| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Polymer Resources NY66-IM2-G33-[color]-H Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized
Nylon 66, 33% Glass Reinforced, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t..
|
|||
| Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy
Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p..
|
|||
| Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Polymer Resources PC/TP-GP1-[color]-3 PC Polyester, High Impact, Good Chemical Resistance, UV-stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Polymer Resources PC/TP-GP3-G20 PC/Polyester Alloy, 20% Glass Reinforced
Superior Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate
Information provided by Ravago.
|
|||
| Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Polymer Resources PC/TP-GP1 PC Polyester, High Impact, Good Chemical Resistance
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Polymer Resources PC/TP-GP2 PC Polyester, High Impact, Excellent Chemical Resistance
(Unverified Data**)&
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Polymer Resources NY66-IMG33-[color]H Nylon, 33% Glass Reinforced, Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
|
Polymer Resources PC/TP-GP1 PC/Polyester Alloy
High Impact, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Pol..
|
|||
| Front Barrel Temperature | 254 - 282 °C | 490 - 540 °F | |
|
LTL Color Compounds ColorFast® NY2115 Nylon 66
Super tough nylon 6,6 with excellent chemical resistance and ductilityAll information provided by LTL Color Compounders, Inc.
|
|||
| Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy
Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati..
|
|||
| Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
MRC Polymers NAXALOYâ„¢ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled
Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc.
|
|||
| Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
MRC Polymers NAXALOYâ„¢ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled
Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc.
|
|||
| Front Barrel Temperature | 257 - 282 °C | 495 - 540 °F | |
|
Star Plastics PC/PBTQX7008 Molding Grade PC/PBT
Information provided by Star Plastics, Inc.
|
|||
| Front Barrel Temperature | 263 - 282 °C | 505 - 540 °F | |
|
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced
Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St..
|
|||
| Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Wellman EcoLon® 2000-BK1 37% Post Consumer Compound Nylon 66
Description: Post Consumer Compound Nylon 66Information provided by Wellman.
|
|||
| Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Wellman EcoLon® MRGF1518-BK Mineral/Glass Fiber Reinforced Nylon 66, Lubricated, Heat Stabilized, PCR
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
|
Wellman Wellamid® 220-N Unfilled Nylon 66, Not Lubricated, Nucleated, or Heat Stabilized
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
|
|||
| Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
|
Wellman Wellamid® 22LHI3 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
|
|||
| Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
|
Wellman Wellamid® 22L-N Unfilled Nylon 66, Lubricated
Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae..
|
|||
| Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
|
Wellman Wellamid® MR410 42H-N 40% Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Wellman Wellamid® MRGF25/15 22H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 66, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Wellman Wellamid® MRGF3822-BK 38% Mineral/10% Glass Fiber Reinforced Nylon 66, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
|
Wellman Wellamid® T423-BK10 Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
|
Wellman Wellamid® XT1482-BK High Impact Nylon 66
Description: High Impact Nylon 66Information provided by Wellman.
|
|||
| Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
|
Wellman Wellamid® XT1482-N Impact Modified Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro..
|
|||
| Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Entec Hylex® P1017FR Polycarbonate
Information provided by Ravago.
|
|||
| Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
|
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
|
|||
| Front Barrel Temperature | 263 - 282 °C | 505 - 540 °F | |
|
Teknor Apex Chemlon® 140 MH Nylon 66, 40% Mineral Reinforced
Notes: 40% Mineral; High rigidity with exceptional control of warpage and surface sink marks; Excellent for large parts; Fast cycling Features: Fast Molding Cycle; High Rigidity; Heat Stabilized; Lo..
|
|||
| Front Barrel Temperature | 243 - 282 °C | 470 - 540 °F | |
|
Polymer Resources PPX-MF-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F, Mineral Reinforced
(Unverified Da
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||