| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 111-55 Thermoplastic Elastomer
(discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 221-73 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 261-87 Thermoplastic Elastomer
(discontinued **)
A hard, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance for use in wet electrical wire and cable applications. This gra..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Vyram™ 9101-45 Thermoplastic Elastomer
(discontinued **)
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Vyram™ 9101-85 Thermoplastic Elastomer
(discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Vyram™ 9103-54 Thermoplastic Elastomer
(discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Vyram™ 9201-85 Thermoplastic Elastomer
(discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber
(discontinued **)
A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
|
|||
| Cushion | 0.330 - 0.635 cm | 0.130 - 0.250 in | |
|
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy
Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati..
|
|||
| Cushion | 0.330 - 0.635 cm | 0.130 - 0.250 in | |
|
MRC Polymers NAXALOYâ„¢ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled
Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc.
|
|||
| Cushion | 0.330 - 0.635 cm | 0.130 - 0.250 in | |
|
MRC Polymers NAXALOYâ„¢ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled
Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc.
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 111-35 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 121-87 Thermoplastic Elastomer
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 123-40 Thermoplastic Elastomer
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 271-64 Thermoplastic Elastomer
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 271-80 Thermoplastic Elastomer
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 271-87 Thermoplastic Elastomer
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 8211-75 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 8271-75 Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated ..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 121-80 Thermoplastic Elastomer
A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 203-50 Thermoplastic Elastomer
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer
(discontinued **)
A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer
(discontinued **)
A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance ..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 223-50 Thermoplastic Elastomer
(discontinued **)
A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer
Product Description: A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 101-80 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
|
|||
| Cushion | 0.317 - 0.635 cm | 0.125 - 0.250 in | |
|
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer