Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Front Barrel Temperature = 316 °C Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Front Barrel Temperature 293 - 316 °C
560 - 600 °F
Polymer Resources PC-FD2-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
Front Barrel Temperature 293 - 316 °C
560 - 600 °F
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Front Barrel Temperature 293 - 316 °C
560 - 600 °F
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE
Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Front Barrel Temperature 304 - 316 °C
580 - 600 °F
Polymer Resources PC-G30-TFE15 Polycarbonate, 30% Glass Reinforced, 15% PTFE
Polycarbonate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
Front Barrel Temperature 293 - 316 °C
560 - 600 °F
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow
Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on..
Front Barrel Temperature 293 - 316 °C
560 - 600 °F
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release
Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Front Barrel Temperature 293 - 316 °C
560 - 600 °F
Polymer Resources PC-IM1 Polycarbonate, Impact Modified, Low Flow
Polycarbonate, Impact Modified, Low FlowProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided ..
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-FR6 Modified-PPO, V-0 Flame Retardant
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 300F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-G10HF Modified-PPO, 10% Glass Reinforced, High Flow
Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-G15 Modified-PPO, 15% Glass Reinforced, High Flow
Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-G20 Modified-PPO, 20% Glass Reinforced
Modified-Polyphenylene Oxide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-G5 Modified-PPO, 5% Glass Reinforced
Modified-Polyphenylene Oxide, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro..
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-GP5 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 270F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-GP6 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Front Barrel Temperature 293 - 316 °C
560 - 600 °F
LTL Color Compounds ColorFast® PC100 Polycarbonate
10 melt standard injection molding gradeAll information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 288 - 316 °C
550 - 600 °F
Star Plastics PC1212FRR Molding Grade PC FR
Information provided by Star Plastics, Inc.
Front Barrel Temperature 288 - 316 °C
550 - 600 °F
Star Plastics PC1212FRRUV Molding Grade PC FR
Information provided by Star Plastics, Inc.
Front Barrel Temperature 288 - 316 °C
550 - 600 °F
Star Plastics PC1212FRUV Molding Grade PC FR
Information provided by Star Plastics, Inc.
Front Barrel Temperature 288 - 316 °C
550 - 600 °F
Star Plastics PC1510FR Molding Grade PC
Information provided by Star Plastics, Inc.
Front Barrel Temperature 288 - 316 °C
550 - 600 °F
Star Plastics PC1510R Molding Grade PC with Release
Information provided by Star Plastics, Inc.
Front Barrel Temperature 288 - 316 °C
550 - 600 °F
Star Plastics PC1212R Molding Grade PC with Release
Information provided by Star Plastics, Inc.
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-G10 Modified PPO, 10% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-G20 Modified PPO, 20% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-G30 Modified PPO, 30% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-GP5 Modified PPO, General Purpose with HDT of 270 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-GP6 Modified PPO, General Purpose with HDT of 290 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-GP7 Modified PPO, General Purpose with HDT of 300 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 293 - 316 °C
560 - 600 °F
LTL Color Compounds ColorFast® FRPC100 Polycarbonate, Flame-Retarded
Flame-retarded V0, high impact injection molding polycarbonateAll information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 293 - 316 °C
560 - 600 °F
LTL Color Compounds ColorFast® FRPC300 Polycarbonate, Flame-Retarded
V2-rated polycarbonateAll information provided by LTL Color Compounders, Inc.
Copyright © lookpolymers.com All Rights Reserved