Polymer Property : Middle Barrel Temperature = 288 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Middle Barrel Temperature 277 - 288 °C
530 - 550 °F
Polymer Resources NY66-G13 Nylon 66, 13% Glass Reinforced
Nylon 66, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
Middle Barrel Temperature 277 - 288 °C
530 - 550 °F
Polymer Resources NY66-G33 Nylon 66, 33% Glass Reinforced
Nylon 66, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
Middle Barrel Temperature 277 - 288 °C
530 - 550 °F
Polymer Resources NY66-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Middle Barrel Temperature 277 - 288 °C
530 - 550 °F
Polymer Resources NY66-IM2-G13 Nylon 66, 13% Glass Reinforced, Impact Modified
Nylon 66, 13% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
Middle Barrel Temperature 277 - 288 °C
530 - 550 °F
Polymer Resources NY66-IM2-G33 Nylon 66, 33% Glass Reinforced, Impact Modified
Nylon 66, 33% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
Middle Barrel Temperature 277 - 288 °C
530 - 550 °F
Polymer Resources NY66-IM2-G33-[color]-H Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized
Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t..
Middle Barrel Temperature 277 - 288 °C
530 - 550 °F
Polymer Resources NY66-M40 Nylon 66, 40% Mineral Filled
Nylon 66, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested..
Middle Barrel Temperature 266 - 288 °C
510 - 550 °F
Polymer Resources PC-IM3 Polycarbonate, Impact Modified, High Flow
Polycarbonate, Impact Modified, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Middle Barrel Temperature 266 - 288 °C
510 - 550 °F
Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow
Polycarbonate, Impact Modified, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Middle Barrel Temperature 277 - 288 °C
530 - 550 °F
Ravago Manufacturing Americas Hylex® P1310LLT Polycarbonate
Information provided by Ravago
Middle Barrel Temperature 260 - 288 °C
500 - 550 °F
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled  (discontinued **)
Information provided by MRC Polymers Inc.
Middle Barrel Temperature 277 - 288 °C
530 - 550 °F
Polymer Resources NY66-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Middle Barrel Temperature 277 - 288 °C
530 - 550 °F
Polymer Resources NY66-G43-[color]H Nylon, 43% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Middle Barrel Temperature 277 - 288 °C
530 - 550 °F
Polymer Resources NY66-IMG33-[color]H Nylon, 33% Glass Reinforced, Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Middle Barrel Temperature 277 - 288 °C
530 - 550 °F
Polymer Resources NY66-M40-[color]H Nylon, 40% Mineral Filled, Lubricated, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Middle Barrel Temperature 260 - 288 °C
500 - 550 °F
Star Plastics PC721HFR Molding Grade PC
Information provided by Star Plastics, Inc.
Middle Barrel Temperature 271 - 288 °C
520 - 550 °F
Wellman Wellamid® 22LHI3 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
Middle Barrel Temperature 271 - 288 °C
520 - 550 °F
Wellman Wellamid® 22LHI4 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
Middle Barrel Temperature 271 - 288 °C
520 - 550 °F
Wellman Wellamid® 22LH-N Unfilled Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
Middle Barrel Temperature 271 - 288 °C
520 - 550 °F
Wellman Wellamid® 22L-N Unfilled Nylon 66, Lubricated
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
Middle Barrel Temperature 271 - 288 °C
520 - 550 °F
Wellman Wellamid® 22LN2-N Unfilled Nylon 66, Lubricated & Nucleated
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
Middle Barrel Temperature 271 - 288 °C
520 - 550 °F
Wellman Wellamid® GS25-66 22LH-N 25% Glass Sphere Filled Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
Middle Barrel Temperature 271 - 288 °C
520 - 550 °F
Wellman Wellamid® MR340 42H-N 34% Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
Middle Barrel Temperature 271 - 288 °C
520 - 550 °F
Wellman Wellamid® XT1482-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
Middle Barrel Temperature 271 - 288 °C
520 - 550 °F
Wellman Wellamid® XT1486-BK Medium Impact Nylon 66
Description: Medium Impact Nylon 66Information provided by Wellman.
Middle Barrel Temperature 260 - 288 °C
500 - 550 °F
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black
Data provided by Clariant Masterbatches
Middle Barrel Temperature 254 - 288 °C
490 - 550 °F
Clariant 66G43HLS-Black Nylon 66, 43% Glass Fiber Reinforced, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
Middle Barrel Temperature 260 - 288 °C
500 - 550 °F
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened
Data provided by Clariant Masterbatches
Middle Barrel Temperature 260 - 288 °C
500 - 550 °F
Clariant Renol PA611D40 Nylon 612, Glass Fiber Reinforced, Molybdenum Disulfide Lubricated
Data provided by Clariant Masterbatches
Middle Barrel Temperature 277 - 288 °C
530 - 550 °F
Entec Hylex® P1010FR Polycarbonate
Information provided by Ravago.