Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Middle Barrel Temperature = 220 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Middle Barrel Temperature 220 °C
428 °F
Zone 3; Cylinder
Premix Thermoplastics PRE-ELEC® ABS 1410
PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141..
Middle Barrel Temperature 220 °C
428 °F
Zone 5; Cylinder
Premix Thermoplastics PRE-ELEC® PET 1451
PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14..
Middle Barrel Temperature 220 °C
428 °F
Zone 2; Cylinder
Premix Thermoplastics PRE-ELEC® PET 1451
PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14..
Middle Barrel Temperature 220 °C
428 °F
Gichem GILAC E200 Acrylonitrile Butadiene Styrene  (discontinued **)
ABS medium fluidity, excellent resilience. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico
Middle Barrel Temperature 220 °C
428 °F
Gichem GILAC D160/MT Acrylonitrile Butadiene Styrene  (discontinued **)
ABS with good resilience, good thermal properties. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico
Middle Barrel Temperature 220 °C
428 °F
Gichem GILAC C120/T Acrylonitrile Butadiene Styrene  (discontinued **)
ABS with excellent thermal properties. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico
Middle Barrel Temperature 220 °C
428 °F
Gichem GILAC A070V3C Acrylonitrile Butadiene Styrene  (discontinued **)
ABS glass fiber filled, excellent mechanical properties. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico
Middle Barrel Temperature 220 °C
428 °F
DuPont Bynel® 39E622 Adhesive Resin  (discontinued **)
Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Middle Barrel Temperature 220 °C
428 °F
For coextrusion with EVA or EVOH.
DuPont Bynel® 41E623 Adhesive Resin  (discontinued **)
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
Middle Barrel Temperature 220 °C
428 °F
Extrusion Coating
DuPont Appeel® LSR11N704 Lidding Sealant Resin  (discontinued **)
Appeel® 11N704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable seal..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Start Point: 225°C
Kingfa JH950-502 Low-temperature Resistant & Flame Retardant PC/ABS Alloy
Features:UL V-0 @ 3.2mmExcellent balance propertiesGood low temperature resistanceGood normal/low temperature impact strengthGood surfaceApplications:ControllerPlugSocketShell of ammeterInformation ..
Middle Barrel Temperature 220 - 250 °C
428 - 482 °F
Start Point: 235°C
Kingfa MAC-851 PC/ABS Alloy
Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical ..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical LUPOS HR2207A ABS+GF20%, General Purpose, Heat Resistance
Feature: Injection Molding, ABS+GF20%, General Purpose, Heat ResistanceApplication: Electric & Electronic (Housing, Components)Information provided by LG Chemical
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
LG Chemical LUPOS HR-2307 Heat Resistant SAN, 30% Glass Fiber Reinforced
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Injection Molding
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose
Feature: Injection Molding, ABS+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Samsung Cheil Industries Starex® SR-0310 Heat Resistant Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Samyang Tribit® 1503S Polybutylene Terephthalate
Characteristics:High impactApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samyang
Middle Barrel Temperature 220 °C
428 °F
For coextrusion with EVA or EVOH.
DuPont Bynel® 41E687 Adhesive Resin
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
Middle Barrel Temperature 220 °C
428 °F
Extrusion lamination
DuPont Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer
Elvaloy® 3117 AC is intended for coextrusion and compounding. Due to its high melt flow rate, it is used also in extrusion coating. Elvaloy® 3117 AC is soft, flexible and has good adhesion to va..
Middle Barrel Temperature 220 °C
428 °F
Extrusion lamination
DuPont Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer
Elvaloy® 3217 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3217 AC has been developed for film applications requiring a combination of softness, toughness and low friction. Typi..
Middle Barrel Temperature 220 °C
428 °F
Extrusion lamination
DuPont Elvaloy® 3427 AC Ethylene and 27% Butyl Acrylate Copolymer
Elvaloy® 3427 AC can be used for coextrusion and compounding. It can also be used in extrusion coating. Elvaloy® 3427 AC is very soft and flexible, and has good adhesion to various polymers. It..
Middle Barrel Temperature 220 - 250 °C
428 - 482 °F
Mid-2. Region Temperature
Tisan TISESTER® Flame Retardant (V0). Heat Stabilized Polybutylene Terephthalate
TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Mid-2. Region Temperature
Tisan TISLAMID® 6 20% Glass Fiber Reinforced, Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Mid-2. Region Temperature
Tisan TISLAMID® 6 Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Middle Barrel Temperature 220 - 240 °C
428 - 464 °F
Pipe Extrusion
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Middle Barrel Temperature 220 °C
428 °F
For coextrusion with EVA or EVOH.
DuPont Bynel® 41E712 Adhesive Resin  (discontinued **)
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
Middle Barrel Temperature 220 °C
428 °F
Extrusion lamination
DuPont Elvaloy® 3108 AC Ethylene and 7% Butyl Acrylate Copolymer  (discontinued **)
Elvaloy® 3108 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3108 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag..
Copyright © lookpolymers.com All Rights Reserved