| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Front Barrel Temperature | 293 - 304 °C | 560 - 580 °F | |
|
Polymer Resources NY66-G33 Nylon 66, 33% Glass Reinforced
Nylon 66, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
|
|||
| Front Barrel Temperature | 293 - 304 °C | 560 - 580 °F | |
|
Polymer Resources NY66-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Front Barrel Temperature | 293 - 304 °C | 560 - 580 °F | |
|
Polymer Resources NY66-G43 Nylon 66, 43% Glass Reinforced
Nylon 66, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test..
|
|||
| Front Barrel Temperature | 293 - 304 °C | 560 - 580 °F | |
|
Polymer Resources NY66-G43-[color]-H Nylon 66, 43% Glass Reinforced, Heat Stabilized
Nylon 66, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
|
|||
| Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources NY66-IM1-G13 Nylon 66, 13% Glass Reinforced, Toughened
Nylon 66, 13% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g..
|
|||
| Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources NY66-IM1-G33-[color]-H Nylon 66, 33% Glass Reinforced, Toughened and Heat Stabilized
Nylon 66, 33% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes..
|
|||
| Front Barrel Temperature | 293 - 304 °C | 560 - 580 °F | |
|
Polymer Resources NY66-IM2-G13 Nylon 66, 13% Glass Reinforced, Impact Modified
Nylon 66, 13% Glass Reinforced, Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
|
|||
| Front Barrel Temperature | 293 - 304 °C | 560 - 580 °F | |
|
Polymer Resources NY66-IMG13-[color]H Nylon, 13% Glass Reinforced, Impact Modified, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources NY66-IM-G40 Nylon 66, 40% Glass Reinforced, Impact Modified
Nylon 66, 40% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g..
|
|||
| Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources NY66-M25G15 Nylon 66, 25% Mineral, 15% Glass Reinforced
Nylon 66, 25% Mineral, 15% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon gr..
|
|||
| Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources NY66-M25G15-[color]-H Nylon 66, 25% Mineral, 15% Glass Reinforced, Heat Stabilized
Nylon 66, 25% Mineral, 15% Glass Reinforced, Lubricated and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, te..
|
|||
| Front Barrel Temperature | 293 - 304 °C | 560 - 580 °F | |
|
Polymer Resources NY66-M40 Nylon 66, 40% Mineral Filled
Nylon 66, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested..
|
|||
| Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources PC-FD3-[color]-1 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig..
|
|||
| Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow
Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc..
|
|||
| Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources PC-GP3-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, High Flow
Polycarbonate, FDA-compliant Feedstocks, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Front Barrel Temperature | 266 - 304 °C | 510 - 580 °F | |
|
Polymer Resources PPX-GP3 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing..
|
|||
| Front Barrel Temperature | 266 - 304 °C | 510 - 580 °F | |
|
Polymer Resources PPX-GP3-[color]-HF Modified-PPO, General Purpose, High Flow
Modified-Polyphenylene Oxide, General Purpose, High Flow, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample..
|
|||
| Front Barrel Temperature | 266 - 304 °C | 510 - 580 °F | |
|
Polymer Resources PPX-GP3-IM Modified-PPO, Impact Modified
Modified-Polyphenylene Oxide, Impact Modified, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
|
|||
| Front Barrel Temperature | 266 - 304 °C | 510 - 580 °F | |
|
Polymer Resources PPX-GP3-WR Modified-PPO, Wear Resistant
Modified-Polyphenylene Oxide, Wear Resistant, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water Absorption • Good Wear ResistanceProcess: Injection MoldingNotes: All physical, mechan..
|
|||
| Front Barrel Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant
Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec..
|
|||
| Front Barrel Temperature | 293 - 304 °C | 560 - 580 °F | |
|
Polymer Resources NY66-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Front Barrel Temperature | 293 - 304 °C | 560 - 580 °F | |
|
Polymer Resources NY66-G33-[color]-H Nylon 66, 33% Glass Reinforced, Heat Stabilized
Nylon 66, 33% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylo..
|
|||
| Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Polymer Resources NY66-IM1-G13-[color]-H Nylon 66, 13% Glass Reinforced, Toughened and Heat Stabilized
Nylon 66, 13% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes..
|
|||
| Front Barrel Temperature | 293 - 304 °C | 560 - 580 °F | |
|
Polymer Resources NY66-IMG13 Nylon, 13% Glass Reinforced, Impact Modified (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Front Barrel Temperature | 293 - 304 °C | 560 - 580 °F | |
|
Polymer Resources NY66-M40-[color]H Nylon, 40% Mineral Filled, Lubricated, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Front Barrel Temperature | 266 - 304 °C | 510 - 580 °F | |
|
Polymer Resources PPX-GP3 Modified PPO, General Purpose with HDT of 235 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Front Barrel Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Polymer Resources PPX-SF2 Modified PPO, Structural Foam Grade, Standard Flow
(Unverified Data**)
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
|
|||
| Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
LTL Color Compounds ColorFast® PC150 Polycarbonate
15 melt high flow polycarbonateAll information provided by LTL Color Compounders, Inc.
|
|||
| Front Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
|
Samyang Trirex® PC-3025IR 10 MFI Clear Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Front Barrel Temperature | 271 - 304 °C | 520 - 580 °F | |
|
Polymer Resources PPX-SF1 Modified PPO, Structural Foam Grade, Easy Flow
(Unverified Data**)
Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel..
|
|||