| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 254 - 293 °C | 490 - 560 °F | |
|
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled
PC/ABS Alloy, General Purpose, 10% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi..
|
|||
| Middle Barrel Temperature | 254 - 293 °C | 490 - 560 °F | |
|
Polymer Resources PC/ABS-G20 General Purpose PC/ABS Alloy, 20% Glass Filled
PC/ABS Alloy, General Purpose, 20% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi..
|
|||
| Middle Barrel Temperature | 254 - 293 °C | 490 - 560 °F | |
|
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized
PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
|
|||
| Middle Barrel Temperature | 254 - 293 °C | 490 - 560 °F | |
|
Polymer Resources PC/ABS-GP2 General Purpose PC/ABS Alloy, High Flow
PC/ABS Alloy, General Purpose, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by ..
|
|||
| Middle Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
|
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy
Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p..
|
|||
| Middle Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
|
Polymer Resources PC/TP-GP1-[color]-3 PC Polyester, High Impact, Good Chemical Resistance, UV-stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Middle Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
|
Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow
High Melt Flow, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by ..
|
|||
| Middle Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
|
Polymer Resources PC/TP-GP1-UV PC/Polyester Alloy, UV-stabilized
High Impact, Good Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
|
|||
| Middle Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
|
Polymer Resources PC/TP-GP2 PC/Polyester Alloy
High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b..
|
|||
| Middle Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
|
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized
High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
|
|||
| Middle Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
|
Polymer Resources PC/TP-GP3-G10 PC/Polyester Alloy, 10% Glass Reinforced
Superior Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Middle Barrel Temperature | 254 - 299 °C | 490 - 570 °F | |
|
Polymer Resources PPX-GP3-[color]-HF Modified-PPO, General Purpose, High Flow
Modified-Polyphenylene Oxide, General Purpose, High Flow, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample..
|
|||
| Middle Barrel Temperature | 254 - 299 °C | 490 - 570 °F | |
|
Polymer Resources PPX-GP3-IM Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
|
|||
| Middle Barrel Temperature | 254 - 299 °C | 490 - 570 °F | |
|
Polymer Resources PPX-GP8 Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 240F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
|
|||
| Middle Barrel Temperature | 254 - 266 °C | 490 - 510 °F | |
|
Ravago Manufacturing Americas Hybrid S451H Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America Flame Retardant High Flow RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago
|
|||
| Middle Barrel Temperature | 254 - 271 °C | 490 - 520 °F | |
|
Ravago Manufacturing Americas Hylex® P1018LLT Polycarbonate
Information provided by Ravago.
|
|||
| Middle Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
|
Polymer Resources PC/TP-GP2 PC Polyester, High Impact, Excellent Chemical Resistance
(Unverified Data**)&
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Middle Barrel Temperature | 254 - 293 °C | 490 - 560 °F | |
|
Oxford Polymers PC/ABS 604i-FR PC/ABS, Flame retardant
Product Description: Amorphous, Polycarbonate & ABS, Flame retardant, Injection Molding Grade, VO rated @ 3.0mm. V2 rated @ 1.5mm Processing and Delivery Form: Pellets and Injection MoldingAdditive..
|
|||
| Middle Barrel Temperature | 254 - 293 °C | 490 - 560 °F | |
|
Polymer Resources PC/ABS-G40 General Purpose PC/ABS Alloy, 40% Glass Filled
PC/ABS Alloy, General Purpose, 40% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi..
|
|||
| Middle Barrel Temperature | 254 - 293 °C | 490 - 560 °F | |
|
Polymer Resources PC/ABS-GP1 General Purpose PC/ABS Alloy
PC/ABS Alloy, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Re..
|
|||
| Middle Barrel Temperature | 254 - 293 °C | 490 - 560 °F | |
|
Polymer Resources PC/ABS-GP1-[color]-3 PC Blend, General Purpose, UV-stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Middle Barrel Temperature | 254 - 293 °C | 490 - 560 °F | |
|
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade
PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p..
|
|||
| Middle Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
|
Polymer Resources PC/TP-GP1 PC/Polyester Alloy
High Impact, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Pol..
|
|||
| Middle Barrel Temperature | 254 - 282 °C | 490 - 540 °F | |
|
LTL Color Compounds ColorFast® NY2115 Nylon 66
Super tough nylon 6,6 with excellent chemical resistance and ductilityAll information provided by LTL Color Compounders, Inc.
|
|||
| Middle Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
|
Wellman Wellamid® GF14-60 XE-N 14% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
|
|||
| Middle Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
|
Wellman Wellamid® GF20-60 XE-N 20% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
|
|||
| Middle Barrel Temperature | 254 - 277 °C | 490 - 530 °F | |
|
Wellman Wellamid® GF30-60 XE-N 30% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
|
|||
| Middle Barrel Temperature | 254 - 271 °C | 490 - 520 °F | |
|
Entec Hylex® P1017FR Polycarbonate
Information provided by Ravago.
|
|||
| Middle Barrel Temperature | 254 - 288 °C | 490 - 550 °F | |
|
Clariant 66G43HLS-Black Nylon 66, 43% Glass Fiber Reinforced, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Middle Barrel Temperature | 254 - 299 °C | 490 - 570 °F | |
|
Polymer Resources PPX-GP8 Modified PPO, General Purpose, Impact Modified
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||