| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | |
|
Multibase TPSiV® 4000-80A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob..
|
|||
| Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | |
|
Huntsman AVALON® 98 AE Thermoplastic Polyurethane
Introduction: AVALON 98 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 98 AE is part of the AVALON Perform Range and offers a premium soiling materi..
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
|
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester
Introduction: IROGRAN A 85 E 4607 is a thermoplastic polyether- polyurethane intended for extrusion and injection molding applications. Additional characteristics of the product are excellent mechan..
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
|
Huntsman IROGRAN® A 85 P 4722 TPU-Polyester
Introduction: IROGRAN A 85 P 4722 is a halogen-free thermoplastic- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are good microbial resista..
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
|
Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 86 E 4486 is a thermoplastic polyester- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are excellent mechanical prop..
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
|
Huntsman IROGRAN® A 87 H 4615 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 87 H 4615 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi..
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
|
Huntsman IROGRAN® A 92 P 4851 Ether-Based TPU-For Cable Industry
Introduction: IROGRAN A 92 P 4851 is a thermoplastic polyether- polyurethane for injection molding and extrusion applications. Additional characteristics of the product are high extrudability and lo..
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
|
Huntsman IROGRAN® A 95 E 4813 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 95 R 4813 is a thermoplastic polyester- polyurethane for injection moulding applications. Additional characteristics of the product are very short cycle times and high dimens..
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
|
Huntsman IROGRAN® A 95 H 4678 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e..
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical LUCEL FW700N Modified POM, Friction Resistance, Abrasion Resistance
Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0Information provided by LG Chemical
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical LUCEL FW715CS Modified POM, Friction Resistance, Abrasion Resistance
Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 471-34-1Information provided by LG ..
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical LUCEL FW720F Modified POM, Friction Resistance, Abrasion Resistance
Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 9002-84-2Information provided by LG..
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical LUCEL HI510 POM+Rubber, High Impact
Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0Information provided by LG Chemical
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
LG Chemical LUCEL HI515W POM+Rubber, High Impact
Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection |
|
Huntsman IROGRAN® A 92 E 4694 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 92 E 4694 is a thermoplastic special- polyester-polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and ..
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
Stellarchem GP-785A TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
Stellarchem GP-915UB TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Nozzle Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
|
Stellarchem GP-980 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Nozzle Temperature | 180 - 220 °C | 356 - 428 °F | Injection |
|
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer
TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r..
|
|||
| Nozzle Temperature | 180 - 195 °C | 356 - 383 °F | |
|
Lubrizol Estane® T470A Thermoplastic Polyurethane
Type: Estane® T470A is a Shore 77A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b..
|
|||
| Nozzle Temperature | 180 °C | 356 °F | |
|
Tisan TISETILEN® Flame Retardant (V0) Polyethylene
TISETILEN has a wide area of application in construction, building auxiliary materials, lighting equipment, household appliance, toy industries, etc. General specifications include Low densityFlexib..
|
|||
| Nozzle Temperature | 180 °C | 356 °F | |
|
Tisan TISETILEN® UNR Polyethylene
TISETILEN has a wide area of application in construction, building auxiliary materials, lighting equipment, household appliance, toy industries, etc. General specifications include Low densityFlexib..
|
|||
| Nozzle Temperature | 180 - 190 °C | 356 - 374 °F | Injection |
|
Lubrizol ESTANE® GP65AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 65AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
|
|||
| Nozzle Temperature | 180 - 220 °C | 356 - 428 °F | |
|
Unitika TERRAMAC TE-1030 Polylactic Acid (PLA)
High-Impact grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
|
|||
| Nozzle Temperature | 180 - 240 °C | 356 - 464 °F | |
|
Arkema Group Pebax® 2533 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 2533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
|
|||
| Nozzle Temperature | 180 - 220 °C | 356 - 428 °F | Average value: 200 °C Grade Count:18 |
|
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..
|
|||
| Nozzle Temperature | 180 - 240 °C | 356 - 464 °F | |
|
Arkema Group Pebax® Rnew 35R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 35R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
|
|||
| Nozzle Temperature | 180 - 195 °C | 356 - 383 °F | |
|
Lubrizol Estane® S175A Thermoplastic Polyurethane
Type: Estane® S175A is a Shore 77A, polyester type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Mid..
|
|||
| Nozzle Temperature | 180 - 220 °C | 356 - 428 °F | Injection |
|
Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer
TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor rec..
|
|||
| Nozzle Temperature | 180 - 195 °C | 356 - 383 °F | |
|
Lubrizol Estane® T865A Thermoplastic Polyurethane
Type: Estane® T865A is a Shore 71A, polyester grade, plasticized low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Corporation
|
|||