| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-G13 Nylon 6, 13% Glass Reinforced
Nylon 6, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-G20 Nylon 6, 20% Glass Reinforced
Nylon 6, 20% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-G30 Nylon 6, 30% Glass Reinforced
Nylon 6, 30% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-G33 Nylon 6, 33% Glass Reinforced
Nylon 6, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-G33-[color]-H Nylon 6, 33% Glass Reinforced, Heat Stabilized
Nylon 6, 33% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-G43 Nylon 6, 43% Glass Reinforced
Nylon 6, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
|
|||
| Front Barrel Temperature | 246 - 268 °C | 475 - 515 °F | |
|
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-G13-[color]-H Nylon 6, 13% Glass Reinforced, Heat Stabilized
Nylon 6, 13% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-G43-[color]-H Nylon 6, 43% Glass Reinforced, Heat Stabilized
Nylon 6, 43% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-M25G15 Nylon 6, 25% Mineral, 15% Glass Reinforced
Nylon 6, 25% Mineral, 15% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon gra..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-M25G15-[color]-H Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized
Nylon 6, 25% Mineral, 15% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-M40 Nylon 6, 40% Mineral Filled
Nylon 6, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested ..
|
|||
| Front Barrel Temperature | 249 - 268 °C | 480 - 515 °F | |
|
Polymer Resources NY6-M40-[color]-H Nylon 6, 40% Mineral Filled, Heat Stabilized
Nylon 6, 40% Mineral Filled, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g..
|
|||
| Front Barrel Temperature | 252 - 268 °C | 485 - 515 °F | |
|
Teknor Apex Chemlon® 240 MH Nylon 6, 40% Short Glass Fiber Reinforced
Features: Heat Stabilized; Warp Resistant Forms: Pellets Additive: Heat Stabilizer Automotive Specifications: GM GMP.PA6.011Information Provided by Teknor Apex
|
|||
| Front Barrel Temperature | 246 - 268 °C | 475 - 515 °F | |
|
Teknor Apex Chemlon® 225-15 MG Nylon 6, 25% Mineral Reinforced, 15% Glass Fiber Reinforced
Features: Compound offering rigidity and strength, especially at high service temperatures; Excellent for large area parts Processing Method: Injection Molding Forms: Pellets Automotive Specificatio..
|
|||
| Front Barrel Temperature | 252 - 268 °C | 485 - 515 °F | |
|
Teknor Apex Chemlon® 233 GH Nylon, 6, 30% Short Glass Fiber Reinforced
Features: Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated Processing Method: Injection Molding Forms: Pellets Addi..
|
|||
| Front Barrel Temperature | 246 - 268 °C | 475 - 515 °F | |
|
Teknor Apex Chemlon® 214 GH Nylon 6, 14% Short Glass Fiber
Features: Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Toughness; Heat Stabilized; High Strength Processing Method: Injection Molding Forms: Pellets Additive: Heat S..
|
|||