| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Injection Velocity | 60.0 - 200 mm/sec | 2.36 - 7.87 in/sec | Average value: 107 mm/sec Grade Count:3 |
|
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | Average value: 150 mm/sec Grade Count:20 |
|
Overview of materials for Polypropylene with 20% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis BC612WG Polypropylene Copolymer
BC612WG is a polypropylene copolymer intended for injection molding. The product is available in natural but other colors can be provided on request. This material has excellent balanced mechanical..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Borcom™ WE007AE Polypropylene
Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Borcom™ WG140AI Polypropylene
Borcom™ WG140AI is a polypropylene microcomposite intended for injection molding. This material has an excellent balance between impact strength and stiffness, high melt flow rate and gives a good..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ ED117AE Polypropylene TPO Compound
Daplen™ ED117AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EE108U Polypropylene TPO Compound
Daplen™ EE108U is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EE168AI Polypropylene TPO Compound
Daplen™ EE168AI is a 10% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. ..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EE260AI Polypropylene TPO Compound
Daplen™ EE260AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process...
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EF005AE Polypropylene TPO Compound
Daplen™ EF005AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EF210AE Polypropylene TPO Compound
Daplen™ EF210AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EG103AI Polypropylene Compound, Mineral Filled
Daplen™ EG103AI is a 15 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and high melt flow rate..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ KB4436 Polypropylene TPO Compound
Daplen™ KB4436 is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gi..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis GB205U Polypropylene Compound, Glass Fiber Reinforced
GB205U is a 20% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Thi..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis GB311U Polypropylene Compound, Glass Fiber Reinforced
GB311U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. ..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis GB364WG Polypropylene Compound, Glass Fiber Reinforced
GB364WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis HF700SA Polypropylene
HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.Infor..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis HK030U Polypropylene Compound
HK030U is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wit..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis MB250WG Polypropylene Compound, Mineral Filled
MB250WG is a 20 % mineral filled polypropylene compound intended for injection molding. Applications: MB250WG has been developed especially for the white goods industry. Washing machine parts, and ..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis ME266U Polypropylene Compound, Mineral Filled
ME266U is a 20% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gives a good surface quality. ..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis PS65T20 Polypropylene Compound, Mineral Filled
PS65T20 is a 20% mineral filled polypropylene compound intended for injection and back injection molding. This material has excellent balanced mechanical properties and high melt flow rate. Applic..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EE065AI Polypropylene Elastomer Modified
Daplen™ EE065AI is an elastomer modified polypropylene with increased crystallinity. This material has an excellent balance between impact strength and stiffness. The product is available in natu..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EE189AI Polypropylene TPO Compound
Daplen™ EE189AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. ..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EF261AI Polypropylene TPO Compound
Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process...
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EF267AI Polypropylene TPO Compound
Daplen™ EF267AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process...
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis MS64T20 Polypropylene Compound, Mineral Filled
MS64T20 is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: automotive p..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EF103AE Polypropylene TPO Compound
Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis MD231U Polypropylene Compound, Mineral Filled
MD231U is a 20 % mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: Air duc..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis ME268Al Polypropylene Compound, Mineral Filled
ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par..
|
|||
| Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
|
Borealis Daplen™ EF209AE Polypropylene TPO Compound
Daplen™ EF209AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..
|
|||