| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Front Barrel Temperature | 235 °C | 455 °F | For film or coating with EVA or EVOH. |
|
DuPont Bynel® 21E553 Adhesive Resin
(discontinued **)
Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in..
|
|||
| Front Barrel Temperature | 235 °C | 455 °F | For coextrusion with EVA or EVOH. |
|
DuPont Bynel® 41E689 Adhesive Resin
(discontinued **)
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
|
|||
| Front Barrel Temperature | 235 - 265 °C | 455 - 509 °F | Start Point: 235°C |
|
Kingfa JH960 6300 Non-halogenated Flame Retardant PC/ABS Alloy
Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platin..
|
|||
| Front Barrel Temperature | 235 - 255 °C | 455 - 491 °F | Injection Molding |
|
LG Chemical KEYFLEX BT 1172D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
|
|||
| Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
|
LG Chemical Lupox® GP1000M PBT
Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical
|
|||
| Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
|
LG Chemical Lupox® GP1000SB PBT
Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
|
|||
| Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
|
LG Chemical Lupox® GP1006FD PBT
Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica..
|
|||
| Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
|
LG Chemical Lupox® SV-1080 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
|
|||
| Front Barrel Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
|
LG Chemical LUPOY HI5002A PC/ABS, High Impact
Description: Injection Molding, PC/ABS, General Purpose, High Flow, High ImpactApplication: E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
|
|||
| Front Barrel Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
|
LG Chemical LUPOY MP5000AM PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, Metal PlatingApplication: Automotive (Exterior), E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
|
|||
| Front Barrel Temperature | 235 - 270 °C | 455 - 518 °F | Injection Molding |
|
LG Chemical LUPOY SG5009FA PC/ABS/PMMA, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High Gloss, Anti-scratchApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9, 9011-14-7 and 181028-79-5Informatio..
|
|||
| Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
|
Solvay TECHNYL® C 402 M PA6, DRY
Description: Unreinforced polyamide PA6, high viscosity, containing monomer, for extrusion.Available in: Europe and North AmericaProduct Applications: It is suitable for applications requiring high ..
|
|||
| Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
|
Solvay Technyl Starâ„¢ S 218 V30 30% Glass Reinforced Nylon 6
Heat stabilized, low viscosity, injection grade.Information provided by Rhodia; Rhodia has been acquired by Solvay.
|
|||
| Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
|
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant
This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr..
|
|||
| Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
|
Borealis Borcoat™ BB125E Polypropylene Adhesive for Steel Pipe Coating
Borcoat BB125E is a chemically modified polypropylene copolymer designed to be used as the tie layer between the epoxy corrosion protection layer and the top-coat polypropylene Borcoat BB108E-1199.B..
|
|||
| Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
|
Borealis Borcoat™ BB127E Polypropylene Adhesive Powder form for Steel Pipe Coating
Borcoat BB127E is a chemically modified polypropylene copolymer designed to be used as the tie layer between the epoxy corrosion protection layer and the Top-coat polypropylene coating Borcoat BB108..
|
|||
| Front Barrel Temperature | 235 °C | 455 °F | |
|
DuPont Bynel® 3126 Adhesive Resin
Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce..
|
|||
| Front Barrel Temperature | 235 °C | 455 °F | For coextrusion with EVA or EVOH. |
|
DuPont Bynel® 4157 Adhesive Resin
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
|
|||
| Front Barrel Temperature | 235 °C | 455 °F | For coextrusion with EVA or EVOH. |
|
DuPont Bynel® 41E687 Adhesive Resin
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
|
|||
| Front Barrel Temperature | 235 - 271 °C | 455 - 520 °F | |
|
Diamond Polymers ASA S310
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Impact and ModulusInformation provided by Diamond Polymers, Inc.
|
|||
| Front Barrel Temperature | 235 - 271 °C | 455 - 520 °F | |
|
Diamond Polymers ASA S319
Description: ASA Weatherable Polymer, Injection Molding Grade, High ModulusInformation provided by Diamond Polymers, Inc.
|
|||
| Front Barrel Temperature | 235 - 271 °C | 455 - 520 °F | |
|
Diamond Polymers ASA S519
Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Front Barrel Temperature | 235 - 271 °C | 455 - 520 °F | |
|
Diamond Polymers ASA S610
Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Front Barrel Temperature | 235 - 271 °C | 455 - 520 °F | |
|
Diamond Polymers ASA S710
Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Front Barrel Temperature | 235 - 271 °C | 455 - 520 °F | |
|
Diamond Polymers ASA S910
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Front Barrel Temperature | 235 - 271 °C | 455 - 520 °F | |
|
Diamond Polymers ASA TW-17
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Front Barrel Temperature | 235 - 271 °C | 455 - 520 °F | |
|
Diamond Polymers ASA/PC TA-35
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc.
|
|||
| Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
|
Beijing Chemical Industry KAIFA® HN301-G0 PA6 Resin
High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
|
Beijing Chemical Industry KAIFA® HN301-M30 PA6 Resin
Mineral filled, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Front Barrel Temperature | 235 °C | 455 °F | For coextrusion with EVA or EVOH. |
|
DuPont Bynel® 50E662 Adhesive Resin
(discontinued **)
Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E662 are based on polypropylene random copolymers. They are available in pellet form for use in conventional extrusion an..
|
|||