<br>@Temperature 77.0 °F
Tra-Con Tra-Bond 2106T Fast Cure Thixotropic Epoxy Adhesive
TRA-BOND 2106T is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This versatile two-part epoxy system contai..
Cure Time 240 - 360 min
<br>@Temperature 25.0 °C
4.00 - 6.00 hour
<br>@Temperature 77.0 °F
Tra-Con Tra-Bond 216R01 Fire Retardant Epoxy
TRA-BOND 216R01 is a fast curing material with a set time of 5 to 7 minutes. Samples tested were certified to the requirements of UL94 V-O, and is RoHS compliant. TRA-BOND 216R01 develops significa..
Cure Time 240 - 360 min
<br>@Temperature 100 °C
4.00 - 6.00 hour
<br>@Temperature 212 °F
Cytec EN-2550 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
Cure Time 240 - 360 min
<br>@Temperature 80.0 °C
4.00 - 6.00 hour
<br>@Temperature 176 °F
Cytec EN-9 (Conap) Casting, Potting, and Molding Compound
High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable..
Cure Time 60.0 - 360 min
<br>@Temperature 80.0 - 110 °C
1.00 - 6.00 hour
<br>@Temperature 176 - 230 °F
optional 3rd step
Abatron AboCast 8502-5/AboCure 8502-5 Colorless, Low-Exotherm Epoxy Casting Compound
AboCast 8502-5/AboCure 8502-5 is a rigid, colorless, low-exotherm epoxy casting compound for spherical masses up to 500 grams. It is a 2-component structural and dielectric liquid system with extrem..
Cure Time 60.0 - 360 min
<br>@Temperature 80.0 °C
1.00 - 6.00 hour
<br>@Temperature 176 °F
optional 3rd step
Abatron AboCast 8502-6/AboCure 8502-6 Colorless, Low-Exotherm Epoxy Casting Compound
AboCast 8502-6/AboCure 8502-6 is a flexible, colorless, low-exotherm epoxy casting compound for spherical masses up to 2000 grams. It is a 2-component structural and dielectric liquid system with lo..
Cure Time 300 - 360 min
<br>@Temperature 150 °C
5.00 - 6.00 hour
<br>@Temperature 302 °F
Abatron AboWeld 8708-5 One-Component Structural/Dielectric Epoxy
AboWeld 8708-5 is a highly filled, class H (180°C) structural, heat-conductive adhesive paste for SLOW high-temperature curing. Suggested Uses: Structural bonding; Casting; Potting; Encapsulating;..
Cure Time 240 - 360 min
<br>@Temperature 65.0 °C
4.00 - 6.00 hour
<br>@Temperature 149 °F
Atom Adhesives AA-BOND 428 Epoxy Adhesive
AA-BOND 428 is a two part, heat-resistant and low exotherm, epoxy adhesive formulation. It is a 100% solid epoxy adhesive, with superior chemical resistance and shear strength. AA-BOND 428 contains ..
Copyright © lookpolymers.com All Rights Reserved