| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
|
Polymer Resources PC/ABS-FR1-[color]-3 PC Blend, Flame Retardant, Standard Flow, UV Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
|
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant
PC/ABS Alloy, Flame Retardant, Standard Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info..
|
|||
| Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
|
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow
PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b..
|
|||
| Middle Barrel Temperature | 232 - 277 °C | 450 - 530 °F | |
|
Polymer Resources PPX-MF-FR1 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha..
|
|||
| Middle Barrel Temperature | 232 - 249 °C | 450 - 480 °F | |
|
Polymer Resources PC/TP-GP3 PC/Polyester Alloy
High Impact, Superior Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
|
|||
| Middle Barrel Temperature | 232 °C | 450 °F | |
|
LyondellBasell Alathon® M6138 High Density Polyethylene
ApplicationsALATHON M 6138, formerly known as XM 6138, is a high density polyethylene resin for use in injection molding applications. This resin exhibits good impact resistance and high stiffness...
|
|||
| Middle Barrel Temperature | 232 - 266 °C | 450 - 511 °F | Injection Molding |
|
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
|
|||
| Middle Barrel Temperature | 232 - 277 °C | 450 - 530 °F | |
|
Wellman Wellamid® 42LH XE-N Unfilled Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc.
|
|||
| Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
|
Diamond Polymers ASA S310
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Impact and ModulusInformation provided by Diamond Polymers, Inc.
|
|||
| Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
|
Diamond Polymers ASA S319
Description: ASA Weatherable Polymer, Injection Molding Grade, High ModulusInformation provided by Diamond Polymers, Inc.
|
|||
| Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
|
Diamond Polymers ASA S510
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
|
Diamond Polymers ASA S519
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
|
Diamond Polymers ASA TW-18B2
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
|
Diamond Polymers ASA TW-20
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
|
Diamond Polymers ASA TW-23V
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
|
Diamond Polymers ASA/PC TA-35
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Middle Barrel Temperature | 232 - 266 °C | 450 - 510 °F | |
|
Diamond Polymers ASA TWP 502
Description: Transparent Weatherable PolymerInformation provided by Diamond Polymers, Inc.
|
|||
| Middle Barrel Temperature | 232 - 277 °C | 450 - 530 °F | |
|
Polymer Resources PPX-MF-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F, Mineral Reinforced
(Unverified Da
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||