| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 190 °C | 374 °F | |
|
Multibase TPSiV™ 3011-70A Thermoplastic Silicone Vulcanizate
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced..
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | |
|
Multibase TPSiV™ 3040-60A Thermoplastic Silicone Vulcanizate
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced..
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | |
|
Multibase TPSiV™ 3111-70A Thermoplastic Silicone Vulcanizate
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced..
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | Zone 2; Cylinder |
|
Premix Thermoplastics PRE-ELEC® ESD 7120
PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject..
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | Zone 3; Cylinder |
|
Premix Thermoplastics PRE-ELEC® CP 1316
(discontinued **)
PRE-ELEC CP 1316 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a very low electrical resis..
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical HF380G ABS, High Flow
Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical HI110 ABS, High Impact, Chemical Resistance
Feature: Injection Molding, High Impact, Chemical ResistanceApplication: Edge of Furniture ApplicationsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical HI121H ABS, High Stiffness
Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical HI153 ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical HT700 ABS, High Stiffness
Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1040D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical LI921NS ASA
Description: High Weatherability, AntistaticApplication: Sanitary ApplicationsCAS: 26299-47-8Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical AF305HT ABS, Flame Retardant, Heat Resistance
Feature: Injection Molding, Flame Retardant, Heat ResistanceApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 9001-96-2, 68928-70-1, and 1309-64-4Inf..
|
|||
| Middle Barrel Temperature | 190 - 240 °C | 374 - 464 °F | Injection |
|
Inno-Comp INNOPOL® CS 1-2120 AP 20% Talc Filled Polypropylene Homopolymer
INNOPOL CS 1-2120 AP is a 20 % talc filled compound based on polypropylene homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 1-2120 AP is recommended especially..
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical XG569C MABS, Anti-Scratch, High Gloss
Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
|
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS
VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | |
|
SK Chemicals SKYTHANE® CS195A Calendaring Series, Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | |
|
SK Chemicals SKYTHANE® R190A Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | cylinder temperature |
|
Borealis FL5580 High Density Polyethylene
FL5580 is a high density polyethylene with an excellent combination of extrusion properties and moisture barrier properties. Applications: FL5580 has been developed especially for applications like..
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Mid-2. Region Temperature |
|
Tisan TISOPLEN® 10% Calcite Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Mid-2. Region Temperature |
|
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Mid-2. Region Temperature |
|
Tisan TISOPLEN® 40% Talc Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | cylinder |
|
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes
BorSafe™ HE3490-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s..
|
|||
| Middle Barrel Temperature | 190 - 250 °C | 374 - 482 °F | |
|
Diamond Polymers ABS 3502
Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Middle Barrel Temperature | 190 - 250 °C | 374 - 482 °F | |
|
Diamond Polymers ABS 7500E
Description: Extrusion Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | Injection |
|
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G90A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
|
|||
| Middle Barrel Temperature | 190 °C | 374 °F | Injection |
|
Alliance Polymers Zythane™ 6080A Thermoplastic Polyurethane Elastomer
Zythane™ 6080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
|
LG Chemical LI912 ASA
Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical
|
|||