Polymer Property : Nozzle Temperature = 193 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® J-60/10 Polypropylene Homopolymer, 10% Glass Reinforced
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® J-60/10/E Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® J-60/10/E/M Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® J-60/20/E Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® J-60/20/H Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® J-60/30/E/HF Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, improved flow
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® J-60/30/F Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® J-60/40 Polypropylene Homopolymer, 40% Glass Reinforced
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® J-60/40/E/EX Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled, high viscosity
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® PP-60/TC/20 Polypropylene Homopolymer, 20% Talc Filled
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® PP-68/TC/20 Polypropylene Copolymer, 20% Talc
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® J-60/20/E/HF Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled, improved flow
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® J-60/20/E8/M Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® J-62/30/E8 Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® J-68/10/E Polypropylene Copolymer, 10% Glass Fiber Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Elastocon TPE Technologies Elastocon® 8068BL Thermoplastic Elastomer
Elastocon® 8068BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068BL is well sui..
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Elastocon TPE Technologies Elastocon® 8068L Thermoplastic Elastomer
Elastocon® 8068L is a colorable lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8068L is well ..
Nozzle Temperature 182 - 193 °C
360 - 380 °F
Fiberfil® J-62/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics