| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-G13 Nylon 66, 13% Glass Reinforced
Nylon 66, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
|
|||
| Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-G43 Nylon 66, 43% Glass Reinforced
Nylon 66, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
|
|||
| Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-IM2-G13 Nylon 66, 13% Glass Reinforced, Impact Modified
Nylon 66, 13% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
|
|||
| Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-IM2-G33 Nylon 66, 33% Glass Reinforced, Impact Modified
Nylon 66, 33% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
|
|||
| Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-IMG33 Nylon, 33% Glass Reinforced, Impact Modified (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-M40 Nylon 66, 40% Mineral Filled
Nylon 66, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested..
|
|||
| Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-M40-[color]-H Nylon 66, 40% Mineral Filled, Heat Stabilized
Nylon 66, 40% Mineral Filled, Lubricated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon ..
|
|||
| Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Polymer Resources PC-FR3-D Polycarbonate, Improved Flame Retardant, High Flow
Polycarbonate, Improved Flame Retardant, High FlowFeatures: • High Impact Resistance • Self Extinguishing • Low ViscosityProcess: Injection MoldingNotes: All physical, mechanical and thermal t..
|
|||
| Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Polymer Resources PC-FR3-D-[color]-3 Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
|
|||
| Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow
Polycarbonate, Flame Retardant, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on..
|
|||
| Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-G13-[color]-H Nylon 66, 13% Glass Reinforced, Heat Stabilized
Nylon 66, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
|
|||
| Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-IMG13 Nylon, 13% Glass Reinforced, Impact Modified (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-IMG33-[color]H Nylon, 33% Glass Reinforced, Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Middle Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
|
Polymer Resources NY66-M40-[color]H Nylon, 40% Mineral Filled, Lubricated, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Middle Barrel Temperature | 277 - 304 °C | 530 - 580 °F | |
|
Wellman Wellamid® GFT15N050-N2 15% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized
&n
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
|
|||
| Middle Barrel Temperature | 277 - 282 °C | 530 - 540 °F | |
|
MRC Polymers EMAREXâ„¢ 400 GF13 Nylon 6/6, 13% Glass Fiber Filled
Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc.
|
|||
| Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Star Plastics PC1212FRR Molding Grade PC FR
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Star Plastics PC1212FRUV Molding Grade PC FR
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Star Plastics PC1510FR Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Star Plastics PC1510R Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Star Plastics PC741 Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Star Plastics PC743 Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 277 - 299 °C | 531 - 570 °F | |
|
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, ..
|
|||
| Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Star Plastics PC1212R Molding Grade PC with Release
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 277 - 304 °C | 530 - 580 °F | |
|
Wellman Wellamid® GB1430-N 33% Glass Bubble Filled, Low Density Nylon 66
Description: Glass Bubble Filled, Low Density Nylon 66Information provided by Wellman.
|
|||
| Middle Barrel Temperature | 277 - 304 °C | 530 - 580 °F | |
|
Wellman Wellamid® GF33-66 XE-N, 33% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
|
|||
| Middle Barrel Temperature | 277 - 304 °C | 530 - 580 °F | |
|
Wellman Wellamid® GF33-66/6 XE-N 33% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
|
|||
| Middle Barrel Temperature | 277 - 304 °C | 530 - 580 °F | |
|
Wellman Wellamid® GF43-66 XE-N 43% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
|
|||
| Middle Barrel Temperature | 277 - 304 °C | 530 - 580 °F | |
|
Wellman Wellamid® GF60-66/6 XE-N 60% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
|
|||
| Middle Barrel Temperature | 277 - 299 °C | 530 - 570 °F | |
|
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||