| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
|
Polymer Resources PPX-FR6 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 300F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
|
|||
| Middle Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
|
Polymer Resources PPX-G15 Modified-PPO, 15% Glass Reinforced, High Flow
Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
|
|||
| Middle Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
|
Polymer Resources PPX-G30 Modified-PPO, 30% Glass Reinforced
Modified-Polyphenylene Oxide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Middle Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
|
Polymer Resources PPX-MF-FRG20 Modified-PPO, 40% Glass/Mineral Reinforced, Flame Retardant
Modified-Polyphenylene Oxide, 40% Glass/Mineral Reinforced, Flame RetardantFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanica..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | Injection Molding |
|
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF10%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM
Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM
Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM
Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM
Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Dry as Molded
Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® R533H01 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H01 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties whe..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® R533T Nylon 66, Translucent, 33% Glass Filled, Dry as Molded
Vydyne® R533T is a translucent 33% glass-reinforced PA66 resin designed specifically for use in power-steeing reservoirs dn other applications where chemical resistance, whiteness and transmittance..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM
Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM
Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded
Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. ..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM
Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM
Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, DAM
Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® R533H BK02 Nylon 66, 33% Glass Reinforced, DAM
Vydyne® R533H BK02 is 33% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when exposed to anti-f..
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | |
|
Ascend Performance Materials Vydyne® R633 Nylon 66 Copolymer, 33% Glass Filled, Dry as Molded
Vydyne® R633 is 33% glass-fiber reinforced, PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold ..
|
|||
| Middle Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
|
Polymer Resources PPX-G10 Modified PPO, 10% Glass Reinforced
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Middle Barrel Temperature | 271 - 310 °C | 520 - 590 °F | |
|
Polymer Resources PPX-G20 Modified PPO, 20% Glass Reinforced
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F | Injection Molding |
|
LG Chemical LUPOY GP2100 PC+GF10%, Heat Resistance
Description: Injection Molding, PC+GF10%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..
|
|||