| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Injection Velocity | 200 mm/sec | 7.87 in/sec | |
|
Ineos ABS Lustran® LGA-SF
(discontinued **)
Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquir..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | |
|
Covestro Apec® 1600 Polycarbonate
(discontinued **)
Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingBlow moldingCalanderingTransfer moldingThermoformingInformation provided by Bay..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | |
|
Ineos ABS Centrex® 813 ASA+AES Blend
(discontinued **)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingInformation provided by Ba..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | |
|
Ineos ABS Centrex® 833 ASA+AES Blend
(discontinued **)
Key Features:UnfilledHigh impact or high impact modifiedLight stabilized or stable to lightU.V. stabilized or stable to weatherSuitable processing methods:Profile extrusionSheet extrusionThermoformi..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | |
|
Ineos ABS Lustran® 446
Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | |
|
Ineos ABS Lustran® 556
Key Features:UnfilledSuitable processing methods:Sheet extrusionThermoforming
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | Injection molding |
|
Styrolution Luran® 358 N SAN
Luran 358 N is an easy-flowing injection molding SAN grade.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile
Luran HH-120 is a grade of AMSAN with high heat resistance and improved mechanical strength. It is suitable for injection molding and extrusion applications and can be used as a modifier for high he..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Styrolution Luran® S 767KE ASA
Luran S 767KE is particular suitable for co-extrusion with PVC at low temperature. Hereby, it provides a glossy surface finish.Enhanced flowabilitySuitable for co-extrusion with PVCEnables high glos..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Styrolution PS 168N GPPS
Styrolution PS 168N is a high molecular weight, heat resistant grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. Also use as a blend componen..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Styrolution PS 2710 HIPS
Styrolution PS 2710 is a high impact grade of polystyrene with improved stress crack resistance, developed for extrusion and thermoforming applications, especially for the refrigerator industry.Impr..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Styrolution PS 454N HIPS
Styrolution PS 454N is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Good balance of toughness, high flow, and heat resistanceHigh gloss..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Styrolution PS 476L HIPS
Styrolution PS 476L is a normal flow and very high impact Polystyrene. It gives good mechanical and heat resistance properties while providing with easy processability and short cycle time.Normal fl..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Styrolution Terlux® HD 2822 MABS
Terlux® HD 2822 is a new standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well ..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Covestro Makroblend® KU 2-7609 Polycarbonate + PBT, Mineral Filled Impact Grade
ISO 7792-1-PC/PBT,MHPR,-030,MD20(PC+PBT)-blendsimpact modifiedInjection molding grade20% mineral filledPreprocessingMax. Water content
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Covestro Makroblend® KU 2-7940 Polycarbonate + PBT, Impact Grade
Developmental productISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Covestro Makrolon® 2405 MAS057 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Covestro Makrolon® 2656 Polycarbonate
ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAv..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Covestro Makrolon® 2867 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFLR,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt tem..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Covestro Makrolon® 9417 Polycarbonate, 10% Glass Filled
ISO 7391-PC,MFLR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityUV stab..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Covestro Makrolon® ET UV510 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• PC/UV absorber concent..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Covestro Makrolon® FU1007 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Covestro Makrolon® GF8001* Polycarbonate, 20% Glass Filled
ISO 7391-PC,MR,(,,)-18-3,GF20Developmental productFormerly Makrolon DP1-1951MVR (300 °C/1.2 kg) 16 cm3/10 min20 % Glass fiber reinforcedLow viscosityEasy releaseInjection molding - Melt temperature..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Covestro Makrolon® Rx2430 Polycarbonate
ISO 7391-PC,M,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minMedical devicessuitable for sterilization with high-energy radiationComplies with the requirements of FDA-modified ISO 10993-1 an..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Covestro Makrolon® 1260 Polycarbonate, Impact Grade
ISO 7391-PC,MPR,(,,)-24-9Global gradeMVR (300 °C/1.2 kg) 34 cm3/10 minImpact modifiedLow viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in light colors onlyPreproc..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Covestro Makrolon® 6487 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFlame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 2..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Covestro Makrolon® DP1-1843* Polycarbonate
ISO 7391-PC,RL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 9.5 cm3/10 minMedium viscosityUV stabilizedRotomoldingAvailable in transparent and translucent colorsGlobe lightsAs of 1 September 2..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Covestro Makrolon® Rx2635 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Med..
|
|||
| Injection Velocity | 200 mm/sec | 7.87 in/sec | ISO 294 |
|
Covestro Makrolon® KU1-1230* Polycarbonate
ISO 7391-PC,EFL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 8.5 cm3/10 minFlame retardant16 mm Triple wall sheet/B1 classification (DIN 4102)Medium viscosityUV stabilizedExtrusionAs of 1 Sept..
|
|||