| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow
Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i..
|
|||
| Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
|
|||
| Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow
Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted..
|
|||
| Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized
Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
|
|||
| Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE
Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
|
|||
| Front Barrel Temperature | 304 - 316 °C | 580 - 600 °F | |
|
Polymer Resources PC-G30-TFE15 Polycarbonate, 30% Glass Reinforced, 15% PTFE
Polycarbonate, 30% Glass Reinforced, 15% PTFEProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide..
|
|||
| Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-GP2-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Medium Flow
Polycarbonate, FDA-compliant Feedstocks, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
|
|||
| Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-GP2-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release
Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
|
|||
| Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-IM1 Polycarbonate, Impact Modified, Low Flow
Polycarbonate, Impact Modified, Low FlowProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided ..
|
|||
| Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
Polymer Resources PC-IM1-UV Polycarbonate, Impact Modified, Low Flow, UV-stabilized
Polycarbonate, Impact Modified, Low Flow, UV-stabilizedProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
|
|||
| Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
|
Polymer Resources PPX-G10 Modified-PPO, 10% Glass Reinforced
Modified-Polyphenylene Oxide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
|
Polymer Resources PPX-G15 Modified-PPO, 15% Glass Reinforced, High Flow
Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
|
|||
| Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
|
Polymer Resources PPX-G30 Modified-PPO, 30% Glass Reinforced
Modified-Polyphenylene Oxide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
|
Polymer Resources PPX-G5 Modified-PPO, 5% Glass Reinforced
Modified-Polyphenylene Oxide, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro..
|
|||
| Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
|
Polymer Resources PPX-GP6 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
|
|||
| Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
|
Polymer Resources PPX-GP7 Modified-PPO, General Purpose
Modified-Polyphenylene Oxide, General Purpose, 300F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati..
|
|||
| Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
LTL Color Compounds ColorFast® PC100 Polycarbonate
10 melt standard injection molding gradeAll information provided by LTL Color Compounders, Inc.
|
|||
| Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
|
Star Plastics PC1212FRR Molding Grade PC FR
Information provided by Star Plastics, Inc.
|
|||
| Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
|
Star Plastics PC1212FRUV Molding Grade PC FR
Information provided by Star Plastics, Inc.
|
|||
| Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
|
Star Plastics PC1510FR Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
|
Star Plastics PC1510R Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
|
Star Plastics PC1510RUV Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
|
Star Plastics PC1510UV Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Front Barrel Temperature | 288 - 316 °C | 550 - 600 °F | |
|
Star Plastics PC743 Molding Grade PC
Information provided by Star Plastics, Inc.
|
|||
| Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
|
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
|
Polymer Resources PPX-G20 Modified PPO, 20% Glass Reinforced
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
|
Polymer Resources PPX-G30 Modified PPO, 30% Glass Reinforced
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Front Barrel Temperature | 282 - 316 °C | 540 - 600 °F | |
|
Polymer Resources PPX-GP6 Modified PPO, General Purpose with HDT of 290 F
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
LTL Color Compounds ColorFast® FRPC100 Polycarbonate, Flame-Retarded
Flame-retarded V0, high impact injection molding polycarbonateAll information provided by LTL Color Compounders, Inc.
|
|||
| Front Barrel Temperature | 293 - 316 °C | 560 - 600 °F | |
|
LTL Color Compounds ColorFast® FRPC400 Polycarbonate, Flame-Retarded
Flame-retarded V0, high impact injection molding polycarbonateAll information provided by LTL Color Compounders, Inc.
|
|||