| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Middle Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
|
|||
| Middle Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release
Polycarbonate, General Purpose, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
|
|||
| Middle Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Polymer Resources PC-GP4-[color]-4 Polycarbonate, UV-stabilized, Easy Flow with Mold Release
Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa..
|
|||
| Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
|
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
|
|||
| Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
|
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant
Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
|
|||
| Middle Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Polymer Resources PC-UV4 Polycarbonate, UV-stabilized, Easy Flow
Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
|
|||
| Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
|
LG Chemical LUMID GP2259AFL PA6+GF25%, Flame Retardant
Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Connector)CAS No. 25038-54-4, 65997-17-3, 1163-19-5, 1309-64-4 and 138265-88-0Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 260 - 285 °C | 500 - 545 °F | Injection Molding |
|
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose
Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 260 - 285 °C | 500 - 545 °F | Injection Molding |
|
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose
Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Middle Barrel Temperature | 260 - 285 °C | 500 - 545 °F | Injection Molding |
|
LG Chemical LUMID HM2604AW PA6+GF60%
Feature: Injection Molding, PA6+GF60%Application: Bath liftInformation provided by LG Chemical
|
|||
| Middle Barrel Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
|
LG Chemical LUPOY GN1008RF PC, Halogen Free, Flame Retardant, High impact strength
Description: Injection Molding, PC, Halogen Free Flame Retardant, High impact strengthApplication: IT&OA (Notebook PC battery pack housing)CAS: 103598-77-2, 137050-02-03 and 139189-30-3Information p..
|
|||
| Middle Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
MRC Polymers EMAREXâ„¢ 300 GF33 Nylon 6, 33% Glass Fiber Filled
Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc.
|
|||
| Middle Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
MRC Polymers EMAREXâ„¢ 300 GF43 Nylon 6, 43% Glass Fiber Filled
Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc.
|
|||
| Middle Barrel Temperature | 260 - 288 °C | 500 - 550 °F | |
|
Star Plastics PC/ABSQX7004 Molding Grade PC/ABS
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 260 - 288 °C | 500 - 550 °F | |
|
Star Plastics PC721HFR Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Mid-2. Region Temperature |
|
Tisan TISLAMID® 66 Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Mid-2. Region Temperature |
|
Tisan TISLAMID® 66 UNR Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Middle Barrel Temperature | 260 - 277 °C | 500 - 530 °F | |
|
Wellman Wellamid® NY1599-N Unfilled Nylon 66
Description: Unfilled Nylon 66Information provided by Wellman.
|
|||
| Middle Barrel Temperature | 260 - 280 °C | 500 - 536 °F | |
|
Unitika L-8005
Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd.
|
|||
| Middle Barrel Temperature | 260 - 288 °C | 500 - 550 °F | |
|
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Middle Barrel Temperature | 260 - 288 °C | 500 - 550 °F | |
|
Clariant Renol BRU0000BN-182 Nylon 66, Lubricated, Nucleated, Weather Resistant
Data provided by Clariant Masterbatches
|
|||
| Middle Barrel Temperature | 260 - 288 °C | 500 - 550 °F | |
|
Clariant Renol PA611D40 Nylon 612, Glass Fiber Reinforced, Molybdenum Disulfide Lubricated
Data provided by Clariant Masterbatches
|
|||
| Middle Barrel Temperature | 260 - 266 °C | 500 - 510 °F | |
|
Diamond Polymers ASA M-143
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Middle Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
|
A. Schulman ComAlloy Hiloy® 610 Nylon 6, Glass/Mineral Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Middle Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
|
A. Schulman ComAlloy Voloy® 612 Nylon 6, Glass Fiber/Bead Reinforced, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Fiber/Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Middle Barrel Temperature | 260 - 265 °C | 500 - 509 °F | |
|
Beijing Chemical Industry KAIFA® MN301-G0 Nylon 66 Resin
High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Middle Barrel Temperature | 260 - 304 °C | 500 - 580 °F | |
|
Polymer Resources PPX-FR3 Modified PPO, UL 94 V-1 with HDT of 265 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||