Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Middle Barrel Temperature = 304 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Middle Barrel Temperature 288 - 304 °C
550 - 580 °F
PlastiComp Complet® LCF50 - PA66 Nylon 66, 50% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
Middle Barrel Temperature 288 - 304 °C
550 - 580 °F
PlastiComp Complet® LGF50 - PA66 MT Nylon 66, 50% Long Glass Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementImpact modifiedInformation provided by ..
Middle Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow
Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted..
Middle Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE
Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Middle Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release
Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Middle Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources PC-GP2-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release
Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
Middle Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources PC-IM1 Polycarbonate, Impact Modified, Low Flow
Polycarbonate, Impact Modified, Low FlowProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided ..
Middle Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-FR7 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 260F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Middle Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
Middle Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-GP2 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 250F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Middle Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant
Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
Middle Barrel Temperature 271 - 304 °C
520 - 580 °F
Polymer Resources PPX-SF1 Modified-PPO, Structural Foam Grade, Flame Retardant, Easy Flow
Modified-Polyphenylene Oxide, Structural Foam Grade, Easy FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechani..
Middle Barrel Temperature 271 - 304 °C
520 - 580 °F
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant
Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec..
Middle Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-GP4 Modified PPO, General Purpose with HDT of 210 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 271 - 304 °C
520 - 580 °F
Polymer Resources PPX-SF2 Modified PPO, Structural Foam Grade, Standard Flow  (Unverified Data**)
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
Middle Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam..
Middle Barrel Temperature 277 - 304 °C
530 - 580 °F
Wellman Wellamid® GB1430-N 33% Glass Bubble Filled, Low Density Nylon 66
Description: Glass Bubble Filled, Low Density Nylon 66Information provided by Wellman.
Middle Barrel Temperature 277 - 304 °C
530 - 580 °F
Wellman Wellamid® GF33-66 XE-N, 33% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Middle Barrel Temperature 277 - 304 °C
530 - 580 °F
Wellman Wellamid® GF33-66/6 XE-N 33% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
Middle Barrel Temperature 277 - 304 °C
530 - 580 °F
Wellman Wellamid® GF43-66 XE-N 43% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Middle Barrel Temperature 277 - 304 °C
530 - 580 °F
Wellman Wellamid® GF60-66/6 XE-N 60% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
Middle Barrel Temperature 277 - 304 °C
530 - 580 °F
Wellman Wellamid® GFT13-66 XE-N 13% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
Middle Barrel Temperature 296 - 304 °C
565 - 579 °F
A. Schulman ComAlloy Hiloy® 441 Glass Reinforced, PET Alloy
Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 296 - 304 °C
565 - 579 °F
A. Schulman ComAlloy Hiloy® 464 Glass Fiber/Bead Reinforced, PET Alloy
Data provided by the manufacturer, ComAlloy International Company.25% Glass Fiber/Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 288 - 304 °C
550 - 580 °F
PlastiComp Complet® LCF50 - PA66 MT Nylon 66, 50% Long Carbon Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementImpact modifiedInformation provided by Pla..
Middle Barrel Temperature 288 - 304 °C
550 - 580 °F
PlastiComp Complet® LGF50 - PA66 Nylon 66, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% long glass fiber reinforcementInformation provided by PlastiComp, In..
Middle Barrel Temperature 260 - 304 °C
500 - 580 °F
Polymer Resources PPX-GP4-WR Modified PPO, Wear Resistant with HDT of 215 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 271 - 304 °C
520 - 580 °F
Polymer Resources PPX-SF1 Modified PPO, Structural Foam Grade, Easy Flow  (Unverified Data**)
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
Middle Barrel Temperature 282 - 304 °C
540 - 580 °F
LTL Color Compounds ColorFast® FRPC200 Polycarbonate, Flame-Retarded
Improved flame-retarded V0/5V injection molding polycarbonateAll information provided by LTL Color Compounders, Inc.