| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
|
PTS POM-270 27.0 MFI Acetal Copolymer
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Middle Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
|
Huntsman AVALON® 98 AE Thermoplastic Polyurethane
Introduction: AVALON 98 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 98 AE is part of the AVALON Perform Range and offers a premium soiling materi..
|
|||
| Middle Barrel Temperature | 160 - 200 °C | 320 - 392 °F | Extrusion |
|
Huntsman IROGRAN® A 85 P 5350 TPU-Polyester
Introduction: IROGRAN A 85 P 5350 is a flame-retardant, halogen-free, polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 5350 is par..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical ALPHALAC SG910 HIPS
High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical ALPHALAC SG970 HIPS
Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical HIPS 60HRI PS, Impact Modified
Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
|
LG Chemical LUCEL FW-710F Friction and Wear Resistant POM, PTEE filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
|
LG Chemical LUCEL N109-02 General Purpose POM, Unreinforced, Externally Lubricated, Standard Viscosity
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
|
LG Chemical LUCEL N115 POM, Unreinforced, High Viscosity
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
|
LG Chemical LUCEL N127-02 General Purpose POM, Unreinforced, Externally Lubricated, High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
|
LG Chemical LUCEL ST-550 Ultra High Impact POM, Unreinforced
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
|
LG Chemical LUCEL VC-145 Antistatic POM, Unreinforced, Ultra High Flow, For VCR Reels
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
|
|||
| Middle Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
|
Huntsman AVALON® 85 AE Thermoplastic Polyurethane
Introduction: AVALON 85 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 85 AE is part of the AVALON Perform Range and offers a premium soiling materi..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
Stellarchem 475-860N TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
Stellarchem AB760LG TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Transition, Extrusion |
|
Stellarchem AB835EM TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Transition, Extrusion |
|
Stellarchem AB860EM TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
Stellarchem AB-860LG TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Transition, Extrusion |
|
Stellarchem AB-860LG TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
Stellarchem AB870LG TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
Stellarchem GP-9401 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Transition, Extrusion |
|
Stellarchem GP-9401 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
Stellarchem GP-945 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
Stellarchem MP-8001 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
Stellarchem MP-950NC TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Middle Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
|
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS
VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Middle Barrel Temperature | 170 - 200 °C | 338 - 392 °F | |
|
Sumitomo Chemical ESPOLEX® WT318 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | |
|
Unitika TERRAMAC TE-7300 Polylactic Acid (PLA)
Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
|
|||
| Middle Barrel Temperature | 170 - 200 °C | 338 - 392 °F | |
|
Elastron® G SEBS Elastomer
Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureshigh temperature resistanceelectrical insulator with v..
|
|||
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow
Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical
|
|||