Polymer Property : Middle Barrel Temperature = 450 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy
PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided..
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Polymer Resources PC/ABS-FR1-[color]-WR Flame Retardant PC/ABS Alloy, Wear Resistant
PC/ABS Alloy, Flame Retardant, Standard Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info..
Middle Barrel Temperature 232 - 277 °C
450 - 530 °F
Polymer Resources PPX-MF-FR1 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha..
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Polymer Resources PC/ABS-FR1-[color]-HH Flame Retardant PC/ABS Alloy, Low Flow
PC/ABS Alloy, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
Middle Barrel Temperature 232 - 249 °C
450 - 480 °F
Polymer Resources PC/TP-GP3 PC/Polyester Alloy
High Impact, Superior Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Middle Barrel Temperature 232 - 266 °C
450 - 511 °F
Injection Molding
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Middle Barrel Temperature 232 - 266 °C
450 - 511 °F
Injection Molding
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade
Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g..
Middle Barrel Temperature 232 - 266 °C
450 - 511 °F
Injection Molding
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Middle Barrel Temperature 232 - 277 °C
450 - 530 °F
Wellman Wellamid® 42LH-N Unfilled Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA S319
Description: ASA Weatherable Polymer, Injection Molding Grade, High ModulusInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA S510
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA S610
Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA S910
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA T-120
Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat ResistanceInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA TW-18B2
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 266 °C
450 - 510 °F
Diamond Polymers ASA TW-23V
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Middle Barrel Temperature 232 - 277 °C
450 - 530 °F
Polymer Resources PPX-MF-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F, Mineral Reinforced  (Unverified Da
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Middle Barrel Temperature 232 - 249 °C
450 - 480 °F
Polymer Resources PC/TP-GP3 PC Polyester, High Impact, Superior Chemical Resistance  (Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.