| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LCF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LCF40 - PA66 Nylon 66, 40% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LCF50 - PA6 Nylon 6, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LCF50 - PA66 Nylon 66, 50% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF20 - PA6 Nylon 6, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 20% long glass reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF20 - PP Homopolymer Polypropylene, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 20% long glass fiber reinforcementInformation provided by PlastiComp, In..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF30 - PP Homopolymer Polypropylene, 30% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% long glass fiber reinforcementInformation provided by PlastiCom..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 30% long glass fiber reinforcementInformation provided by Plas..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF40 - PA6 Nylon 6, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF50 - PA6 Nylon 6, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF50 - PA66 MT Nylon 66, 50% Long Glass Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementImpact modifiedInformation provided by ..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF50 - PP Homopolymer Polypropylene, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% long glass fiber reinforcementInformation provided by PlastiCom..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF60 - PA66 Nylon 66, 60% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 60% long glass fiber reinforcementInformation provided by PlastiComp, In..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LCF30 - PA66 Nylon 66, 30% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LCF40 - PA6 Nylon 6, 40% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LCF40 - PA66 MT Nylon 66, 40% Long Carbon Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementImpact modifiedInformation provided by Pla..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LCF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 40% carbon fiber reinforcementInformation provided by PlastiComp, In..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LCF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 50% long glass fiber reinforcementInformation provided by Plas..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF60 - TPU Rigid Thermoplastic Polyurethane, 60% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 60% long glass fiber reinforcementInformation provided by Plas..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | Average value: 63.5 mm/sec Grade Count:3 |
|
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LCF50 - PA66 MT Nylon 66, 50% Long Carbon Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 50% carbon fiber reinforcementImpact modifiedInformation provided by Pla..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF20 - PA66 Nylon 66, 20% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF30 - PA66 Nylon 66, 30% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 30% long glass fiber reinforcementInformation provided by PlastiComp, In..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | |
|
PlastiComp Complet® LGF40 - PA66 Nylon 66, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementInformation provided by PlastiComp, In..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | Average value: 63.5 mm/sec Grade Count:5 |
|
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi..
|
|||
| Injection Velocity | 50.8 - 76.2 mm/sec | 2.00 - 3.00 in/sec | Average value: 63.5 mm/sec Grade Count:3 |
|
Overview of materials for Polypropylene, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o..
|
|||