| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Front Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
PolyOne Versaflex™ OM 6059-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6059-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
|
|||
| Front Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
PolyOne Versaflex™ OM 6258-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6258-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
|
|||
| Front Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
PolyOne Versaflex™ OM 6258-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6258-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-G13 Nylon 6, 13% Glass Reinforced
Nylon 6, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-G30 Nylon 6, 30% Glass Reinforced
Nylon 6, 30% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
|
|||
| Front Barrel Temperature | 249 - 282 °C | 480 - 540 °F | |
|
Polymer Resources PC/TP-FR3 Flame Retardant PC/Polyester Alloy
Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p..
|
|||
| Front Barrel Temperature | >= 249 °C | >= 480 °F | |
|
Polymer Resources PPX-GP3-[color]-EN Modified-PPO, Extrusion Grade
Modified-Polyphenylene Oxide, Extrusion Grade, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: ExtrusionNotes: All physical, mechanical and thermal testing conduct..
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TP-FR IM PBT, Impact Modified, Flame Retardant, Low Flow
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TP-FRHG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame Retardant
Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TP-FRHG30 Polybutylene Terephthalate, 30% Glass Reinforced Alloy, Flame Retardant
Polybutylene Terephthalate, 30% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant
Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t..
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TP-FV699 PBT, 10% Glass Reinforced Structural Foam Grade, Low Shrinkage
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TP-G10 Polybutylene Terephthalate, 10% Glass Reinforced
Polybutylene Terephthalate, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov..
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TP-G20 Polybutylene Terephthalate, 20% Glass Reinforced
Polybutylene Terephthalate, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov..
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced
Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov..
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TP-HG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy
Polybutylene Terephthalate, 15% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio..
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TP-IG30 Polybutylene Terephthalate, 30% Glass Reinforced, Reduced Warpage
Polybutylene Terephthalate, 30% Glass Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TP-IM-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Impact Modified
Polybutylene Terephthalate, 30% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TP-IM-G7.5 Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact Modified
Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample..
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TPSF-FR1 PBT, 30% Glass Reinforced Structural Foam Grade, Flame Retardant
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TPSF-FRG30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, ..
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced
Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info..
|
|||
| Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
|
Polymer Resources TPSF-GP1 PBT, 30% Glass Reinforced Structural Foam Grade
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-G13-[color]-H Nylon 6, 13% Glass Reinforced, Heat Stabilized
Nylon 6, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-M25G15 Nylon 6, 25% Mineral, 15% Glass Reinforced
Nylon 6, 25% Mineral, 15% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon gra..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-M40 Nylon 6, 40% Mineral Filled
Nylon 6, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested ..
|
|||
| Front Barrel Temperature | 249 °C | 480 °F | |
|
MTI ThermoStran® PP-30G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
|
|||
| Front Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Wellman Wellamid® GF14-60 XE-N 14% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
|
|||
| Front Barrel Temperature | 249 - 271 °C | 480 - 520 °F | |
|
Wellman Wellamid® GF30-60 XE-N 30% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
|
|||
| Front Barrel Temperature | 249 - 288 °C | 480 - 550 °F | |
|
Polymer Resources PPX-FR5 Modified PPO, UL 94 V-0 with HDT of 225 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||