| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 246 - 279 °C | 475 - 535 °F | |
|
PTS PCA-30G11-(V) UV Stabilized, Glass Reinforced PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Middle Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
|
PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy
This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Middle Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
|
PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy
This is a non-halogenated flame retardant, UV stabilized grade. Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
|
Honeywell Aegis™ H73MP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **)
Description: Aegis H73MP is a lubricated nucleated low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR ..
|
|||
| Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
|
Honeywell Aegis™ H85MP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **)
Description: Aegis H85MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 C..
|
|||
| Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
|
Honeywell Aegis™ H85ZP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **)
Description: Aegis H85ZP is a medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well as EU..
|
|||
| Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
|
Honeywell Aegis™ H135KQP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **)
Description: Aegis H135KQP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to applicable FDA requirements, including 21 CFR 177.1500 for N6 an..
|
|||
| Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
|
Honeywell Aegis™ H135XP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **)
Description: Aegis H135XP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon..
|
|||
| Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
|
Honeywell Aegis™ H205QP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **)
Description: Aegis H205QP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500. It possesses the combination..
|
|||
| Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
|
Honeywell Aegisâ„¢ H100ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H100ZP is a medium viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well ..
|
|||
| Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
|
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
|
|||
| Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
|
Honeywell Aegisâ„¢ H135QP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135QP is a lubricated high viscosity, N6, film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements including, 21 CFR 177.1500 as well as EU Direct..
|
|||
| Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
|
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon..
|
|||
| Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
|
Honeywell Aegisâ„¢ H155MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H155MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
|
|||
| Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
|
Honeywell Aegisâ„¢ H73QP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H73QP is a lubricated low viscosity, nylon 6 extrusion grade homopolymer for cast coextrusion. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well..
|
|||
| Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
|
Honeywell Aegisâ„¢ H73ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H73ZP is a low viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR 177.1500 as well as E..
|
|||
| Middle Barrel Temperature | 246 - 254 °C | 475 - 489 °F | Tubular (Blown) Film |
|
Honeywell Aegisâ„¢ H85QP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H85QP is a lubricated, medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 a..
|
|||
| Middle Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
|
Star Plastics PC/ABSFR9002 Molding Grade PC/ABSFR
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 246 - 288 °C | 475 - 550 °F | |
|
Star Plastics PC/ABSQX7002 Molding Grade PC/ABS High Flow
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 246 - 260 °C | 475 - 500 °F | |
|
Star Plastics PC/PBT7804 Molding Grade PC/PBT
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 246 - 257 °C | 475 - 495 °F | |
|
Teknor Apex Chemlon® 225-15 MG Nylon 6, 25% Mineral Reinforced, 15% Glass Fiber Reinforced
Features: Compound offering rigidity and strength, especially at high service temperatures; Excellent for large area parts Processing Method: Injection Molding Forms: Pellets Automotive Specificatio..
|
|||
| Middle Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
|
CTC X-PRO PP 100 P1015 Polypropylene Homopolymer
X-PRO PP 1015 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled..
|
|||
| Middle Barrel Temperature | 246 - 277 °C | 475 - 531 °F | |
|
A. Schulman ComAlloy Comtuf® 520 Polycarbonate/Styrenic Alloy
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
|
|||
| Middle Barrel Temperature | 246 - 277 °C | 475 - 531 °F | |
|
A. Schulman ComAlloy Comtuf® 522 Polycarbonate/Styrenic Alloy
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
|
|||
| Middle Barrel Temperature | 246 - 277 °C | 475 - 531 °F | |
|
A. Schulman ComAlloy Comtuf® 523 Polycarbonate/Styrenic Alloy
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
|
|||
| Middle Barrel Temperature | 246 - 277 °C | 475 - 531 °F | |
|
A. Schulman ComAlloy Comtuf® 525 Polycarbonate/Styrenic Alloy
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
|
|||
| Middle Barrel Temperature | 246 - 266 °C | 475 - 511 °F | |
|
A. Schulman ComAlloy Hiloy® 261 Glass Reinforced, Modified SMA
Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Middle Barrel Temperature | 246 - 277 °C | 475 - 531 °F | |
|
A. Schulman ComAlloy Comtuf® 524 Polycarbonate/Styrenic Alloy
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
|
|||
| Middle Barrel Temperature | 246 - 266 °C | 475 - 511 °F | |
|
A. Schulman ComAlloy Hiloy® 262 Glass Reinforced, Modified SMA
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Middle Barrel Temperature | 246 - 266 °C | 475 - 511 °F | |
|
A. Schulman ComAlloy Hiloy® 263 Glass Reinforced, Modified SMA
Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||