Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Front Barrel Temperature = 540 °F Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Front Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources NY66-IM1-G13 Nylon 66, 13% Glass Reinforced, Toughened
Nylon 66, 13% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g..
Front Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources NY66-IM-G40 Nylon 66, 40% Glass Reinforced, Impact Modified
Nylon 66, 40% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g..
Front Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources NY66-M25G15 Nylon 66, 25% Mineral, 15% Glass Reinforced
Nylon 66, 25% Mineral, 15% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon gr..
Front Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources NY66-M25G15-[color]-H Nylon 66, 25% Mineral, 15% Glass Reinforced, Heat Stabilized
Nylon 66, 25% Mineral, 15% Glass Reinforced, Lubricated and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, te..
Front Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources PC-FD3 Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Front Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources PC-GP3-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, High Flow
Polycarbonate, FDA-compliant Feedstocks, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
Front Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources PC-GP3-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release
Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp..
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-G10HF Modified-PPO, 10% Glass Reinforced, High Flow
Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-GP5 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 270F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-GP6 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-GP7 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 300F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-MF-FRG20 Modified-PPO, 40% Glass/Mineral Reinforced, Flame Retardant
Modified-Polyphenylene Oxide, 40% Glass/Mineral Reinforced, Flame RetardantFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanica..
Front Barrel Temperature 282 - 299 °C
540 - 570 °F
Ravago Manufacturing Americas Hylex® P1010LLT Polycarbonate
Information provided by Ravago.
Front Barrel Temperature 282 - 299 °C
540 - 570 °F
Ravago Manufacturing Americas Hylex® P1310LLT Polycarbonate
Information provided by Ravago
Front Barrel Temperature 282 - 299 °C
540 - 570 °F
PTS Tristar® PC-10 10 MFI Extrusion Grade Polycarbonate
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources NY66-IM1-G33 Nylon 66, 33% Glass Reinforced, Toughened
Nylon 66, 33% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g..
Front Barrel Temperature 282 - 304 °C
540 - 580 °F
Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow
Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P..
Front Barrel Temperature 282 - 299 °C
540 - 570 °F
PTS Tristar® PC-10R 10 MFI Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 282 - 299 °C
540 - 570 °F
PTS Tristar® PC-10R-CL(V) 10 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 282 - 304 °C
540 - 580 °F
LTL Color Compounds ColorFast® PC150 Polycarbonate
15 melt high flow polycarbonateAll information provided by LTL Color Compounders, Inc.
Front Barrel Temperature 282 - 299 °C
540 - 570 °F
Mitsubishi Iupilon® S2000R 9.5 MFI Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 282 - 299 °C
540 - 570 °F
Mitsubishi Iupilon® S2001R 9.5 MFI FDA Compliant Polycarbonate With Release
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 282 - 304 °C
540 - 580 °F
Samyang Trirex® PC-3025N2 10 MFI Flame Retardant Clear Polycarbonate
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-G10 Modified PPO, 10% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-G20 Modified PPO, 20% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-G30 Modified PPO, 30% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-GP5 Modified PPO, General Purpose with HDT of 270 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-GP6 Modified PPO, General Purpose with HDT of 290 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Front Barrel Temperature 282 - 316 °C
540 - 600 °F
Polymer Resources PPX-GP7 Modified PPO, General Purpose with HDT of 300 F  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Copyright © lookpolymers.com All Rights Reserved