| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
|
Polymer Resources NY6-GP1 General Purpose Nylon 6
General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry ..
|
|||
| Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
|
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized
General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade..
|
|||
| Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
|
Polymer Resources NY6-GP1-[color]H Nylon, General Purpose, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
|
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated
General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry ..
|
|||
| Middle Barrel Temperature | >= 238 °C | >= 460 °F | |
|
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade
Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct..
|
|||
| Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
|
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant
Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided..
|
|||
| Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
|
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks
Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam..
|
|||
| Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
|
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow
Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat..
|
|||
| Middle Barrel Temperature | 238 - 260 °C | 460 - 500 °F | |
|
Ravago Manufacturing Americas Hybrid S464LGUV Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America UV Stabilizer Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color:..
|
|||
| Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
|
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
|
Polymer Resources NY6-IM1 Nylon 6, Impact Modified
Nylon 6, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (..
|
|||
| Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
|
Polymer Resources NY6-IM1-[color]-H Nylon 6, Impact Modified, Heat Stabilized
Nylon 6, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad..
|
|||
| Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
|
Polymer Resources NY6-IM1-[color]H Nylon, Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Middle Barrel Temperature | 238 - 249 °C | 460 - 480 °F | |
|
Firestone C200-001 Nylon 6
Natural color. Not heat stabilized, modified, or lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone
|
|||
| Middle Barrel Temperature | 238 - 249 °C | 460 - 480 °F | |
|
Firestone C212-15C Nylon 6, Heat Stabilized
Off white color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone
|
|||
| Middle Barrel Temperature | 238 - 249 °C | 460 - 480 °F | |
|
Firestone CR212-203-D Nylon 6, Heat Stabilized
Black color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3 mm.Information provided by Firestone
|
|||
| Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
|
LTL Color Compounds ColorFast® FRPBT200 PBT, Flame Retarded
V-0 rated, unfilled PBTAll information provided by LTL Color Compounders, Inc.
|
|||
| Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
|
LTL Color Compounds ColorFast® FRPBT210 PBT, Flame Retarded, Impact Modified
V-0 rated, impact modified unfilled PBTAll information provided by LTL Color Compounders, Inc.
|
|||
| Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
|
LTL Color Compounds ColorFast® PBT100 PBT
General purpose injection molding grade unfilled PBT with lubeAll information provided by LTL Color Compounders, Inc.
|
|||
| Middle Barrel Temperature | 238 °C | 460 °F | |
|
MTI ThermoStran® PP-30C Long Carbon Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
|
|||
| Middle Barrel Temperature | 238 °C | 460 °F | |
|
MTI ThermoStran® PP-30G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
|
|||
| Middle Barrel Temperature | 238 °C | 460 °F | |
|
MTI ThermoStran® PP-40G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
|
|||
| Middle Barrel Temperature | 238 °C | 460 °F | |
|
MTI ThermoStran® PP-50G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
|
|||
| Middle Barrel Temperature | 238 °C | 460 °F | |
|
MTI ThermoStran® TPU-40G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
|
|||
| Middle Barrel Temperature | 238 °C | 460 °F | |
|
MTI ThermoStran® TPU-50G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
|
|||
| Middle Barrel Temperature | 238 - 249 °C | 460 - 480 °F | |
|
Entec Hylox® 9030 PBT, 30% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
|
|||
| Middle Barrel Temperature | 238 - 257 °C | 460 - 495 °F | |
|
Diamond Polymers ASA/PC FA-30
Description: ASA Weatherable Polymer, Injection Molding Grade, Flame RetardantInformation provided by Diamond Polymers, Inc.
|
|||
| Middle Barrel Temperature | 238 - 249 °C | 460 - 480 °F | |
|
Entec Hylox® 9015 PBT, 15% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
|
|||
| Middle Barrel Temperature | 238 - 282 °C | 460 - 540 °F | |
|
Polymer Resources PPX-FR5 Modified PPO, UL 94 V-0 with HDT of 225 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Middle Barrel Temperature | 238 - 254 °C | 460 - 490 °F | |
|
LTL Color Compounds ColorFast® FRPBT220 PBT, Flame Retarded
Super tough, flame retarded unreinforcedAll information provided by LTL Color Compounders, Inc.
|
|||