Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Front Barrel Temperature | 188 - 199 °C | 370 - 390 °F | |
Polymer Resources AC-G10 Acetal Copolymer, 10% Glass Reinforced Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/10/E/M Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/20 Polypropylene Homopolymer, 20% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/20/H Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/30/E Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/30/E/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/30/E/NS Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, NSF listed Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/30/F Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/40/E Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/40/E/EX Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled, high viscosity Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-68/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® M-1812 Polypropylene Homopolymer, 45% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® M-2149 Polypropylene Homopolymer, 30% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® M-2450 Polypropylene Copolymer Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® PP-60/CC/40 Polypropylene Homopolymer, 40% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 188 - 199 °C | 370 - 390 °F | |
Kraton® D2104 DI-N (SBS) Compound Description: Kraton D2104 DI-N is an easy processing, general purpose material designed for a wide variety of applications. It is supplied from North America in the physical form identified: D2104 D.. |
|||
Front Barrel Temperature | 188 - 199 °C | 370 - 390 °F | |
Kraton® D2109 DS-N (SBS) Compound Description: Kraton D2109 DS-N is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/15/MI/20 Polypropylene Homopolymer, 35% Glass/mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Teknor Apex Flexalloy® 3500-75NT Polyvinyl Chloride Elastomer Features: Good Thermal Stability; Recyclable Material; Good Weather Resistance; Ultra High Molecular Weight Uses: Medical/Healthcare Applications; Pump Parts; Tubing Agency Ratings: FDA Unspecified .. |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Teknor Apex Flexalloy® 9100-75 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Elastocon TPE Technologies Elastocon® 8078B Thermoplastic Elastomer Elastocon® 8078B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8078B is well suited for consumer goods a.. |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Elastocon TPE Technologies Elastocon® 8078N Thermoplastic Elastomer Elastocon® 8078N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8078N is FDA compliant and well suited.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8201-60 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8281-45MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |