Polymer Property : Middle Barrel Temperature = 204 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
Multibase Multi-Pro® 2006 T Polypropylene
Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
Multibase Multi-Pro® 4006 TH Polypropylene
Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: ConnectorsElectrical/Electronic ApplicationsAppliancesInformation provided by Multibase
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products F4702-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Exterior door moldingsRigid bumper coversInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products G20P100-00 20% Glass Fiber Reinforced Polypropylene, Natural
Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products HP800-706UV 20% Talc Reinforced High Performance Polypropylene Copolymer, Scratch Resistant, UV Stabilized, Impact Modified, SWB White
Applications: Interior trim/Instrument panel componentsA/B pillarsGlove box doorsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products RCT120-01 20% Talc Reinforced Polypropylene, Black, Recycled Content
Applications: HVAC and I/P ComponentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products T20P100-00 20% Talc Reinforced Polypropylene, Natural
Applications: Electronic housingsConsolesIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products..
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products T20P100-00UV 20% Talc Reinforced Polypropylene, UV Stabilized, Natural
Applications: Electronic housingsConsolesIP componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 204 - 216 °C
400 - 420 °F
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products T20P250-01 20% Talc Reinforced Polypropylene Copolymer, Black
Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products T20P252-00 20% Talc Reinforced Polypropylene, Natural
Applications: IP Structural componentsGlove box binWire troughInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 204 - 216 °C
400 - 420 °F
PlastiComp Complet® LGF30 - PP Homopolymer Polypropylene, 30% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% long glass fiber reinforcementInformation provided by PlastiCom..
Middle Barrel Temperature 204 - 227 °C
400 - 440 °F
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade
General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam..
Middle Barrel Temperature 204 - 221 °C
400 - 430 °F
Ravago Manufacturing Americas Hylac® GP74G30 ABS, 30% Glass Fiber Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Middle Barrel Temperature 204 °C
400 °F
PTS Trilac® ABS-EX1000 High Impact Extrusion Grade ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products HP505-01 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black
Applications: Glove box binConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products HP506-01 20% Talc Reinforced High Performance Polypropylene, Black
Applications: Underhood componentsLamp housingsHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products HP531-01UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: IP structural componentsAir ducts - distributionA/B/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 204 °C
400 °F
PTS Trilac® FR1 ABS- Flame Retardant ABS Resin  (Unverified Data**)
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 204 - 227 °C
400 - 440 °F
Fiberfil® J-60/20/H Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Middle Barrel Temperature 204 - 227 °C
400 - 440 °F
Fiberfil® J-60/30 Polypropylene Homopolymer, 30% Glass Reinforced
Information provided by FIBERFIL Engineered Plastics
Middle Barrel Temperature 204 - 227 °C
400 - 440 °F
Fiberfil® J-60/30/F Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Middle Barrel Temperature 204 - 227 °C
400 - 440 °F
Fiberfil® M-2450 Polypropylene Copolymer
Information provided by FIBERFIL Engineered Plastics
Middle Barrel Temperature 204 - 227 °C
400 - 440 °F
Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled
Information provided by FIBERFIL Engineered Plastics
Middle Barrel Temperature 204 - 227 °C
400 - 440 °F
Fiberfil® J-60/20/E8/M Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Middle Barrel Temperature 204 - 227 °C
400 - 440 °F
Fiberfil® PP-60/CC/20 Polypropylene Homopolymer, 20% Calcium Carbonate
Information provided by FIBERFIL Engineered Plastics
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
Star Plastics ABS9020 Molding Grade ABS
Information provided by Star Plastics, Inc.
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products GC20P255-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: BracketsUnderhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 204 - 232 °C
400 - 450 °F
RheTech Products GC20P105-08FA 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black
Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products.