| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | Average value: 150 mm/sec Grade Count:20 |
|
Overview of materials for Polypropylene with 20% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Borcom™ WE007AE Polypropylene
Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ ED117AE Polypropylene TPO Compound
Daplen™ ED117AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ ED230HP Polypropylene TPO Compound
Daplen™ ED230HP is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EE108U Polypropylene TPO Compound
Daplen™ EE108U is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EE158AI Polypropylene TPO Compound
Daplen™ EE158AI is a 13% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EE168AI Polypropylene TPO Compound
Daplen™ EE168AI is a 10% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. ..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EE188HP Polypropylene TPO Compound
Daplen™ EE188HP is a 15% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and g..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EF341AE Polypropylene TPO Compound
Daplen™ EF341AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EG103AI Polypropylene Compound, Mineral Filled
Daplen™ EG103AI is a 15 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and high melt flow rate..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EG250AI Polypropylene TPO Compound
Daplen™ EG250AI is a 20% mineral reinforced impact modified polypropylene compound suitable for injection molding. This material has an excellent balance between impact strength and stiffness, giv..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EH104AE Polypropylene TPO Compound
Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis EE002AE Polypropylene Elastomer Modified
EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis GB364WG Polypropylene Compound, Glass Fiber Reinforced
GB364WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis GD310U Polypropylene Compound, Glass Fiber Reinforced
GD310U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. ..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis HB601WG Polypropylene Homopolymer
HB601WG is a polypropylene homopolymer intended for injection molding and blow molding. The product is available in natural but other colors can be provided on request. This material has excellent ..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis HF700SA Polypropylene
HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.Infor..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis MD441U Polypropylene Compound, Mineral Filled
MD441U is a 40% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: air cond..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis ME266U Polypropylene Compound, Mineral Filled
ME266U is a 20% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gives a good surface quality. ..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis MG302Al Polypropylene Compound, Mineral Filled
MG302AI is a 30% mineral filled polypropylene compound intended for injection and back injection molding. This material has an excellent balance between impact strength and stiffness and high melt ..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis PS65C40 Polypropylene Compound, Mineral Filled
PS65C40 is a 40% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis PS65T20 Polypropylene Compound, Mineral Filled
PS65T20 is a 20% mineral filled polypropylene compound intended for injection and back injection molding. This material has excellent balanced mechanical properties and high melt flow rate. Applic..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EE065AI Polypropylene Elastomer Modified
Daplen™ EE065AI is an elastomer modified polypropylene with increased crystallinity. This material has an excellent balance between impact strength and stiffness. The product is available in natu..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EE188AI Polypropylene TPO Compound
Daplen™ EE188AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. ..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EF261AI Polypropylene TPO Compound
Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process...
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EF267AI Polypropylene TPO Compound
Daplen™ EF267AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process...
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis ME212U Polypropylene Compound, Mineral Filled
ME212U is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: air ducts, air..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EF103AE Polypropylene TPO Compound
Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis ME268Al Polypropylene Compound, Mineral Filled
ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EF209AE Polypropylene TPO Compound
Daplen™ EF209AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..
|
|||