| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Injection Velocity | 10.0 - 25.0 mm/sec | 0.394 - 0.984 in/sec | Molding a 6 gram (shot weight) gasket with a 50 ton injection molding machine; screw diameter of 25 mm |
|
Premix Thermoplastics PRETHERM TPE 1050 Thermoplastic Elastomer, Boron Nitride / SEBS compound
PRETHERM TPE 1050 is a thermoplastic elastomer based highly thermally conductive compound intended primarily for heat dissipation. It is used as gap filler between processor and heat sink or co-mold..
|
|||
| Injection Velocity | 10.0 - 25.0 mm/sec | 0.394 - 0.984 in/sec | Molding a 6 gram (shot weight) gasket with a 50 ton injection molding machine; screw diameter of 25 mm |
|
Premix Thermoplastics PRETHERM TPE 1075 Thermoplastic Elastomer, Boron Nitride / SEBS compound
PRETHERM TPE 1075 is a thermoplastic elastomer based highly thermally conductive compound intended primarily for heat dissipation. It can be used as gap filler between processor and heat sink or co-..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Zythane™ 3045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 4045D Thermoplastic Polyurethane Elastomer
Zythane™ 4045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 4050D Thermoplastic Polyurethane Elastomer
Zythane™ 4050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 4060A Thermoplastic Polyurethane Elastomer
Zythane™ 4060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 4060D Thermoplastic Polyurethane Elastomer
Zythane™ 4060D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 4065D Thermoplastic Polyurethane Elastomer
Zythane™ 4065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 4080A Thermoplastic Polyurethane Elastomer
Zythane™ 4080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 4090A Thermoplastic Polyurethane Elastomer
Zythane™ 4090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 5045D Thermoplastic Polyurethane Elastomer
Zythane™ 5045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 5070A Thermoplastic Polyurethane Elastomer
Zythane™ 5070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 5090A Thermoplastic Polyurethane Elastomer
Zythane™ 5090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 6050D Thermoplastic Polyurethane Elastomer
Zythane™ 6050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 6055D Thermoplastic Polyurethane Elastomer
Zythane™ 6055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 6065D Thermoplastic Polyurethane Elastomer
Zythane™ 6065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 6080A Thermoplastic Polyurethane Elastomer
Zythane™ 6080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 6090A Thermoplastic Polyurethane Elastomer
Zythane™ 6090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 7045A Thermoplastic Polyurethane Elastomer
Zythane™ 7045A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 7050D Thermoplastic Polyurethane Elastomer
Zythane™ 7050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 7055D Thermoplastic Polyurethane Elastomer
Zythane™ 7055D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer
Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 7070A Thermoplastic Polyurethane Elastomer
Zythane™ 7070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer
Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 7085AF Thermoplastic Polyurethane Elastomer
Zythane™ 7085AF is a FR polyether-based TPU specifically formulated with non-halogenated flame retardants for extrusion applications with ease of processing. It exhibits excellent abrasion resistan..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 4070A Thermoplastic Polyurethane Elastomer
Zythane™ 4070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 5085A Thermoplastic Polyurethane Elastomer
Zythane™ 5085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 7075A Thermoplastic Polyurethane Elastomer
Zythane™ 7075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer
Zythane™ 7085UF is a UV stabilized polyether-based TPU specifically formulated for extrusion applications. It exhibits excellent abrasion resistance and toughness and has good hydrolytic stability,..
|
|||
| Injection Velocity | >= 10.0 mm/sec | >= 0.394 in/sec | Injection |
|
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer
Zythane™ 7090A is a polyether-based TPU specifically formulated for extrusion molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good hydroly..
|
|||