| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 190 °C | 374 °F | |
|
Multibase TPSiV™ 3010-60A Thermoplastic Silicone Vulcanizate
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced..
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | |
|
Multibase TPSiV™ 3011-50A Thermoplastic Silicone Vulcanizate
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced..
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | Zone 6; Cylinder |
|
Premix Thermoplastics PRE-ELEC® ESD 7120
PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject..
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | Zone 5; Cylinder |
|
Premix Thermoplastics PRE-ELEC® ESD 7120
PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject..
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | Zone 2; Cylinder |
|
Premix Thermoplastics PRE-ELEC® ESD 7120
PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject..
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | Zone 3; Cylinder |
|
Premix Thermoplastics PRE-ELEC® CP 1316
(discontinued **)
PRE-ELEC CP 1316 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resis..
|
|||
| Middle Barrel Temperature | 190 - 220 °C | 374 - 428 °F | Start Point: 205°C |
|
Kingfa FW-620 Flame Retardant ABS
Features:UL 94 V-0 @ 1.5-3.0mmWeather resistanceHeat resistanceGood surfaceApplications:Injection moldingOA deviceChargerTransformerInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Middle Barrel Temperature | 190 - 220 °C | 374 - 428 °F | Start Point: 205°C |
|
Kingfa FW-650 Flame Retardant ABS
Features:Weather resistanceSuper high impact resistanceApplications:Injection moldingSwitchSocketInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical HF380I ABS, High Flow
Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical HF380NS ABS, High Flow, General Anti-Static
Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical HF380XC ABS, High Flow, High Surface Gloss
Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres..
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical HI100 ABS, High Impact
Feature: Injection Molding, High ImpactApplication: Helmet, Pipe & Fittings, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical HI100X ABS, High Impact, Semi-Transparency, Flexible
Feature: Injection Molding, High Impact, Semi-Transparency, FlexibleApplication: Artificial Nails, Miscellaneous Goods)CAS No. 9010-94-0Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 190 - 200 °C | 374 - 392 °F | Injection Molding |
|
LG Chemical HIPS 405AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 158725-44-1 and 1309-64-4Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | |
|
LG Chemical LUCEL EC-610B Electrically Conductive POM, 10% Carbon Black Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Middle Barrel Temperature | 190 - 260 °C | 374 - 500 °F | Injection |
|
Inno-Comp INNOPOL® CS 1-7120 AP 20% Talc Filled Polypropylene Homopolymer
INNOPOL® CS 1-7120 is a 20 % talc-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-7120 is recommended for extrusion of sheet..
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical SG175NS ABS, Super Surface Gloss, General Anti-Static
Feature: Injection Molding, Super Surface Gloss, General Anti-StaticApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | Compress zone |
|
Taiwan PU Corporation TPU-B95 General Grade, Blow Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Blow MoldingInformation provided by Taiwan PU Corporation.
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | Compress zone |
|
Taiwan PU Corporation TPUI-H95 High Hydrolysis Resistance, Injection Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Injection MoldingInformation provided by Taiwan PU Corporation.
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | |
|
SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
|
|||
| Middle Barrel Temperature | 190 - 230 °C | 374 - 446 °F | cylinder |
|
Borealis BEC5012 Polypropylene Block Copolymer for Non-Pressure Pipes
BEC5012 is a high molecular weight, low flow rate polypropylene block copolymer with very high impact strength. Applications: BEC5012 is recommended for non-pressure pipes and fittings, structured..
|
|||
| Middle Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
|
Borealis BL2571 High Density Polyethylene
BL2571 is a high-density polyethylene with high stiffness and high environmental stress crack resistance. This product is intended for blow molding. Applications: household and chemical containers..
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Mid-2. Region Temperature |
|
Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Middle Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
|
Borealis RB607MO Polypropylene Random Copolymer
RB607MO is a random copolymer for blow molding, with good transparency and contact clarity, very good gloss and surface finish. Bottles up to 2 liters can be steam sterilized due to heat distortion ..
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Mid-2. Region Temperature |
|
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Middle Barrel Temperature | 190 - 250 °C | 374 - 482 °F | |
|
Diamond Polymers ABS 3003MC Black 1722
Description: BlackInformation provided by Diamond Polymers, Inc.
|
|||